MOLTEN STEEL DESULFURIZATION METHOD, MOLTEN STEEL SECONDARY REFINING METHOD, AND MOLTEN STEEL MANUFACTURING METHOD
    1.
    发明申请
    MOLTEN STEEL DESULFURIZATION METHOD, MOLTEN STEEL SECONDARY REFINING METHOD, AND MOLTEN STEEL MANUFACTURING METHOD 审中-公开
    钼钢脱硫方法,钢铁二次精炼方法和钢铁制造方法

    公开(公告)号:US20140096643A1

    公开(公告)日:2014-04-10

    申请号:US14123688

    申请日:2012-08-08

    IPC分类号: C21C7/064

    摘要: There are provided a method for desulfurizing molten steel, characterized in that a sample taken out from molten steel after the tapping from a converter or during the secondary refining is analyzed rapidly in a high accuracy by a method comprising a high frequency induction heating step wherein the sample is combusted and oxidized under the high frequency induction heating in a pure oxygen atmosphere to convert S in the sample into SO2 and an analyzing step wherein SO2-containing gas produced in the high frequency induction heating step is analyzed through an ultraviolet fluorescence method to quantify S concentration of the sample, whereby S concentration of molten steel after the tapping from the converter can be controlled in a high accuracy to prevent failure of S concentration and also desulfurization time in the secondary refining can be shortened and the amount of the desulfurizer or the like used can be reduced, and a method of manufacturing molten steel by using such a method.

    摘要翻译: 提供了一种用于钢水脱硫的方法,其特征在于,通过包括高频感应加热步骤的方法,以高精度快速地分析从转炉中或在二次精炼过程中从钢水中取出的样品,其中, 样品在纯氧气氛中在高频感应加热下燃烧和氧化,将样品中的S转化成SO2,分析步骤,其中通过紫外荧光法分析在高频感应加热步骤中产生的含SO 2的气体,以量化 S浓度,可以高精度地控制从转炉出料后的钢水的S浓度,以防止S浓度的降低,并且可以缩短二次精炼中的脱硫时间,并且脱硫剂或 可以减少使用的方法,以及使用这种方法制造钢水的方法 。

    METHOD FOR DESULFURIZING HOT METAL
    2.
    发明申请
    METHOD FOR DESULFURIZING HOT METAL 有权
    冷却金属的方法

    公开(公告)号:US20140083251A1

    公开(公告)日:2014-03-27

    申请号:US14119692

    申请日:2012-08-08

    IPC分类号: C21C1/02

    摘要: In a method for desulfurizing hot metal by analyzing S concentration of a sample taken out from the hot metal, the S concentration is analyzed rapidly and precisely by a method comprising a high frequency induction heating step of oxidizing the sample under a high frequency induction heating in a pure oxygen atmosphere to convert S in the hot metal to SO2 and an analysis step of analyzing SO2-containing gas generated in the high frequency induction heating step through an ultraviolet fluorescence method to quantify S concentration in the sample, whereby S concentration after the desulfurization is controlled precisely and hence fault of S concentration is prevented but also the increase of the cost due to the excessive addition of a desulfurization agent and step disruption at steel-making step are prevented.

    摘要翻译: 在通过分析从铁水中取出的样品的S浓度来分析硫酸铁的方法中,通过包括在高频感应加热下对样品进行氧化的高频感应加热步骤的方法,迅速且精确地分析S浓度 将氧化铁中的S转化为SO2的纯氧气氛和通过紫外线荧光法分析在高频感应加热工序中产生的含SO 2气体的分析步骤,以量化样品中的S浓度,由此脱硫后的S浓度 被精确地控制,因此防止了S浓度的故障,并且防止了由于过度添加脱硫剂而造成的成本的增加以及在炼钢步骤中的阶段破坏。

    Method for desulfurizing hot metal
    3.
    发明授权
    Method for desulfurizing hot metal 有权
    铁水脱硫方法

    公开(公告)号:US09068237B2

    公开(公告)日:2015-06-30

    申请号:US14119692

    申请日:2012-08-08

    摘要: In a method for desulfurizing hot metal by analyzing S concentration of a sample taken out from the hot metal, the S concentration is analyzed rapidly and precisely by a method comprising a high frequency induction heating step of oxidizing the sample under a high frequency induction heating in a pure oxygen atmosphere to convert S in the hot metal to SO2 and an analysis step of analyzing SO2-containing gas generated in the high frequency induction heating step through an ultraviolet fluorescence method to quantify S concentration in the sample, whereby S concentration after the desulfurization is controlled precisely and hence fault of S concentration is prevented but also the increase of the cost due to the excessive addition of a desulfurization agent and step disruption at steel-making step are prevented.

    摘要翻译: 在通过分析从铁水中取出的样品的S浓度来分析硫酸铁的方法中,通过包括在高频感应加热下对样品进行氧化的高频感应加热步骤的方法,迅速且精确地分析S浓度 将氧化铁中的S转化为SO2的纯氧气氛和通过紫外线荧光法分析在高频感应加热工序中产生的含SO 2气体的分析步骤,以量化样品中的S浓度,由此脱硫后的S浓度 被精确地控制,因此防止了S浓度的故障,并且防止了由于过度添加脱硫剂而造成的成本的增加以及在炼钢步骤中的阶段破坏。

    Apparatus for continuous electrolytic treatment of steel sheet and method for producing surface-treated steel sheet using the same
    5.
    发明授权
    Apparatus for continuous electrolytic treatment of steel sheet and method for producing surface-treated steel sheet using the same 有权
    钢板的连续电解处理装置及使用该钢板的表面处理钢板的制造方法

    公开(公告)号:US09580816B2

    公开(公告)日:2017-02-28

    申请号:US13819500

    申请日:2011-09-14

    摘要: Provided are an apparatus for continuous electrolytic treatment of a steel sheet that is suitable for producing a surface-treated steel sheet and a method for producing the surface-treated steel sheet using the apparatus for continuous electrolytic treatment of a steel sheet. The apparatus includes N pairs of tabular electrodes having a length L and being arranged to respectively face two surfaces of a steel sheet. Each electrode includes n sections arranged in the longitudinal direction of the electrode and disposed on the surface of the electrode facing the steel sheet surface. Each section is constituted by a conductive portion including an electrode portion having a length T1 and a nonconductive portion made by making an electrode portion having a length T2 nonconductive, where n×N≧10, 0.96≧T2/(T1+T2)≧0.05, and 0.9≧T1/L≧0.1.

    摘要翻译: 提供一种适用于生产表面处理钢板的钢板的连续电解处理装置以及使用钢板的连续电解处理装置的表面处理钢板的制造方法。 该装置包括N对长度为L的平板状电极,并分别面对钢板的两个表面。 每个电极包括沿着电极的纵向布置的n个部分,并且设置在面对钢板表面的电极的表面上。 每个部分由包括具有长度T1的电极部分和通过制造具有长度T2不导电的电极部分制成的非导电部分的导电部分构成,其中n×N≥10,0.96≥T2/(T1 + T2)≥0.05 ,0.9≥T1/L≥0.1。

    APPARATUS FOR CONTINUOUS ELECTROLYTIC TREATMENT OF STEEL SHEET AND METHOD FOR PRODUCING SURFACE-TREATED STEEL SHEET USING THE SAME
    6.
    发明申请
    APPARATUS FOR CONTINUOUS ELECTROLYTIC TREATMENT OF STEEL SHEET AND METHOD FOR PRODUCING SURFACE-TREATED STEEL SHEET USING THE SAME 有权
    用于钢板的连续电解处理的装置以及使用其生产表面处理钢板的方法

    公开(公告)号:US20130228467A1

    公开(公告)日:2013-09-05

    申请号:US13819500

    申请日:2011-09-14

    IPC分类号: C23C28/02

    摘要: Provided are an apparatus for continuous electrolytic treatment of a steel sheet that is suitable for producing a surface-treated steel sheet and a method for producing the surface-treated steel sheet using the apparatus for continuous electrolytic treatment of a steel sheet. The apparatus includes N pairs of tabular electrodes having a length L and being arranged to respectively face two surfaces of a steel sheet. Each electrode includes n sections arranged in the longitudinal direction of the electrode and disposed on the surface of the electrode facing the steel sheet surface. Each section is constituted by a conductive portion including an electrode portion having a length T1 and a nonconductive portion made by making an electrode portion having a length T2 nonconductive, where n×N≧10, 0.96≧T2/(T1+T2)≧0.05, and 0.9≧T1/L≧0.1.

    摘要翻译: 提供一种适用于生产表面处理钢板的钢板的连续电解处理装置以及使用钢板的连续电解处理装置的表面处理钢板的制造方法。 该装置包括N对长度为L的平板状电极,并分别面对钢板的两个表面。 每个电极包括沿着电极的纵向布置的n个部分,并且设置在面对钢板表面的电极的表面上。 每个部分由包括具有长度T1的电极部分和通过使具有长度T2不导电的电极部分制成的不导电部分的导电部分构成,其中n×N> = 10,0.96> = T2 /(T1 + T2) > = 0.05,0.9> = T1 / L> = 0.1。

    METHOD AND APPARATUS FOR MANUFACTURING SI-CONTAINING COLD ROLLED STEEL SHEETS
    10.
    发明申请
    METHOD AND APPARATUS FOR MANUFACTURING SI-CONTAINING COLD ROLLED STEEL SHEETS 有权
    用于制造含SI的冷轧钢板的方法和装置

    公开(公告)号:US20140013814A1

    公开(公告)日:2014-01-16

    申请号:US14008353

    申请日:2012-03-26

    IPC分类号: C23G3/02

    摘要: This invention provides methods and apparatuses which can manufacture Si-containing cold rolled steel sheets exhibiting excellent chemical conversion properties even if a chemical conversion treatment solution is used at a lower temperature while minimally suppressing the generation of sludge as well as reducing running costs. The method includes steps of cold rolling a steel containing 0.5 to 3.0 mass % Si, continuously annealing the cold rolled steel sheet, pickling the surface of the continuously annealed cold rolled steel sheet, and repickling the surface of the pickled steel sheet with a non-oxidative acid. The repickling is performed such that a repickling solution is sampled continuously or periodically, an acid concentration in the sampled solution is measured, and the acid concentration in the repickling solution is regularly controlled within a prescribed concentration range.

    摘要翻译: 本发明提供了即使在较低温度下使用化学转化处理液同时极少地抑制污泥的产生以及降低运行成本的情况下,也可以制造出具有优异的化学转化性能的含Si冷轧钢板的方法和装置。 该方法包括冷轧含有0.5〜3.0质量%Si的钢,对冷轧钢板进行连续退火,酸洗连续退火的冷轧钢板的表面, 氧化酸。 进行复印,使得连续或周期性地取样补液,测定取样溶液中的酸浓度,并将反复溶液中的酸浓度定期控制在规定浓度范围内。