    摘要: A method for fabricating multi-component nanowires is disclosed, which can make multi-component nanowires used to realize a nanowire-based memory device by an electroplating process using a multi-component solution. The method for fabricating multi-component nanowires in accordance with the present invention includes the steps of: (a) preparing an anodized aluminum oxide nanotemplate having a plurality of pores; (b) forming an electrode layer on one surface of the anodized aluminum oxide nanotemplate; (c) injecting the anodized aluminum oxide nanotemplate in a predetermined multi-component solution and then growing multi-component nanowires through the pores of the anodized aluminum oxide nanotemplate by an electroplating process in which the anodized aluminum oxide nanotemplate is used as a cathode; and (d) removing the anodized aluminum oxide nanotemplate.

    摘要翻译: 公开了一种制造多组分纳米线的方法,其可以通过使用多组分溶液的电镀工艺制造用于实现基于纳米线的存储器件的多组分纳米线。 根据本发明的制造多组分纳米线的方法包括以下步骤:(a)制备具有多个孔的阳极化氧化铝纳米模板; (b)在阳极化氧化铝纳米模板的一个表面上形成电极层; (c)将阳极氧化的氧化铝纳米模板注入预定的多组分溶液中,然后通过电镀工艺将阳极氧化的氧化铝纳米模板用作阴极,然后通过阳极氧化的氧化铝纳米模板的孔生长多组分纳米线; 和(d)去除阳极氧化的氧化铝纳米模板。

    Bifunctional magnetic core-semiconductor shell nanoparticles and manufacturing method thereof
    7.
    发明授权
    Bifunctional magnetic core-semiconductor shell nanoparticles and manufacturing method thereof 有权
    双功能磁芯 - 半导体壳纳米粒子及其制造方法

    公开(公告)号:US07910164B2

    公开(公告)日:2011-03-22

    申请号:US11860002

    申请日:2007-09-24

    IPC分类号: B05D7/00 B32B5/16

    摘要: Provided are bifunctional magnetic core-semiconductor shell nanoparticles and a manufacturing method thereof. The method includes mixing magnetic core material precursors and a reducing agent for the core material precursors; preparing a first mixture solution; heating and cooling the first mixture solution and preparing magnetic core materials; mixing the magnetic core materials with semiconductor shell material precursors and a reducing agent for the semiconductor shell material precursors; preparing a second mixture solution; and heating and cooling the second mixture solution and coating the magnetic core materials with the semiconductor shell materials.

    摘要翻译: 提供双功能磁芯 - 半导体壳纳米粒子及其制造方法。 该方法包括混合磁芯材料前体和芯材前体的还原剂; 制备第一混合溶液; 加热冷却第一混合液并制备磁芯材料; 将磁芯材料与半导体外壳材料前体和用于半导体外壳材料前体的还原剂混合; 制备第二混合溶液; 并加热和冷却第二混合物溶液并用半导体外壳材料涂覆磁芯材料。

    Polyethoxylated ascorbic acid derivatives as a novel antioxidant and process for preparing thereof
    8.
    发明授权
    Polyethoxylated ascorbic acid derivatives as a novel antioxidant and process for preparing thereof 失效
    聚乙氧基化抗坏血酸衍生物作为新型抗氧化剂及其制备方法

    公开(公告)号:US06444144B1

    公开(公告)日:2002-09-03

    申请号:US09671094

    申请日:2000-09-27

    IPC分类号: C09K1506

    CPC分类号: C07D307/62

    摘要: Provided with a novel ascorbic acid derivative represented by the formula (I) and a method for preparing the same: wherein R1 and R2 are different from each other and, independently H or —CH2CH2—(O—CH2—CH2)n—OR3, wherein n is an integer from 2 to 400; and R3 is a lower alkyl group having 1 to 10 carbon atoms. The novel ascorbic acid derivatives of this invention have excellent characteristics such as long-lasting anti-oxidation effect, high solubility in both water and organic solvents, and high stability in an aqueous solution. Furthermore, the novel ascorbic acid derivatives are useful for feed, food, cosmetic and pharmaceutical products due to their low toxicity and high thermal stability.

    摘要翻译: 提供由式(I)表示的新型抗坏血酸衍生物及其制备方法:其中R1和R2彼此不同,独立地为H或-CH2CH2-(O-CH2-CH2)n-OR3, 其中n是2至400的整数; 并且R 3是具有1至10个碳原子的低级烷基。 本发明的新型抗坏血酸衍生物具有优异的特性,如持久的抗氧化效果,在水和有机溶剂中的高溶解度,以及在水溶液中的高稳定性。 此外,新型抗坏血酸衍生物由于其低毒性和高热稳定性而可用于饲料,食品,化妆品和药物产品。