摘要:
There is provided an aluminum alloy casting consisting essentially of 7.0 to 11.5 mass % of Si, 0.9 to 4.0 mass % of Mg, 0.1 to 0.65 mass % of Fe, 0.1 to 0.8 mass % of Mn and the balance being Al and unavoidable impurities, or consisting essentially of 7.0 to 11.5 mass % of Si, 0.9 to 4.0 mass % of Mg, 0.1 to 0.65 mass % of Fe, 0.1 to 0.8 mass % of Mn, 0.3 to 1.0 mass % of Cu and the balance being Al and unavoidable impurities, and containing eutectic Si grains having an aspect ratio of 2.0 or smaller and an average grain size of 1.0 micrometer or smaller. There is also provided an automotive part formed with the aluminum alloy casting and a production method of the aluminum alloy casting.
摘要:
There is provided an aluminum alloy casting consisting essentially of 7.0 to 11.5 mass % of Si, 0.9 to 4.0 mass % of Mg, 0.1 to 0.65 mass % of Fe, 0.1 to 0.8 mass % of Mn and the balance being Al and unavoidable impurities, or consisting essentially of 7.0 to 11.5 mass % of Si, 0.9 to 4.0 mass % of Mg, 0.1 to 0.65 mass % of Fe, 0.1 to 0.8 mass % of Mn, 0.3 to 1.0 mass % of Cu and the balance being Al and unavoidable impurities, and containing eutectic Si grains having an aspect ratio of 2.0 or smaller and an average grain size of 1.0 micrometer or smaller. There is also provided an automotive part formed with the aluminum alloy casting and a production method of the aluminum alloy casting.
摘要:
In joining members to be joined (1, 1) by heating the members to be joined (1, 1) that are mated with intervening an insert (2) while applying opposing loads to the members to be joined (1, 1), so as to allow eutectic reaction to occur between the members to be joined (1, 1) and the insert (2) to discharge a eutectic melt from a joining plane along with an oxide film (1a) of the members to be joined, the members to be joined (1) are brought into contact with the insert (2) so that the oxide film (1a) is broken by a stress concentrating means previously provided at least one of joining portions breaks to produce a starting point of the eutectic reaction.
摘要:
Disclosed is a bonding method for dissimilar materials made from metals and its resulting structures. The materials to be bonded are formed by layering three or more sheets such that a dissimilar material interface and a same material interface are formed. A first current is conducted between a three-sheet layered plate material wherein an aluminum alloy plate, a zinc plated steel plate and a bare steel plate, for example, are layered in order. A nugget is formed in an interface between the zinc plated steel plate and the bare steel plate, which are the same materials. Then, a second current greater than the first current is conducted, and a nugget is formed in an interface between the aluminum alloy plate and the zinc plated steel plate.
摘要:
In joining a magnesium alloy material 1 (first material) and a steel material (second material), a zinc-plated steel plate 2 plated with zinc (metal C) is used as a steel material, Al (metal D) is added to the magnesium alloy material 1. Next, eutectic melting of Mg and Zn is caused so as to remove a product produced by the eutectic melting with an oxide film 1f and impurities from a joint interface. Moreover, an Al—Mg system intermetallic compound such as Al3Mg2 and an Fe—Al system intermetallic compound such as FeAl3 are produced, whereby regenerated surfaces of both materials 1 and 2 are joined via a compound layer 3 containing those intermetallic compounds.
摘要:
Disclosed herein are bonded structures and methods of forming the same. One embodiment of a bonded structure comprises first and second metallic layers and a bonding interface between the first and second metallic layers formed by diffusion and comprising a layer of at least one intermetallic compound. The intermetallic compound layer is formed in an area 52% or greater of an area of the bonding interface and has a thickness of 0.5 to 3.2 μm.
摘要:
According to a metal joining method of the present invention, first and second dissimilar metals are joined together by interposing between the first and second metal materials a third metal material dissimilar to the first and second metal materials and causing eutectic melting at least either at an interface between the first and third metal materials or at an interface between the second and third metal materials.
摘要:
In joining a magnesium alloy material 1 (first material) and a steel material (second material), a zinc-plated steel plate 2 plated with zinc (metal C) is used as a steel material, Al (metal D) is added to the magnesium alloy material 1. Next, eutectic melting of Mg and Zn is caused so as to remove a product produced by the eutectic melting with an oxide film 1f and impurities from a joint interface. Moreover, an Al—Mg system intermetallic compound such as Al3Mg2 and an Fe—Al system intermetallic compound such as FeAl3 are produced, whereby regenerated surfaces of both materials 1 and 2 are joined via a compound layer 3 containing those intermetallic compounds.
摘要:
Embodiments of the present invention provide a data group for each parameter that is classified into a first group and a second group, based on the performance of the products, a base point of a distribution of the data group is calculated, based on the distribution, and a distance range from the base point is decided. The number of data within this range belonging to the first group is counted and substituted for variable FX, the number of data belonging to the second group is counted and substituted for variable SX, the number of data outside this certain range belonging to the first group is counted and substituted for variable FY, and the number of data belonging to the second group is counted and substituted for variable SY. Moreover, a failure content ratio is calculated from variables FX, FY, SX and SY, and the yield impact is calculated.
摘要:
In joining members to be joined (1, 1) by heating the members to be joined (1, 1) that are mated with intervening an insert (2) while applying opposing loads to the members to be joined (1, 1), so as to allow eutectic reaction to occur between the members to be joined (1, 1) and the insert (2) to discharge a eutectic melt from a joining plane along with an oxide film (1a) of the members to be joined, the members to be joined (1) are brought into contact with the insert (2) so that the oxide film (1a) is broken by a stress concentrating means previously provided at least one of joining portions breaks to produce a starting point of the eutectic reaction.