摘要:
In accordance with the invention, containers or interfaces having two surfaces 201a and 201b to be joined, and a region to be sealed, are fused by providing between the surfaces 201a and 201b a thin strip or wire of RCM 102 embedded within a fusible material 101, applying pressure 205 and igniting the RCM 102. The released energy from the ignited RCM 102 results in a melting of the fusible material 101 and subsequent bonding of the fusible material 101 upon cooling to the 101 surrounding surfaces 201a and 201b, achieving a hermetic seal there between without the use of a separate gasket component.
摘要:
Applicants have discovered new composite materials and have developed a variety of new ways of making reactive composite materials (RCMs) and methods of controlling the properties and characteristics of the materials that are pertinent to numerous new or improved applications. This patent application is directed to new and improved ways of making reactive composite materials using mechanical deformation and making such materials with controlled, predictable characteristics. This application is also directed toward useful applications of the resulting materials.In accordance with the invention, RCMs are fabricated by a series of mechanical deformation steps. In the first deformation step, an assembly of reactive layers and/or particles is plastically deformed to reduce its cross sectional area by one-half or more. This severe initial deformation substantially eliminates the tendency of deformed layers to delaminate and eliminates the necessity of using specially cleaned metal layers. Portions of the deformed sheets are stacked or bent into a new assembly, and the new assembly is then deformed. The steps of assembly and deformation are repeated a sufficient number of times that the resulting materials are only locally layered but have relatively uniform reaction velocity and heat generating characteristics predictable by stochastic models derived herein. The resulting product is a controllable, locally layered reactive composite material (LLRCM) that can be fabricated quickly and is useful in a wide variety of applications.
摘要:
Novel reactive composite materials and associated methods for making the same which are pertinent to numerous new or improved applications. The method for making the reactive composite materials utilizes mechanical deformation to manufacture such materials with controlled, predictable characteristics. In the first deformation step, an assembly of reactive layers and/or particles is plastically deformed to reduce its cross sectional area by one-half or more. Portions of the deformed sheets are stacked or bent into a new assembly, and the new assembly is then deformed. The steps of assembly and deformation are repeated a sufficient number of times that the resulting materials are only locally layered but have relatively uniform reaction velocity and heat generating characteristics predictable by stochastic models derived herein.
摘要:
Applicants have discovered that electrostatic discharge (ESD) may, in some circumstances, result in current densities sufficient to ignite unprotected reactive composite materials. They have further discovered that a reactive composite material (RCM) can be protected from ESD ignition without adversely affecting the desirable properties of the RCM by the application of conducting and/or insulating materials at appropriate locations on the RCM. Thus ESD-protected RCM structures can be designed for such sensitive applications as ignition of propellants, generation of light bursts, and structural materials for equipment that may require controlled self-destruction.
摘要:
Applicants have discovered that electrostatic discharge (ESD) may, in some circumstances, result in current densities sufficient to ignite unprotected reactive composite materials. They have further discovered that a reactive composite material (RCM) can be protected from ESD ignition without adversely affecting the desirable properties of the RCM by the application of conducting and/or insulating materials at appropriate locations on the RCM. Thus ESD-protected RCM structures can be designed for such sensitive applications as ignition of propellants, generation of light bursts, and structural materials for equipment that may require controlled self-destruction.
摘要:
A method for bonding a concentrating photovoltaic receiver module to a heat sink using a reactive multilayer foil as a local heat source, together with layers of solder, to provide a high thermal conductivity interface with long term reliability and ease of assembly.
摘要:
The invention includes a method of joining two components. The method includes providing at least two components to be joined, a reactive multilayer foil, and a compliant element, placing the reactive multilayer foil between the at least two components, applying pressure on the two components in contact with the reactive multilayer foil via a compliant element, and initiating a chemical transformation of the reactive multilayer foil so as to physically join the at least two components. The invention also includes two components joined using the aforementioned method.
摘要:
The invention includes a method of joining two components. The method includes providing at least two components to be joined, a reactive multilayer foil, and a compliant element, placing the reactive multilayer foil between the at least two components, applying pressure on the two components in contact with the reactive multilayer foil via a compliant element, and initiating a chemical transformation of the reactive multilayer foil so as to physically join the at least two components. The invention also includes two components joined using the aforementioned method.
摘要:
The present inventors have observed that in some applications of reactive composite joining there is escape of a portion of the molten joining material through the edges of the joining regions. Such escape is not only a waste of expensive material (e.g. gold or indium) but also a reduction from the optimal thickness of the joining regions. In some applications, such escape also presents risk of short circuits or even fire. In this invention, two approaches are taken toward preventing damage to surroundings by the escape of molten joining material. First, escape may be prevented by trapping or containing the molten material near the joint, using barriers, dams, or similar means. Second, escape may be reduced by adjusting parameters within the joint, such as solder composition, joining pressure, or RCM thickness.
摘要:
Embodiments of the invention include a method for sealing a container. The method includes, providing at least two components of the container, positioning a crushable material between the at least two components, positioning a reactive multilayer material between the at least two components, deforming the crushable material so as to form a seal between the at least two components, chemically transforming the reactive multilayer material so as to join the at least two components.