Latex composition
    2.
    发明授权

    公开(公告)号:US11118038B2

    公开(公告)日:2021-09-14

    申请号:US16337244

    申请日:2017-09-19

    申请人: ZEON CORPORATION

    摘要: A latex composition containing a conjugated diene polymer latex and a medium-chain fatty acid glyceride, wherein a content proportion of the medium-chain fatty acid glyceride is 1 to 40 parts by weight with respect to 100 parts by weight of the conjugated diene polymer. In the present invention, a medium-chain fatty acid forming the medium-chain fatty acid glyceride is preferably a fatty acid having 6 to 18 carbon atoms. In the present invention, the medium-chain fatty acid glyceride is preferably a medium-chain fatty acid triglyceride. The latex composition preferably further contains a crosslinking agent.

    Method for manufacturing polymer latex

    公开(公告)号:US11034799B2

    公开(公告)日:2021-06-15

    申请号:US16077612

    申请日:2017-02-16

    申请人: ZEON CORPORATION

    摘要: A method for producing a polymer latex, including an emulsification step of mixing a polymer solution obtained by dissolution of synthetic polyisoprene and/or a styrene-isoprene-styrene block copolymer in an organic solvent, with an aqueous solution including 0.1 to 30 parts by weight of a rosinate based on 100 parts by weight in total of the synthetic polyisoprene and the styrene-isoprene-styrene block copolymer, and emulsifying the resultant in water to thereby obtain an emulsified liquid, a solvent removal step of removing the organic solvent in the emulsified liquid, and a concentration step of concentrating the emulsified liquid from which the organic solvent is removed, and also adjusting the content rate of the rosinate in the emulsified liquid after concentration, in the range of 0.1 to 3 parts by weight based on 100 parts by weight in total of the synthetic polyisoprene and the styrene-isoprene-styrene block copolymer in the emulsified liquid.

    Polymer latex production method
    7.
    发明授权

    公开(公告)号:US10934399B2

    公开(公告)日:2021-03-02

    申请号:US16071997

    申请日:2017-01-26

    申请人: ZEON CORPORATION

    摘要: A method for producing a polymer latex, including an emulsification step of emulsifying a polymer solution obtained by dissolution of synthetic polyisoprene and/or a styrene-isoprene-styrene block copolymer having a molecular weight distribution of 1.0 to 2.6 in an organic solvent, in water in the presence of a surfactant, to thereby obtain an emulsified liquid, wherein as the synthetic polyisoprene and/or styrene-isoprene-styrene block copolymer, used are/is synthetic polyisoprene and/or a styrene-isoprene-styrene block copolymer which, when dissolved in an organic solvent to thereby be formed into a polymer solution having a viscosity at a temperature of 60° C. of 20,000 cps, have/has a solid content concentration in the range of 10 to 60% by weight.

    Polymer latex production method
    8.
    发明授权

    公开(公告)号:US10759926B2

    公开(公告)日:2020-09-01

    申请号:US16071921

    申请日:2017-01-26

    申请人: ZEON CORPORATION

    摘要: A polymer latex, including a polymerization step of polymerizing a monomer in organic solvent to thereby obtain polymer solution of synthetic polyisoprene and/or styrene-isoprene-styrene block copolymer, antioxidant addition step of adding antioxidant to the polymer solution of synthetic polyisoprene and/or styrene-isoprene-styrene block copolymer at proportion of 0.01-1.00 parts by weight per 100 parts by weight of the synthetic polyisoprene and/or styrene-isoprene-styrene block copolymer, and emulsification step of emulsifying the polymer solution which the antioxidant is added, in water in the presence of a surfactant, to thereby obtain polymer latex, wherein the emulsification performs in the emulsification step so the ratio D75/D25 of the volume particle size D75 at a cumulative frequency of 75% to the volume particle size D25 at a cumulative frequency of 25% of a particle of the synthetic polyisoprene and/or styrene-isoprene-styrene block copolymer included in the polymer latex is 1.90 or more and 2.30 or less.