INFRARED REFLECTION METHOD
    3.
    发明申请
    INFRARED REFLECTION METHOD 审中-公开
    红外反射方法

    公开(公告)号:US20120009416A1

    公开(公告)日:2012-01-12

    申请号:US13257005

    申请日:2010-02-26

    Abstract: An infrared reflection method includes the steps of: preparing an object to be coated; and applying a coloring composition containing an infrared reflective pigment to the object to obtain a black coated object, the infrared reflective pigment having a structure including a metallic substrate, a metal oxide interference layer covering a surface of the metallic substrate, and metallic particles partially covering a surface of the metal oxide interference layer.

    Abstract translation: 红外反射方法包括以下步骤:准备待涂覆的物体; 以及将含有红外线反射颜料的着色组合物施加到所述物体上以获得黑色涂覆物体,所述红外线反射颜料具有包括金属基底,覆盖所述金属基底表面的金属氧化物干涉层和部分覆盖的金属颗粒的结构 金属氧化物干涉层的表面。

    Faux Finish and Process for Applying and Creating a Faux Finish
    4.
    发明申请
    Faux Finish and Process for Applying and Creating a Faux Finish 审中-公开
    虚拟完成和应用和创建虚拟完成的过程

    公开(公告)号:US20130017331A1

    公开(公告)日:2013-01-17

    申请号:US13181008

    申请日:2011-07-12

    Applicant: Raymond Sandor

    Inventor: Raymond Sandor

    Abstract: A process for applying a faux finish includes the steps of applying a textured paint to a surface as a base coat, the textured paint having approximately 250 grams to approximately 500 grams of pumice per liquid gallon of paint, allowing the applied textured paint to dry on the surface, randomly applying to the dried textured paint a wet slurry composition, partially drying the applied wet composition, and dry brushing the partially dried composition about the dried textured paint to create a faux effect on the surface. The wet slurry composition comprises concentrations of approximately 40% to approximately 70% by volume of water, approximately 0.2% to approximately 0.5% by volume of methylcellulose, approximately 15% to approximately 25% by volume of acrylic resin, and approximately 15% to approximately 25% by volume of mica particles having a mesh size of between approximately 250 mesh and approximately 400 mesh.

    Abstract translation: 施用人造漆的方法包括以下步骤:将纹理涂料作为底涂层施加到表面上,纹理涂料每液体加仑油漆具有约250克至约500克浮石,允许施加的纹理漆干燥 表面随机地施加到干燥的纹理涂料上的湿浆料组合物,部分干燥所施加的湿组合物,以及干燥地将干燥的组合物刷干干燥的织构化涂料以在表面上产生人造影响。 湿浆料组合物包含约40体积%至约70体积%的水,约0.2%至约0.5体积%的甲基纤维素,约15体积%至约25体积%的丙烯酸树脂和约15%至约 25%体积的具有大约250目和大约400目之间的筛目尺寸的云母颗粒。

    PAINT FILMS WHICH HAVE EXCELLENT HEAT-RADIATING PROPERTIES, AND A METHOD FOR THEIR FORMATION
    5.
    发明申请
    PAINT FILMS WHICH HAVE EXCELLENT HEAT-RADIATING PROPERTIES, AND A METHOD FOR THEIR FORMATION 有权
    具有优异耐热性能的涂膜及其形成方法

    公开(公告)号:US20100129558A1

    公开(公告)日:2010-05-27

    申请号:US12514211

    申请日:2007-10-10

    Abstract: To provide paint films which have excellent heat-radiating properties and with which many colors with light colors in the main can be obtained. (Means of Resolution). A paint film which has excellent heat-radiating properties which comprises an undercoat paint film layer which contains from 1 to 20 mass % with respect to the total solid fraction of the paint film of carbon black and a top-coat paint film layer which contains 1 to 40 mass % with respect to the total solid fraction of the paint film of a pearl pigment and which does not contain aluminum powder and the paint film thickness of the top-coat paint film layer is from 11 to 50 μm which can be formed with a method of forming paint films which have excellent heat-radiating properties wherein an undercoat paint which contains from 1 to 20 mass % with respect to the total solid fraction of the paint film of carbon black is applied and hardened and an undercoat paint film layer is formed and then a top-coat paint which contains 1 to 40 mass % with respect to the total solid fraction of the paint film of a pearl pigment and which does not contain aluminum powder is applied over said undercoat paint film layer and hardened and a top-coat paint film layer of which the paint film thickness is from 11 to 50 μm is formed.

    Abstract translation: 为了提供具有优异的散热性能并且可以获得主要颜色的许多颜色的油漆膜。 (解决方法)。 具有优异的散热性的漆膜,其包含相对于炭黑的漆膜的总固体成分含有1〜20质量%的底涂漆膜层和含有1 相对于珠光颜料的漆膜的全部固体成分为40质量%,并且不含铝粉末,并且顶涂漆膜层的漆膜厚度为11〜50μm,可以与 形成具有优异的散热性的涂膜的方法,其中涂布含有相对于炭黑漆膜的总固体成分为1〜20质量%的底漆,硬化,底涂漆膜层为 然后在所述底涂层上施加相对于珠光颜料的漆膜的总固体成分含有1〜40质量%的不含铝粉末的面漆, 并且硬化,并且形成漆膜厚度为11至50μm的顶涂层漆层。

    Shining coating film formation method and coated article
    6.
    发明申请
    Shining coating film formation method and coated article 有权
    镀膜成膜方法和涂层制品

    公开(公告)号:US20090246545A1

    公开(公告)日:2009-10-01

    申请号:US12391335

    申请日:2009-02-24

    Abstract: There are provided: a method for forming a shining coating film which can form a coating film extremely excellent in a leveling property and a brightness with good workability and can also realize the reduction of environmental burden; and a coated article excellent in a design property obtained by this method. In a method comprising the steps of sequentially coating a shining material-containing solvent type first base coat coating, a shining material-containing solvent type second base coat coating and a top clear coating onto a base material and baking a formed multilayered coating film at the same time, an improvement is made so that the resin composition and coating nonvolatile concentration of the first and second base coat coatings and the amount of nonvolatiles in the first and second base coating films will have specific conditions.

    Abstract translation: 提供了一种形成能形成水平性极好的涂膜的亮光涂膜的方法和具有良好可加工性的亮度,并且还可以实现环境负担的降低; 以及通过该方法获得的设计特性优异的涂布制品。 在一种方法中,包括以下步骤:将含发光材料的溶剂型第一底涂层涂层,含发光材料的溶剂型第二底涂层涂层和顶部透明涂层依次涂覆到基材上并在其上烘烤形成的多层涂膜 同时,改进了第一和第二底涂层的树脂组合物和涂层不挥发物浓度以及第一和第二基底涂膜中的非挥发物的量将具有特定的条件。

    TWO-TONE PAINTING METHOD
    8.
    发明申请
    TWO-TONE PAINTING METHOD 审中-公开
    双音绘画方法

    公开(公告)号:US20080171145A1

    公开(公告)日:2008-07-17

    申请号:US11623186

    申请日:2007-01-15

    Abstract: A two-tone painting method includes applying a powder primer to a substrate, followed by a powder basecoat applied dry-on-dry onto the powder primer. The powder basecoat is preferably applied in the same painting booth as the powder primer, i.e., without curing the powder primer. The powder basecoat includes a flake additive, such as a mica flake or a metal flake, which prevents surface irregularities from forming in the powder primer and the powder basecoat as a result of not curing the powder primer before applying the powder basecoat. The substrate is then masked, and a second basecoat is applied. The masking is then removed and a clearcoat is applied. The second basecoat and the clearcoat are then cured simultaneously in an oven.

    Abstract translation: 双色涂布方法包括将粉末底漆涂布到基材上,然后将粉末底涂层干燥涂于粉末底漆上。 粉末底涂层优选应用于与粉末底漆相同的涂漆室,即不固化粉末底漆。 粉末底漆包括片状添加剂,例如云母片或金属片,其在施加粉末底漆之前防止粉末底漆和粉末底漆中的表面不规则形成,因为未固化粉末底漆。 然后掩蔽基底,并施加第二底涂层。 然后除去掩蔽物并施加透明涂层。 然后将第二底漆和透明涂料在烘箱中同时固化。

    Method of forming coating films
    9.
    发明授权
    Method of forming coating films 失效
    涂膜形成方法

    公开(公告)号:US5362521A

    公开(公告)日:1994-11-08

    申请号:US036407

    申请日:1993-03-24

    Abstract: The invention provides a method of forming a coating film by forming in sequence a pigmented base coat and a clear top coat on a substrate followed by finishing by the two-coat one-bake technique, the method being characterized by using, as a coating composition for pigmented base coat formation, a composition comprising, as essential components thereof,(1) an OH-containing resin,(2) an amino resin,(3) a polyorganosiloxane which has, on an average, at least two groups, per molecule, each selected from the class consisting of a silanol group and an alkoxysilane group and has a number average molecular weight of at least 1,000,(4) a metal chelate compound(5) a flaky metal powder and/or a mica powder, and(6) an organic solvent,and using, as a coating composition for clear top coat formation, a composition comprising, as essential components thereof,(1) an OH- and epoxy-containing base resin which further contains at least one group selected from the group consisting of a silanol group and a hydrolyzable group bound directly to a silicon atom,(2) a curing catalyst, and(3) an organic solvent.

    Abstract translation: 本发明提供了一种形成涂膜的方法,该方法通过在基材上依次形成着色底涂层和透明面漆,然后通过双涂层单烘烤技术进行精加工,该方法的特征在于使用作为涂料组合物 对于着色底涂层形成,包含作为其主要组分的组合物,(1)含OH树脂,(2)氨基树脂,(3)每分子平均具有至少两个基团的聚有机硅氧烷 各自选自由硅烷醇基和烷氧基硅烷基组成的类别,数均分子量为1,000以上,(4)金属螯合物(5)为片状金属粉末和/或云母粉末,( 6)有机溶剂,并且使用作为透明外涂层形成用涂料组合物的组合物,其包含作为其主要组分的组合物,(1)含OH-和环氧基的基础树脂,其还含有至少一种选自 由硅烷醇组成的组 (2)固化催化剂,和(3)有机溶剂。