摘要:
An object of the present invention is to provide a copper foil excellent in softening resistance performance which reduces decrease in tensile strength after heat treatment at about 350° C. to 400° C. In order to achieve the object, a surface-treated copper foil provided with a rust-proofing treatment layer on both surfaces of a copper foil in which a rust-proofing treatment layer is constituted by zinc alloy, and the either rust-proofing treatment layer is a zinc alloy layer having zinc amount of 20 mg/m2 to 1,000 mg/m2; and the copper foil contains one or two or more of small amount elements selected from carbon, sulfur, chlorine and nitrogen, and a sum amount thereof is 100 ppm or more is adopted.
摘要翻译:本发明的目的是提供一种耐软化性能优异的铜箔,其在约350℃〜400℃下热处理后的抗拉强度降低。为了达到上述目的,将表面处理铜箔 在由铜合金构成的防锈处理层的铜箔的两面上设有防锈处理层,防锈处理层为锌量为20mg / m 2的锌合金层 至1,000 mg / m2; 铜箔含有一种或两种以上选自碳,硫,氯和氮的少量元素,其总量为100ppm以上。
摘要:
A manufacturing method of a multilayer printed wiring board in which a copper foil with carrier foil consists of at least four layers, a carrier foil/a release layer/a heat-resistant metal layer/a copper foil layer is used; a supporting substrate is manufactured by laminating an insulating layer constituting material on the surface of the copper foil layer constituting the copper foil with carrier foil; a supporting substrate with build-up wiring layer is manufactured by forming a build-up wiring layer on the surface of the carrier foil constituting the copper foil with carrier foil in the supporting substrate; the resulted supporting substrate with build-up wiring layer is separated at the release layer to manufacture a multilayered laminate; the resulted multilayered laminate is processed a necessary procedures to manufacture a multilayer printed wiring board.
摘要:
A manufacturing method of a multilayer printed wiring board in which a copper foil with carrier foil consists of at least four layers, a carrier foil/a release layer/a heat-resistant metal layer/a copper foil layer is used; a supporting substrate is manufactured by laminating an insulating layer constituting material on the surface of the copper foil layer constituting the copper foil with carrier foil; a supporting substrate with build-up wiring layer is manufactured by forming a build-up wiring layer on the surface of the carrier foil constituting the copper foil with carrier foil in the supporting substrate; the resulted supporting substrate with build-up wiring layer is separated at the release layer to manufacture a multilayered laminate; the resulted multilayered laminate is processed a necessary procedures to manufacture a multilayer printed wiring board.
摘要:
An object of the present invention is to provide a copper foil excellent in softening resistance performance which reduces decrease in tensile strength after heat treatment at about 350° C. to 400° C. In order to achieve the object, a surface-treated copper foil provided with a rust-proofing treatment layer on both surfaces of a copper foil in which a rust-proofing treatment layer is constituted by zinc alloy, and the either rust-proofing treatment layer is a zinc alloy layer having zinc amount of 20 mg/m2 to 1,000 mg/m2; and the copper foil contains one or two or more of small amount elements selected from carbon, sulfur, chlorine and nitrogen, and a sum amount thereof is 100 ppm or more is adopted.
摘要翻译:本发明的目的是提供一种耐软化性能优异的铜箔,其在约350℃〜400℃下热处理后的抗拉强度降低。为了达到上述目的,将表面处理铜箔 在由铜合金构成的防锈处理层的铜箔的两面上设有防锈处理层,防锈处理层为锌量为20mg / m 2的锌合金层 至1,000 mg / m2; 铜箔含有一种或两种以上选自碳,硫,氯和氮的少量元素,其总量为100ppm以上。
摘要:
An object of the present invention is to provide a production method which enables efficient production of an electro-deposited copper foil with further lower profile when compared to the low-profile electro-deposited copper foils which have been supplied to the market and is excellent in mechanical strength. For the purpose of achieving the object, a production method adopted obtains the electro-deposited copper foil by electrolyzing a sulfuric acid based copper electrolytic solution which contains a quaternary ammonium salt polymer having cyclic structure and chlorine, wherein for the quaternary ammonium salt polymer contained in the sulfuric acid based copper electrolytic solution, a DDAC dimer or higher polymer is used. For the quaternary ammonium salt polymer, a diallyl dimethyl ammonium chloride polymer having a number average molecular weight of 300 to 10000 is preferably used. The sulfuric acid based copper electrolytic solution preferably contains bis(3-sulfopropyl) disulfide or 3-mercapto-1-propanesulfonic acid that is a compound having a mercapto group.
摘要:
A manufacturing method of a multilayer printed wiring board in which a copper foil with carrier foil consists of at least four layers, a copper foil layer/a release layer/a heat-resistant metal layer/a carrier foil is used; a supporting substrate is manufactured by laminating an insulating layer constituting material to the surface of the carrier foil constituting the copper foil with carrier foil; a supporting substrate with build-up wiring layer is manufactured by forming a build-up wiring layer on the surface of the copper foil layer constituting the copper foil with carrier foil in the supporting substrate; the resulted supporting substrate with build-up wiring layer is separated at the release layer to manufacture a multilayered laminate; the resulted multilayered laminate is processed a necessary procedures to manufacture a multilayer printed wiring board.
摘要:
A manufacturing method of a multilayer printed wiring board in which a copper foil with carrier foil consists of at least four layers, a copper foil layer/a release layer/a heat-resistant metal layer/a carrier foil is used; a supporting substrate is manufactured by laminating an insulating layer constituting material to the surface of the carrier foil constituting the copper foil with carrier foil; a supporting substrate with build-up wiring layer is manufactured by forming a build-up wiring layer on the surface of the copper foil layer constituting the copper foil with carrier foil in the supporting substrate; the resulted supporting substrate with build-up wiring layer is separated at the release layer to manufacture a multilayered laminate; the resulted multilayered laminate is processed a necessary procedures to manufacture a multilayer printed wiring board.
摘要:
An object of the present invention is to provide a method for preparing a sulfuric acid base copper electrolytic solution used for formation of an electro-deposited copper film comprising a surface excellent in smoothness and gloss when formed by using the solution just after preparation and is prepared by using mono-sulfides. To achieve the object, a sulfuric acid base copper electrolytic solution is made to contain a sulfonated active sulfur compound, the bis(3-sulfopropyl)disulfide which is recommended for formation of a glossy electro-deposited copper film. And the bis(3-sulfopropyl)disulfide contained is obtained by converting a 3-mercapto-1-propanesulfonic acid into the bis(3-sulfopropyl)disulfide in an aqueous solution of the 3-mercapto-1-propanesulfonic acid by an oxidation reaction. In the oxidation reaction, an air bubbling method is preferably used to prevent oxidative decomposition of the 3-mercapto-1-propanesulfonic acid.
摘要:
An object of the present invention is to provide a copper foil excellent in softening resistance performance which reduces decrease in tensile strength after heat treatment at about 350° C. to 400° C. In order to achieve the object, a surface-treated copper foil provided with a rust-proofing treatment layer on both surfaces of a copper foil in which a rust-proofing treatment layer is constituted by zinc, and the either rust-proofing treatment layer is a zinc layer having zinc amount of 20 mg/m2 to 1,000 mg/m2; and the copper foil contains one or two or more of small amount elements selected from carbon, sulfur, chlorine and nitrogen, and a sum amount thereof is 100 ppm or more is adopted.
摘要翻译:本发明的目的是提供一种耐软化性能优异的铜箔,其在约350℃〜400℃下热处理后的抗拉强度降低。为了达到上述目的,将表面处理铜箔 在由铜构成的防锈处理层的铜箔的两面上设有防锈处理层,任一防锈处理层为锌量为20mg / m 2〜1000的锌层 mg / m2; 铜箔含有一种或两种以上选自碳,硫,氯和氮的少量元素,其总量为100ppm以上。
摘要:
An object of the present invention is to provide a method for preparing a sulfuric acid base copper electrolytic solution used for formation of an electro-deposited copper film comprising a surface excellent in smoothness and gloss when formed by using the solution just after preparation and is prepared by using mono-sulfides. To achieve the object, a sulfuric acid base copper electrolytic solution is made to contain a sulfonated active sulfur compound, the bis(3-sulfopropyl)disulfide which is recommended for formation of a glossy electro-deposited copper film. And the bis(3-sulfopropyl)disulfide contained is obtained by converting a 3-mercapto-1-propanesulfonic acid into the bis(3-sulfopropyl)disulfide in an aqueous solution of the 3-mercapto-1-propanesulfonic acid by an oxidation reaction. In the oxidation reaction, an air bubbling method is preferably used to prevent oxidative decomposition of the 3-mercapto-1-propanesulfonic acid.