Photoacid generator, method for producing the same, and resist composition comprising the same
    1.
    发明授权
    Photoacid generator, method for producing the same, and resist composition comprising the same 有权
    光生酸产生剂,其制备方法和含有它的抗蚀剂组合物

    公开(公告)号:US08889901B2

    公开(公告)日:2014-11-18

    申请号:US13367762

    申请日:2012-02-07

    摘要: A photoacid generator represented by the following formula (1), a method for producing the photoacid generator, and a resist composition containing the photoacid generator are provided. wherein in the formula (1), Y, X, R1, R2, n1, n2 and A+ have the same meanings as defined in the detailed description of the invention. The photoacid generator can maintain an appropriate contact angle at the time of ArF liquid immersion lithography, can reduce defects occurring during liquid immersion lithography, and has excellent solubility in resist solvents and excellent compatibility with resins. Furthermore, the photoacid generator can be produced by an efficient and simple method using an epoxy compound that is industrially easily available.

    摘要翻译: 提供由下式(1)表示的光致酸发生剂,光酸产生剂的制造方法和含有光酸产生剂的抗蚀剂组合物。 其中,在式(1)中,Y,X,R1,R2,n1,n2和A +具有与本发明的详细说明中所定义的相同的含义。 光致酸发生器可以在ArF液浸光刻时保持适当的接触角,可以减少液浸光刻过程中发生的缺陷,并且在抗蚀剂溶剂中具有优异的溶解性和与树脂的相容性优异。 此外,光致酸产生剂可以通过使用工业上容易获得的环氧化合物的有效且简单的方法制备。

    Method of preparing positive active material for lithium battery
    2.
    发明授权
    Method of preparing positive active material for lithium battery 有权
    锂电池正极活性物质的制备方法

    公开(公告)号:US08585874B2

    公开(公告)日:2013-11-19

    申请号:US12625646

    申请日:2009-11-25

    IPC分类号: C23C14/34

    摘要: Disclosed is a method of preparing a positive active material for a lithium battery. The method comprises: depositing a positive active material on an electrode on a substrate (1); and putting metal chips on a metal oxides target and performing a sputtering process, thereby depositing mixed metal-oxides on the positive active material (2). In another aspect, the method comprises: preparing an electrode active material; preparing a precursor solution including the electrode active material; and printing the precursor solution on the substrate, and evaporating a solvent at a temperature of 80-120° C.

    摘要翻译: 公开了一种锂电池正极活性物质的制备方法。 该方法包括:在衬底(1)上的电极上沉积正极活性材料; 并将金属屑放在金属氧化物靶上并进行溅射工艺,从而在正极活性物质(2)上沉积混合的金属氧化物。 另一方面,该方法包括:制备电极活性材料; 制备包括电极活性材料的前体溶液; 并将前体溶液印刷在基材上,并在80-120℃的温度下蒸发溶剂。

    SULFONIUM COMPOUND, PHOTOACID GENERATOR, AND RESIST COMPOSITION
    3.
    发明申请
    SULFONIUM COMPOUND, PHOTOACID GENERATOR, AND RESIST COMPOSITION 有权
    磺化合物,光致发电机和耐腐蚀组合物

    公开(公告)号:US20130035503A1

    公开(公告)日:2013-02-07

    申请号:US13557893

    申请日:2012-07-25

    IPC分类号: C07C309/06

    摘要: A sulfonium compound represented by the following formula (1), a photoacid generator containing the sulfonium compound, and a resist composition containing the photoacid generator are provided: wherein X represents an electron donor group; R1 and R2 each independently represent an alkyl group or the like; R4 to R6 each independently represent an alkyl group, or the like; R3 represents a cyclic alkenediyl group or the like; and −A represents an anion. The sulfonium compound has a photon yield that is controllable by introducing different absorbers to the cation region in one molecule, can address the inconvenience of using a mixture of different photoacid generators when the sulfonium compound is applied as a photoacid generator, has excellent miscibility in a resist, and has enhanced resolution and line edge roughness.

    摘要翻译: 提供由下式(1)表示的锍化合物,含有锍化合物的光酸产生剂和含有光致酸发生剂的抗蚀剂组合物,其中X表示电子给体基团; R1和R2各自独立地表示烷基等; R4至R6各自独立地表示烷基等; R3表示环状亚烯基等; -A表示阴离子。 锍化合物具有通过在一个分子中向阳离子区域引入不同吸收剂可控制的光子产率,可以解决当将锍化合物用作光致酸发生剂时使用不同光酸产生剂的混合物的不便之处,在 抗蚀,并具有增强的分辨率和线边缘粗糙度。

    METHOD OF PREPARING POSITIVE ACTIVE MATERIAL FOR LITHIUM BATTERY
    5.
    发明申请
    METHOD OF PREPARING POSITIVE ACTIVE MATERIAL FOR LITHIUM BATTERY 有权
    制备锂电池正极活性材料的方法

    公开(公告)号:US20110056824A1

    公开(公告)日:2011-03-10

    申请号:US12625646

    申请日:2009-11-25

    IPC分类号: C23C14/34 B05D5/12

    摘要: Disclosed is a method of preparing a positive active material for a lithium battery. The method comprises: depositing a positive active material on an electrode on a substrate (1); and putting metal chips on a metal oxides target and performing a sputtering process, thereby depositing mixed metal-oxides on the positive active material (2). In another aspect, the method comprises: preparing an electrode active material; preparing a precursor solution including the electrode active material; and printing the precursor solution on the substrate, and evaporating a solvent at a temperature of 80-120° C.

    摘要翻译: 公开了一种锂电池正极活性物质的制备方法。 该方法包括:在衬底(1)上的电极上沉积正极活性材料; 并将金属屑放在金属氧化物靶上并进行溅射工艺,从而在正极活性物质(2)上沉积混合的金属氧化物。 另一方面,该方法包括:制备电极活性材料; 制备包括电极活性材料的前体溶液; 并将前体溶液印刷在基材上,并在80-120℃的温度下蒸发溶剂。

    Wireless mouse system containing a flash memory
    9.
    发明申请
    Wireless mouse system containing a flash memory 有权
    包含闪存的无线鼠标系统

    公开(公告)号:US20080048982A1

    公开(公告)日:2008-02-28

    申请号:US11605384

    申请日:2006-11-29

    IPC分类号: G09G5/08

    摘要: The present invention relates to a wireless mouse system. Particularly, the present invention relates to a wireless mouse system in which includes a controller, which controls a receiver and a flash memory device integrated into an interfacing device, can be performed function of the receiver and the flash memory device smoothly. A wireless mouse system comprises a wireless mouse and an interfacing device with a USB terminal, electrically communicated with a USB port of a information-displaying device. The interfacing device comprises a receiver receiving a signal data transferred wirelessly from the wireless mouse, and transferring the signal data to the information-displaying device, a flash memory device exchanging data with the information-displaying device through the USB terminal and a controller controlling the receiver and the flash memory device, and transferring optionally the signal of the receiver and the flash memory device to the information-displaying device.

    摘要翻译: 无线鼠标系统技术领域本发明涉及无线鼠标系统。 特别地,本发明涉及无线鼠标系统,其中包括控制接收机的控制器和集成到接口设备中的闪存设备,可以平滑地执行接收机和闪存设备的功能。 无线鼠标系统包括无线鼠标和具有USB端子的接口装置,与信息显示装置的USB端口电连通。 接口装置包括:接收器,接收从无线鼠标无线传送的信号数据,并将信号数据传送到信息显示装置,闪速存储装置通过USB终端与信息显示装置交换数据;控制器 接收机和闪存设备,并且可选地将接收机和闪存设备的信号传送到信息显示设备。

    Catalyst for partial oxidation of methylbenzenes, method for preparing the same, and method for producing aromatic aldehydes using the same
    10.
    发明申请
    Catalyst for partial oxidation of methylbenzenes, method for preparing the same, and method for producing aromatic aldehydes using the same 有权
    用于部分氧化甲基苯的催化剂,其制备方法以及使用其制备芳族醛的方法

    公开(公告)号:US20080021248A1

    公开(公告)日:2008-01-24

    申请号:US11603213

    申请日:2006-11-22

    IPC分类号: B01J23/30 C07C45/90

    摘要: A catalyst for gas phase oxidation of methylbenzenes in the presence of molecular oxygen to produce corresponding aromatic aldehydes, a method for preparing the catalyst, and a method for producing aromatic aldehydes from methylbenzenes by using the catalyst. The catalyst comprises a compound represented by the following formula (1): WaXbYcOx   (1) wherein W represents a tungsten atom, X represents one or more alkali metals selected from the group consisting of Li, Na, K, Rb, and Cs, Y represents one or more elements selected from the group consisting of Fe, Co, Ni, Cu, Mn, Re, Cr, V, Nb, Ti, Zr, Zn, Cd, Y, La, Ce, B, Al, Sn, Mg, Ca, Sr, and Ba, O stands for an oxygen atom, and the ratio of a:b:c is 12:0.001˜1:0˜5.

    摘要翻译: 用于在分子氧存在下甲基苯气相氧化以产生相应的芳族醛的催化剂,制备该催化剂的方法,以及通过使用该催化剂由甲基苯制备芳族醛的方法。 催化剂包含由下式(1)表示的化合物:<?in-line-formula description =“In-line formula”end =“lead”?> W (1)<?in-line-formula description =“In-line Formulas”end =“tail”?>其中W表示(x,y) 钨原子,X表示选自Li,Na,K,Rb和Cs中的一种以上的碱金属,Y表示选自Fe,Co,Ni,Cu,Mn, Re,Cr,V,Nb,Ti,Zr,Zn,Cd,Y,La,Ce,B,Al,Sn,Mg,Ca,Sr和Ba,O表示氧原子, b:c为12:0.001〜1:0〜5。