Backflow-preventing valves for injection-molding machines
    12.
    发明授权
    Backflow-preventing valves for injection-molding machines 失效
    注塑机防回流阀

    公开(公告)号:US4951920A

    公开(公告)日:1990-08-28

    申请号:US249125

    申请日:1988-09-26

    申请人: Nobuo Tsuno

    发明人: Nobuo Tsuno

    IPC分类号: B29C45/52 F16K25/00

    摘要: A backflow-preventing valve for use in a screw head of a screw injection-molding machine which has an annular shape and comprises a ceramic member is disclosed and a metallic member. At least a surface portion of a backflow-preventing valve which is brought into contact with a material to be injected and a screw groove or a valve seat is constituted by a ceramic material.

    摘要翻译: 公开了一种用于螺旋注射成型机的螺旋头的防回流阀,其具有环形形状并且包括陶瓷构件,并且具有金属构件。 至少与被注入材料接触的防回流阀的表面部分和螺纹槽或阀座由陶瓷材料构成。

    Metallizing paste and a process for metallizing ceramic articles by
using such a metallizing paste
    14.
    发明授权
    Metallizing paste and a process for metallizing ceramic articles by using such a metallizing paste 失效
    金属化糊料和通过使用这种金属化糊料对陶瓷制品进行金属化的方法

    公开(公告)号:US4822645A

    公开(公告)日:1989-04-18

    申请号:US105225

    申请日:1987-10-07

    摘要: Metallizing pastes are disclosed, which contain, as inorganic materials, 15 to 50% by weight of a component to form a glass phase and 50 to 85% by weight of a metallic molybdenum powder. The glass phase essentially consists of 5 to 25% by weight of Al.sub.2 O.sub.3, 35 to 55% by weight of SiO.sub.2 and 30 to 55% by weight of MnO. A process for metallizing ceramic members is also disclosed. The metallizing paste is applied to surfaces of the ceramic member and the dried. The ceramic member with the dried metallizing paste is then fired in a temperature range from 1,200.degree. to 1,400.degree. C. for 0.5 to 10 hours in a mixed gas of hydrogen gas and nitrogen gas in which a ratio in partial pressure between steam and hydrogen, (P.sub.H.sbsb.2.sub.O /P.sub.H.sbsb.2), is adjusted in a range from 10.sup.-6 to 10.sup.0.

    摘要翻译: 公开了金属化糊料,其包含作为无机材料的15至50重量%的组分以形成玻璃相和50至85重量%的金属钼粉末。 玻璃相基本上由5至25重量%的Al 2 O 3,35至55重量%的SiO 2和30至55重量%的MnO组成。 还公开了用于金属化陶瓷构件的方法。 将金属化糊料施加到陶瓷构件的表面并干燥。 然后,在氢气和氮气的混合气体中,在1200〜1400℃的温度范围内,将具有干燥金属化糊料的陶瓷构件烧成0.5〜10小时,其中蒸汽与氢气之间的分压比, (PH 2 O / PH 2)调整为10-6〜100的范围。

    Composite type magnetic head using composite metallic wire
    19.
    发明授权
    Composite type magnetic head using composite metallic wire 失效
    复合型磁头采用复合金属丝

    公开(公告)号:US06180890B2

    公开(公告)日:2001-01-30

    申请号:US09548336

    申请日:2000-04-12

    IPC分类号: H01B500

    摘要: A composite metallic wire includes: an inner layer having a cross-sectional shape of a rough circle; and a metal outer layer having a cross-sectional shape of a rough ring; wherein the composite metallic wire has a diameter of 15 &mgr;m or less and an electric resistance of 300 &OHgr;/m or less. A composite type magnetic head using as a coil wire a composite wire comprising: (1) a composite metallic wire comprising: an inner layer having a cross-sectional shape of a rough circle; and a metal outer layer having a cross-sectional shape of a rough ring; wherein the composite metallic wire has a diameter of 15 &mgr;m or less and an electric resistance of 300 &OHgr;/m or less, and (2) an insulating coat provided in the outer periphery of the outer layer.

    摘要翻译: 复合金属线包括:具有粗圆的横截面形状的内层; 以及具有粗环的横截面形状的金属外层; 所述复合金属线的直径为15μm以下,电阻为300Ω/ m以下。 一种复合型磁头,其使用作为线圈线的复合线,其包括:(1)复合金属线,其包括:具有粗圆的横截面形状的内层; 以及具有粗环的横截面形状的金属外层; 其中复合金属线的直径为15μm或更小,电阻为300欧姆/米或更小,和(2)设置在外层外周的绝缘涂层。