摘要:
A method of producing a stretched film comprising melt-coextruding a thermoplastic resin A and a thermoplastic resin B to produce a composite film 1 having both-end films 2 of the thermoplastic resin B arranged in parallel at both end portions of the main film 1a of the thermoplastic resin A in the direction of width thereof, stretching the composite film, and cutting and removing both end portions of the stretched film in the direction of width, wherein a film stretch stress value of the both-end films 2 is larger than a film stretch stress value of the main film 1a at the same stretching ratio. This minimizes an increase in the thickness at both end portions of the film in stretching the film and decreases the widths by which both end portions of the expensive resin film are to be cut and removed for producing a film.
摘要:
Disclosed are a method and an apparatus for forming an oxide coating film with excellent corrosion resistance and adhesiveness on a cathode made of a metal plate by a simple process at low cost. A direct current voltage is applied between an anode (12) and a cathode (13) in an electrolyte solution which cathode (13) is made of a metal plate to be coated with oxide and arranged opposite to the anode (12), while supplying oxygen or a gas containing oxygen into the electrolyte solution, so that the metal plate cathode (13) is coated with oxide, thereby being formed into a oxide-coated metal plate.
摘要:
A method for manufacturing a resin-coated metal sheet comprising: laminating two or more kinds of molten resins, to form a multilayer film; extruding the multilayer film through a multi-manifold die onto a metal sheet; wherein at least one kind of molten resin contains a coloring component; wherein said molten resins include a first resin having a high melt viscosity and a second resin having a low melt viscosity; wherein the multi-manifold die has plural resin passages through which plural resins pass; wherein the resin passage through which the first resin passes is maintained at a higher temperature than the resin passage through which the low melt viscosity resin passes; wherein the difference in melt viscosity of adjoining resin layers is 3,000 poises or less at a shear rate of 20 to 500 s−1; wherein the molten resin containing a coloring component has a melt tension Tm in the range of 0.5 g≧1.0 g, and a thickness of the layer of the resin containing a coloring component is equal to one-third or more of the total thickness of the resin coating.
摘要:
A preventive film for a polarizer which comprises a non-oriented three-layer film comprising a polycarbonate film having a glass transition temperature or 100° C. or higher and, laminated on both surfaces thereof, a polybutylene terephthalate film: a releasable preventive film for a polarizing film which comprises the three-layer film and, applied on the surface of the polybutylene terephthalate film side, a silicon based releasing agent; and a polarizing plate preventive film for a polarizing film and the releasable preventive film for a polarizing film as uppermost surface layers of a polarizing film containing a polarizer. The preventive film for a polarizing film and the releasable preventive film for a polarizing film exhibit an extremely small double refraction and can be produced at a low cost, and the polarizing plate using these films allows the detection of optical defects with ease.
摘要:
A manufacturing method and apparatus of an organic resin coated metal sheet is provided. Temperatures of edge portions of the metal sheet and a temperature of an approximately central portion of the metal sheet are respectively measured using a metal-sheet temperature measuring device arranged directly upstream of lamination rolls. Respectively measured temperature values are inputted to a heating temperature controller, and output values calculated by the heating temperature controllers are inputted to a metal sheet center portion heater and the metal sheet center portion heater, respectively, to control the heating of a widthwise approximately center portion and edge portion, respectively, to a first and second temperature, respectively, the second temperature being higher than the first. A resin film is extruded to pre-rolls and is sandwiched and pressure-bonding to the metal sheet between a pair of lamination rolls. Resin portions projecting from both edge portions are then removed.
摘要:
The present invention aims at the continuous and stable production of an organic-resin-coated metal sheet in producing the organic-resin-coated metal sheet by an extrusion method using a laminating roll which can prevent resin portions (ear portions) protruding from the metal sheet being wound around shaft portions of the laminating roll. Using a laminating roll in which a width (A) of a region thereof coated with a lining material satisfies a relationship of 0≦A−B≦20 mm with respect to a width (B) of the metal sheet, a thermally melted organic resin is extruded and is applied to the metal sheet such that end portions of the organic resin in the widthwise direction protrude from outer portions of the laminating roll applied with the lining material, and the resin portions in a semi-molten state which protrude from respective edges of the metal sheet are removed by press-cutting.
摘要:
Disclosed are a method and an apparatus for forming an oxide coating film with excellent corrosion resistance and adhesiveness on a cathode made of a metal plate by a simple process at low cost. A direct current voltage is applied between an anode (12) and a cathode (13) in an electrolyte solution which cathode (13) is made of a metal plate to be coated with oxide and arranged opposite to the anode (12), while supplying oxygen or a gas containing oxygen into the electrolyte solution, so that the metal plate cathode (13) is coated with oxide, thereby being formed into a oxide-coated metal plate.
摘要:
A polarizer protective film of the present invention comprises a thermoplastic resin layer having a moisture permeability of 100 g/m2/24 hours or less; and a resin layer that comprises a copolymer containing a styrene monomer unit and is laminated on the thermoplastic resin layer through an adhesive resin layer. The polarizer protective film can have good adhesion to a polarizer when it is bonded to the polarizer through an adhesive layer to form a polarizing plate, and can form a polarizing plate with good polarization properties.
摘要翻译:本发明的偏振片保护膜包含透湿度为100g / m 2/24小时以下的热塑性树脂层, 以及包含含有苯乙烯单体单元的共聚物并通过粘合树脂层层压在热塑性树脂层上的树脂层。 偏振片保护膜通过粘接层与偏振片接合而形成偏光板时,可以对偏振片具有良好的粘附性,可以形成具有良好的偏振特性的偏光板。
摘要:
A method for producing a multi-layer resin film, wherein a plurality of molten resins being different in the melt viscosity are laminated on the surface of a film containing at least one resin containing a coloring component without formation of irregularities; and a method for producing a metal sheet having a resin coating film which comprises laminating said film on a metal sheet. The above method for producing a multi-layer resin film comprises keeping the temperatures of an extruder, a manifold and a dye portion adjacent to the manifold for the pass of a resin having a higher melt viscosity at a level higher than those of the temperatures of an extruder, a manifold and a dye portion adjacent to the manifold for the pass of a resin having a lower melt viscosity, to thereby reduce the difference in the melt viscosities of adjacent resin layers to 3000 poise or less at a shear rate of 20 to 500 sec−1, and laminating respective molten resins while adjusting a resin containing a coloring component so as to have 0.5 g≦Tm≦1.0 g, wherein Tm represents a melt strength, and a thickness of one half of the total thickness or more or having Tm≧1.0 g and a thickness of one third of the total thickness or more, to thereby form a multi-layer film.
摘要:
Provided are a multilayer film with small surface unevenness, constructed from resin layers with different molten viscosities: a resin-coated metal plastic, formed by layering a multilayer resin film on a metal plate: a method reproducing a multilayer resin film by layering molten resins with different molten viscosities without forming unevenness on the surface of the film; and a method of producing a resin-coated metal plate. The difference in molten viscosities or adjacent resin layers is set to 3000 poise or lower at a shear rate of 20 to 500 s−1, with the temperature of an extruder, a manifold, and that part of a die which is adjacent to the manifold through which of these a resin with a high molten viscosity passes maintained higher than the temperature of an extruder, a manifold, and that part or a die which is adjacent to the manifold through which of these a resin with a low molten viscosity passes. After that, the individual molten resins are layered on each other to form a multilayer film such that the thickness of a resin whose molten tensile force is 1 g or greater is one third or more of the total thickness.