Abstract:
The object of the present invention is to provide a curable composition for forming a cured product having high tensile strength and high elongation. A polyurethane curable composition of the present invention contains a polyol (A) and a polyisocyanate (B) as an essential component, wherein the composition contains polymer fine particles (C) having a core-shell structure including at least two layers of a core layer and a shell layer, the polymer fine particles (C) are contained in an amount of 1 to 150 parts by mass per 100 parts by mass of a total amount of the polyol (A) and the polyisocyanate (B), the core layer has a glass transition temperature (Tg) of more than 0° C. as calculated by the following numerical formula (1), a cured product formed by the curable composition has an elongation of more than 47% at a maximum tensile stress, 1/Tg=Σ(Mi/Tgi) (1) wherein Mi represents a weight fraction of a non-crosslinking monomer i constituting the core layer of the polymer fine particles (C), Tgi represents a glass transition temperature (K) of a homopolymer polymerized with the non-crosslinking monomer i, and i represents an integer of 1 or more.
Abstract:
Provided are a waterproof coating material and a roof having a coating film formed therefrom which have low VOC content, good film curability under low-temperature/high-humidity conditions, high stain resistance, and low water absorbency. The coating material comprises: (A) 100 parts by weight of a polyoxyalkylene polymer (a1) and/or a vinylic polymer (a2), the polymers each containing a reactive silyl group of formula (1): —SiR13-aXa (1) wherein each R1 independently represents a C1-C20 alkyl, C6-C20 aryl, or C7-C20 aralkyl group, or a triorganosiloxy group of (R′)3SiO— where R's each independently represent a C1-C20 substituted or unsubstituted hydrocarbon group; each X independently represents a hydroxy or hydrolyzable group; and a represents 1, 2 or 3; and (B) 0.1-20 parts by weight of at least one compound including a compound (b3) obtained by partial condensation of silyl groups of an aminosilane alone or of a combination of an aminosilane and another alkoxysilane compound.
Abstract:
The object of the present invention is to provide a curable composition for forming a cured product having high tensile strength and high elongation. A polyurethane curable composition of the present invention contains a polyol (A) and a polyisocyanate (B) as an essential component, wherein the composition contains polymer fine particles (C) having a core-shell structure including at least two layers of a core layer and a shell layer, the polymer fine particles (C) are contained in an amount of 1 to 150 parts by mass per 100 parts by mass of a total amount of the polyol (A) and the polyisocyanate (B), the core layer has a glass transition temperature (Tg) of more than 0° C. as calculated by the following numerical formula (1), a cured product formed by the curable composition has an elongation of more than 47% at a maximum tensile stress, 1/Tg=Σ(Mi/Tgi) (1) wherein Mi represents a weight fraction of a non-crosslinking monomer i constituting the core layer of the polymer fine particles (C), Tgi represents a glass transition temperature (K) of a homopolymer polymerized with the non-crosslinking monomer i, and i represents an integer of 1 or more.
Abstract:
The present invention relates to a curable resin composition comprising a polyol (A) having an average hydroxyl value of 200 to 1500 mg KOH/g, a polyisocyanate (B), and polymer fine particles (C), and a curable resin composition comprising a polyol (A), a polyisocyanate (B), and polymer fine particles (C), wherein the polyol (A) comprises a polyester polyol (a2) as an essential component, and the amount of the polyester polyol (a2) is not less than 20 parts by mass per 100 parts by mass of the polyol(A).
Abstract:
A resin composition contains polymer particles (A) and a matrix resin (B) such that the polymer particles (A) have a graft part having a glass transition temperature of −25° C. to 18° C. The resin composition has excellent handleability.
Abstract:
One or more embodiments of the present invention provide an adhesion method that provides excellent workability by using a curable resin composition whose viscosity has low temperature dependence. The method of adhesion includes a step of applying a curable resin composition, a step of spreading the curable resin composition, and a step of curing the curable resin composition. The curable resin composition contains specific amounts of an epoxy resin, fine polymer particles whose shell layers have a cyano group in a specific amount, and blocked urethane.
Abstract:
The present invention relates to a curable resin composition comprising a polyol (A) having an average hydroxyl value of 200 to 1500 mg KOH/g, a polyisocyanate (B), and polymer fine particles (C), and a curable resin composition comprising a polyol (A), a polyisocyanate (B), and polymer fine particles (C), wherein the polyol (A) comprises a polyester polyol (a2) as an essential component, and the amount of the polyester polyol (a2) is not less than 20 parts by mass per 100 parts by mass of the polyol (A).
Abstract:
The present invention relates to a curable resin composition comprising a polyol (A) having an average hydroxyl value of 200 to 1500 mg KOH/g, a polyisocyanate (B), and polymer fine particles (C), and a curable resin composition comprising a polyol (A), a polyisocyanate (B), and polymer fine particles (C), wherein the polyol (A) comprises a polyester polyol (a2) as an essential component, and the amount of the polyester polyol (a2) is not less than 20 parts by mass per 100 parts by mass of the polyol (A).
Abstract:
The present invention relates to a curable resin composition containing 100 parts by mass of an epoxy resin (A), 1 to 100 parts by mass of polymer fine particles (B), and 1 to 100 parts by mass of a blocked urethane (C), wherein the polymer fine particles have a core-shell structure of a core layer and a shell layer, the core layer contains diene rubber, the shell layer contains at least a hydroxyl group, and the content of the hydroxyl group of the polymer fine particles (B) is 0.01 to 0.8 mmol/g.
Abstract:
An object of the present invention is to provide a curable composition that can be used as sealing materials, adhesives, and the like, has excellent curing properties, and gives a cured product excellent in elongation properties. The object can be attained by means of a curable composition comprising: a reactive silyl group-containing polyether polymer (A) that contains a reactive silyl group with high activity (e.g., (ClCH2)(CH3O)2Si—, (CH3OCH2)(CH3O)2Si—, or CH3(CH3O)2Si—CH2—NH—C(═O)—); and a reactive silyl group-containing polyether polymer (B) that contains a reactive silyl group (e.g., CH3(CH3O)2Si— or (CH3O)3Si—) different from that mentioned above and/or a (meth)acrylic polymer (C) containing a reactive silyl group that is not particularly limited.