Abstract:
The invention relates to a process for the treatment of heavy petroleum feedstocks in order to produce a gas oil fraction having a sulphur content of less than 50 ppm and generally 10 ppm which comprises the following stages: a) mild hydrocracking in a catalyst fixed bed, b) separation of the hydrogen sulphide, of a distillate cut including a gas oil fraction and of a fraction which is heavier than the gas oil, c) hydrotreating, by contact with at least one catalyst, of at least a portion of the said distillate cut obtained in stage b) including the gas oil fraction, as a mixture with a feedstock resulting from a crude or refined renewable source, d) separation of a gas oil cut comprising less than 50 ppm of sulphur. Advantageously, the heavy fraction is sent for catalytic cracking. Preferably, the process is carried out with makeup hydrogen introduced in stage c) and very advantageously all the makeup hydrogen for the process is introduced in stage c).The invention also relates to a plant which can be used for implementing this process.
Abstract:
A process is described for preparing a solution formed by at least one cobalt and/or nickel salt of at least one heteropolyanion combining molybdenum and cobalt or molybdenum and nickel in its structure, said process comprising: a) mixing at least one source of molybdenum and at least one oxidizing compound in aqueous solution to synthesize peroxomolybdate ions at an acidic pH, the (oxidizing compound/molybdenum source) mole ratio being in the range 0.1 to 20; b) introducing at least one cobalt precursor and/or at least one nickel precursor into the solution from step a) to form a solution comprising at least said salt in which the (Co+Ni)/Mo mole ratio is in the range 0.25 to 0.85.
Abstract:
A supported and sulphur-containing catalyst is described, comprising; a porous support constituted by an organic-inorganic hybrid material for which the covalent bond between the organic and inorganic phases conforms to the formula M-O—Z—R where M represents at least one metal constituting the inorganic phase, Z at least one heteroelement from among phosphorus and silicon and R an organic fragment, at least one metal of group VIB and/or of group VB and/or of group VIII. The invention also relates to the use of this catalyst for the hydrorefining and the hydroconversion of hydrocarbon-containing feedstocks such as petroleum fractions, fractions from coal or biomass or hydrocarbons produced from natural gas.
Abstract:
A redox mass for chemical looping combustion processes includes a redox pair or set of pairs having a material able to be alternatively oxidized and reduced between CuO and Cu, between Cu2O and Cu, between NiO and Ni, between MnO2 and Mn2O3, between Mn2O3 and Mn3O4, between Mn3O4 and MnO, between MnO and Mn, between CO3O4 and CoO or between CoO and Co, and a binder containing at least one mixed cerine-zirconia oxide (Ce/Zr) of the general formula CexZr1-xO2, where 0.05≦x≦0.95.
Abstract translation:用于化学循环燃烧过程的氧化还原物质包括在MnO 2和Mn 2 O 3之间,Mn 2 O 3和Mn 3 O 4之间具有能够在CuO和Cu之间,NiO和Ni之间,NiO和Ni之间,MnO 2和Mn 2 O 3之间在CuO和Cu之间交替氧化和还原的材料的氧化还原对或成对 MnO和Mn之间,CO 3 O 4与CoO之间或CoO和Co之间的粘合剂,以及含有至少一种通式CexZr1-xO2的混合铈 - 氧化锆(Ce / Zr)的粘合剂,其中0.05< x≦̸ 0.95。
Abstract:
A process is described for preparing a solution formed by at least one cobalt and/or nickel salt of at least one heteropolyanion combining molybdenum and cobalt or molybdenum and nickel in its structure, said process comprising: a) mixing at least one source of molybdenum and at least one oxidizing compound in aqueous solution to synthesize peroxomolybdate ions at an acidic pH, the (oxidizing compound/molybdenum source) mole ratio being in the range 0.1 to 20; b) introducing at least one cobalt precursor and/or at least one nickel precursor into the solution from step a) to form a solution comprising at least said salt in which the (Co+Ni)/Mo mole ratio is in the range 0.25 to 0.85.
Abstract:
The present invention relates to a new type of redox mass that can be used in any chemical looping combustion process, said mass comprising a binder containing at least cerine-zirconia.
Abstract:
A process for the hydrocracking a hydrocarbon-containing feedstock in which at least 50% by weight of the compounds have an initial boiling point above 340° C. and a final boiling point below 540° C., using a catalyst having, in its oxide form, at least one metal selected from the metals of groups VIB, VIII and VB, said metals being present in the form of at least one polyoxometallate of formula (HhXxMmOy)q−, said polyoxometallates being present within a mesostructured matrix based on oxide of at least one element Y, said matrix having a pore size between 1.5 and 50 nm and having amorphous walls of thickness between 1 and 30 nm, said catalyst being sulphurized before used in said process.
Abstract:
The invention relates to a process of hydrodesulphuration of at least one gasoline cut implementing a catalyst comprising, in its oxide form, at least one metal from group VIB and/or at least one metal from group VIII of the periodic table, present in the form of at least one polyoxometalate of the formula (HhXxMmOy)q−, wherein X is an element selected from phosphorus (P), silicon (Si), boron (B), nickel (Ni) and cobalt (Co), the said element being taken alone, M is one or more element(s) selected from molybdenum (Mo), tungsten (W), nickel (Ni) and cobalt (Co), O is oxygen, H is hydrogen, h is an integer within the range 0 to 12, x is an integer within the range 0 to 4, m is an integer equal to 5, 6, 7, 8, 9, 10, 11, 12 and 18, y is an integer within the range 17 to 72 and q is an integer within the range 1 to 20, the said polyoxometalates being present within a mesostructured silicon oxide matrix having a pore size within the range 1.5 to 50 nm and having amorphous walls of thickness within the range 1 to 30 nm, the said catalyst being sulphured before being implemented in the said process.
Abstract:
A process for the hydrocracking a hydrocarbon-containing feedstock in which at least 50% by weight of the compounds have an initial boiling point above 340° C. and a final boiling point below 540° C., using a catalyst having, in its oxide form, at least one metal selected from the metals of groups VIB, VIII and VB, said metals being present in the form of at least one polyoxometallate of formula (HhXxMmOy)q−, said polyoxometallates being present within a mesostructured matrix based on oxide of at least one element Y, said matrix having a pore size between 1.5 and 50 nm and having amorphous walls of thickness between 1 and 30 nm, said catalyst being sulphurized before used in said process.
Abstract:
Preparation of a catalyst having at least one metal from group VIII, at least one metal from group VIB and at least one support; in succession: i) one of i1) contacting a pre-catalyst with metal from group VIII, metal from group VIB and support with a cyclic oligosaccharide naming at least 6 α-(1,4)-bonded glucopyranose subunits; i2) contacting support with a solution containing a precursor of metal from group VIII, a precursor of said metal from group VIB and a cyclic oligosaccharide composed of at least 6 α-(1,4)-bonded glucopyranose subunits; or i3) contacting support with a cyclic oligosaccharide composed of at least 6 α-(1,4)-bonded glucopyranose subunits followed by contacting solid derived therefrom with a precursor of metal from group VIII and a precursor of metal from group VIB.