Abstract:
A process of producing a component includes providing a substrate having an electrically conductive surface in the form of an electrically conductive layer; subdividing the layer with the aid of a laser process into a first electrically autonomous region and a second electrically autonomous region, wherein an electrically insulating region is formed in the electrically conductive layer to electrically separate the electrically autonomous regions; forming an electrical potential difference between the first electrically autonomous region and the second electrically autonomous region; and applying an electrically charged substance or an electrically charged substance mixture onto the first electrically autonomous region and/or the second electrically autonomous region, wherein the electrically autonomous region and/or an amount of the applied electrically charged substance or of the electrically charged substance mixture are adjusted by the electrical potential difference.
Abstract:
A luminophore having the empirical formula A3M*OxF9-2x:Mn4+ where A may be or include Li, Na, Rb, K, Cs, or combinations thereof. M* may be or include Cr, Mo, W, or combinations thereof. x may be or include 0
Abstract:
A light-emitting device includes a light-emitting semiconductor component that emits first light in a first wavelength range during operation A wavelength conversion element converts the first light at least partly into second light in a second wavelength range is arranged in the beam path of the first light. The second wavelength range differs from the first wavelength range. The wavelength conversion element includes nanoparticles containing organic luminescent molecules in a basic material formed from an SiO2-based material. A method for producing a light-emitting device is furthermore specified.
Abstract:
A process of producing a component includes providing a substrate having an electrically conductive surface in the form of an electrically conductive layer; subdividing the layer with the aid of a scratching process into a first electrically autonomous region and a second electrically autonomous region, wherein an electrically insulating region is formed in the electrically conductive layer to electrically separate the electrically autonomous regions; forming an electrical potential difference between the first electrically autonomous region and the second electrically autonomous region; and applying an electrically charged substance or an electrically charged substance mixture onto the first electrically autonomous region and/or the second electrically autonomous region, wherein the electrically autonomous region and/or an amount of the applied electrically charged substance or of the electrically charged substance mixture are adjusted by the electrical potential difference.
Abstract:
A method of producing an optoelectronic component includes providing a lead frame having an upper side including a contact region and a chip reception region raised relative to the contact region; arranging an electrically conductive element on the contact region; embedding the lead frame in a molded body, wherein the contact region is covered by the molded body, and the chip reception region and the electrically conductive element remain accessible on an upper side of the molded body; arranging an optoelectronic semiconductor chip on the chip reception region; and connecting the optoelectronic semiconductor chip and the electrically conductive element by a bonding wire.
Abstract:
A process of producing a component includes providing a substrate having an electrically conductive surface in the form of an electrically conductive layer; subdividing the layer with the aid of a scratching process into a first electrically autonomous region and a second electrically autonomous region, wherein an electrically insulating region is formed in the electrically conductive layer to electrically separate the electrically autonomous regions; forming an electrical potential difference between the first electrically autonomous region and the second electrically autonomous region; and applying an electrically charged substance or an electrically charged substance mixture onto the first electrically autonomous region and/or the second electrically autonomous region, wherein the electrically autonomous region and/or an amount of the applied electrically charged substance or of the electrically charged substance mixture are adjusted by the electrical potential difference.
Abstract:
A method of manufacturing optoelectronic components includes spraying a fluorescent layer of an optoelectronic component onto a substrate, the substance or the substance mixture of the fluorescent layer including an electric charge when sprayed on, and wherein the electrically charged substance or the at least partially electrically charged substance mixture includes a larger electric potential when the fluorescent layer is sprayed on than at least one area of the substrate; and locally adjusting the thickness of the fluorescent layer of the sprayed-on fluorescent substance when spraying on the fluorescent layer onto the substrate by an electric potential gradient.
Abstract:
A method for producing a multifunctional layer, a method for producing an electrophoresis substrate, and a method for producing a converter plate and an optoelectronic component are disclosed. In an embodiment the method includes providing an electrophoresis substrate comprising a carrier having a front side and a back side, wherein a first electrically conductive layer and a second electrically conductive layer are located on the front side, electrophoretically depositing a first material onto the first electrically conductive layer, electrophoretically depositing a second material onto the second electrically conductive layer and arranging a filler material between the first material and the second material, wherein the filler material forms a common boundary surface with the first material and the second material.
Abstract:
A ceramic conversion element includes a first ceramic layer having a first luminescent material, which transforms electromagnetic radiation of a first wavelength range into electromagnetic radiation of a second wavelength range. A second ceramic layer includes a second luminescent material, which transforms electromagnetic radiation of the first wavelength range into electromagnetic radiation of a third wavelength range. The first luminescent material and the second luminescent material are based on at least one inorganic compound containing oxygen and are different from one another. An optoelectronic component with a ceramic conversion element and a method for producing a ceramic conversion element are also specified.
Abstract:
A method can be used for fixing a matrix-free electrophoretically deposited layer on a semiconductor chip. A semiconductor wafer has a carrier substrate-and at least one semiconductor chip. The at least one semiconductor chip has an active zone for generating electromagnetic radiation. At least one contact area is formed on a surface of the at least one semiconductor chip facing away from the carrier substrate. A material is electrophoretically deposited on the surface of the at least one semiconductor chip facing away from the carrier substrate in order to form the electrophoretically deposited layer. Deposition of the material on the at least one contact area is prevented. An inorganic matrix material is applied to at least one section of a surface of the semiconductor wafer facing away from the carrier substrate in order to fix the material on the at least one semiconductor chip.