Abstract:
One or more aspects of the disclosure pertain to an article including a film disposed on a glass substrate, which may be strengthened, where the interface between the film and the glass substrate is modified, such that the article has an improved average flexural strength, and the film retains key functional properties for its application. Some key functional properties of the film include optical, electrical and/or mechanical properties. In one or more embodiments, the interface exhibits an effective adhesion energy of about less than about 4 J/m2. In some embodiments, the interface is modified by the inclusion of a crack mitigating layer containing an inorganic material between the glass substrate and the film.
Abstract:
Embodiments of this disclosure pertain to articles that exhibit scratch-resistance and improved optical properties. In some examples, the article exhibits a color shift of about 2 or less, when viewed at an incident illumination angle in the range from about 0 degrees to about 60 degrees from normal under an illuminant. In one or more embodiments, the articles include a substrate, and an optical film disposed on the substrate. The optical film includes a scratch-resistant layer and a refractive index gradient. In one or more embodiments, the refractive index includes a refractive index that increases from a first surface at the interface between the substrate and the optical film to a second surface. The refractive index gradient may be formed from a compositional gradient and/or a porosity gradient.
Abstract:
Delamination resistant glass containers with heat-tolerant coatings are disclosed. In one embodiment, a glass container may include a glass body having an interior surface, an exterior surface and a wall thickness extending from the exterior surface to the interior surface. At least the interior surface of the glass body is delamination resistant. The glass container may further include a heat-tolerant coating positioned on at least a portion of the exterior surface of the glass body. The heat-tolerant coating may be thermally stable at temperatures greater than or equal to 260° C. for 30 minutes.
Abstract:
An article that includes: a substrate having a glass, glass-ceramic or a ceramic composition and comprising a primary surface; and a protective film disposed on the primary surface. The protective film comprises a thickness of greater than 1.5 microns and a maximum hardness of greater than 15 GPa at a depth of 500 nanometers, as measured on the film disposed on the substrate. Further, the protective film comprises a metal oxynitride that is graded such that an oxygen concentration in the film varies by 1.3 or more atomic %. In addition, the substrate comprises an elastic modulus less than an elastic modulus of the film.
Abstract:
Described herein are organosilicon modification layers and associated deposition methods and inert gas treatments that may be applied on a sheet, a carrier, or both, to control van der Waals, hydrogen and covalent bonding between a sheet and carrier. The modification layers bond the sheet and carrier together such that a permanent bond is prevented at high temperature processing as well as maintaining a sufficient bond to prevent delamination during high temperature processing.
Abstract:
Embodiments of glass containers resistant to delamination and methods for forming the same are disclosed. According to one embodiment, a delamination resistant glass container may include a glass article having a body extending between an interior surface and an exterior surface. The body defines an interior volume. The body may include an interior region extending from 10 nm below the interior surface of the body into a thickness of the body. The interior region has a persistent layer homogeneity such that the body is resistant to delamination.
Abstract:
A method of controllably bonding a thin sheet having a thin sheet bonding surface with a carrier having a carrier bonding surface, by depositing a carbonaceous surface modification layer onto at least one of the thin sheet bonding surface and the carrier bonding surface, incorporating polar groups with the surface modification layer, and then bonding the thin sheet bonding surface to the carrier bonding surface via the surface modification layer. The surface modification layer may include a bulk carbonaceous layer having a first polar group concentration and a surface layer having a second polar group concentration, wherein the second polar group concentration is higher than the first polar group concentration. The surface modification layer deposition and the treatment thereof may be performed by plasma polymerization techniques.
Abstract:
Embodiments of glass containers resistant to delamination and methods for forming the same are disclosed. According to one embodiment, a delamination resistant glass container may include a glass article having a body extending between an interior surface and an exterior surface. The body defines an interior volume. The body may include an interior region extending from 10 nm below the interior surface of the body into a thickness of the body. The interior region has a persistent layer homogeneity such that the body is resistant to delamination.
Abstract:
Embodiments of glass containers resistant to delamination and methods for forming the same are disclosed. According to one embodiment, a delamination resistant glass container may include a glass article having a body extending between an interior surface and an exterior surface. The body defines an interior volume. The body may include an interior region extending from 10 nm below the interior surface of the body into a thickness of the body. The interior region has a persistent layer homogeneity such that the body is resistant to delamination.
Abstract:
Embodiments of this disclosure pertain to a coating material comprising silicon and/or aluminum, hydrogen and any two or more of oxygen, nitrogen, carbon, and fluorine. The coating material exhibits a hardness of about 17 GPa or greater and an optical band gap of about 3.5 eV or greater. In some embodiments, the coating material includes, in atomic %, silicon and/or aluminum in an amount of about 40 or greater, hydrogen in an amount in the range from about 1 to about 25, nitrogen in an amount of about 30 or greater, oxygen in an amount in the range from about 0 to about 7.5, and carbon in an amount in the range from about 0 to about 10. The coating material may optionally include fluorine and/or boron. Articles including the coating material are also described and exhibit an average transmittance of about 85% or greater over an optical wavelength regime in the range from about 380 nm to about 720 nm and colorlessness.