Abstract:
A method for fabricating semiconductor device is disclosed. The method includes the steps of: providing a substrate having gate structure thereon, wherein the gate structure comprises a high-k dielectric layer; increasing an ambient pressure around the gate structure to a predetermined pressure by injecting a first gas; reducing the ambient pressure to a base pressure; and forming a spacer around the gate structure.
Abstract:
A method for fabricating p-type field effect transistor (FET) includes the steps of first providing a substrate, forming a pad layer on the substrate, forming a well in the substrate, performing an ion implantation process to implant germanium ions into the substrate to form a channel region, and then conducting an anneal process to divide the channel region into a top portion and a bottom portion. After removing the pad layer, a gate structure is formed on the substrate and a lightly doped drain (LDD) is formed adjacent to two sides of the gate structure.
Abstract:
A method for fabricating of semiconductor device is provided, including providing a substrate. A first trench isolation and a second trench isolation are formed in the substrate. A portion of the substrate is etched to have a height between a top and a bottom of the first and second trench isolations. A germanium (Ge) doped layer region is formed in the portion of the substrate. A fluorine (F) doped layer region is formed in the portion of the substrate, lower than and overlapping with the germanium doped layer region. An oxidation process is performed on the portion of the substrate to form a gate oxide layer between the first and second trench isolations.
Abstract:
A p-type field effect transistor (pFET) includes a gate structure on a substrate, a channel region in the substrate directly under the gate structure, and a source/drain region adjacent to two sides of the gate structure. Preferably, the channel region includes a top portion and a bottom portion, in which a concentration of germanium in the bottom portion is lower than a concentration of germanium in the top portion and a depth of the top portion is equal to a depth of the bottom portion.
Abstract:
A semiconductor structure includes a substrate, fin-shaped structures disposed on the substrate, an isolation layer disposed between the fin-shaped structures, and a doped region disposed in an upper portion of the isolation layer, where the doped region is doped with helium or neon.
Abstract:
A semiconductor device and a method for manufacturing the same are provided in the present invention. The semiconductor device includes a substrate, a gate structure on the substrate and two spacers on both sidewalls of the gate structure. Each spacer comprises an inner first spacer portion made of SiCN and an outer second spacer portion made of SiOCN.
Abstract:
A semiconductor device includes a substrate, an electrode layer disposed on the substrate, and a tri-layered gate-control stack sandwiched between the substrate and the electrode layer. The tri-layered gate-control stack includes a ferroelectric layer disposed on the substrate, a mid-gap metal layer sandwiched between the ferroelectric layer and the substrate, and an anti-ferroelectric layer. The anti-ferroelectric layer is sandwiched between the substrate and the mid-gap metal layer. Alternatively, the ferroelectric layer and the mid-gap metal layer are sandwiched between the anti-ferroelectric layer and the substrate.
Abstract:
A method for fabricating semiconductor device is disclosed. The method includes the steps of: providing a substrate having gate structure thereon, wherein the gate structure comprises a high-k dielectric layer; increasing an ambient pressure around the gate structure to a predetermined pressure by injecting a first gas; reducing the ambient pressure to a base pressure; and forming a spacer around the gate structure.
Abstract:
A method for forming a HfOx film based on atomic layer deposition (ALD) process includes: providing a substrate; dividing a plurality of ALD cycles as needed into multiple depositing stages, wherein each of the ALD cycles includes applying HfCl4 pulse and applying H2O pulse over the substrate and a content ratio of HfCl4 to H2O is different and increasing for the depositing stages; and performing the depositing stages to form a HfOx film.
Abstract:
A method for fabricating p-type field effect transistor (FET) includes the steps of first providing a substrate, forming a pad layer on the substrate, forming a well in the substrate, performing an ion implantation process to implant germanium ions into the substrate to form a channel region, and then conducting an anneal process to divide the channel region into a top portion and a bottom portion. After removing the pad layer, a gate structure is formed on the substrate and a lightly doped drain (LDD) is formed adjacent to two sides of the gate structure.