摘要:
To provide a branched propylene-based polymer that is excellent in ductility when melting, while retaining melt tension necessary for molding. A branched propylene-based polymer having the following properties (1), (2) and (3): property (1): a multi-branching index (MBI) is 0.45 or more and 1.00 or less; property (2): a strain hardening index at a strain rate (dε/dt) of 1.0/see (SHI@1s−1) is 0.70 or more and 3.00 or less; and property (3): a maximum drawing rate (MaxDraw) at 230° C. and a melt flow rate (MFR) satisfy a relation represented by the following formula (1-1):
摘要:
This decorative film is to be bonded to a resin molded body by means of thermoforming, and comprises a sealing layer (I) that contains a polypropylene resin (A) and a layer (II) that contains a polypropylene resin (B). The polypropylene resin (A) satisfies the requirement (a1), while the polypropylene resin (B) satisfies the requirement (b1). (a1) The melt flow rate (MFR (A)) (at 230° C. under a load of 2.16 kg) is more than 0.5 g/10 minutes. (b1) The melt flow rate (MFR (B)) (at 230° C. under a load of 2.16 kg) and the MFR (A) satisfy relational expression (b-1). MFR (B)
摘要:
A catalyst configured to be handled more easily than conventional catalysts and configured to copolymerize an α-olefin and a (meth)acrylic acid ester with high activity. The objects are achieved by polymerization using an olefin polymerization catalyst which contains a metal complex obtained by reacting a ligand having a specific structure and a transition metal compound containing a transition metal selected from nickel or palladium having a specific structure.
摘要:
An object of the present invention is to provide a novel catalyst for olefin (co)polymer production, which has high activity without using a large amount of a cocatalyst and is aimed for obtaining a particulate olefin (co)polymer. The invention relates to an olefin polymerization catalyst which comprises: a solid carrier (1) that has been brought into contact with a specific compound; and a metal catalyst component (2) that contains a transition metal compound (C) containing a transition metal M belonging to Group 9, 10, or 11 of the periodic table and has a reactive group Ra.
摘要:
An object of the present invention is to prevent an occurrence of flow-mark molding defects to improve an appearance of molded articles, and as a means for achieving the object, a propylene-based block copolymer is used as an appearance improver, the copolymer comprising 80 to 60% by weight of crystalline propylene polymer portion which has an intrinsic viscosity [η]p of 0.90 dL/g or less and 20 to 40% by weight of propylene/ethylene random copolymer portion which has an ethylene content of 35 to 50% by weight and an intrinsic viscosity [η]c of 7.0 dL/g or higher ([η]c/[η]p being 7.5 to 30), in which the propylene-based block copolymer has a MFR of 10 to 50 g/10 min.
摘要:
Provided is a process of effectively producing an ethylene/unsaturated carboxylic acid copolymer having excellent mechanical and thermal properties. A process for producing an ethylene/unsaturated carboxylic acid copolymer comprises: producing an ethylene/unsaturated carboxylic acid ester copolymer from ethylene and unsaturated carboxylic acid ester using a late-transition-metal complex catalyst; and heating the ethylene/unsaturated carboxylic acid ester copolymer at a temperature capable of converting the ester group into a carboxylic acid group, thereby converting into the ethylene/unsaturated carboxylic acid copolymer.
摘要:
An object of the present invention is to prevent an occurrence of flow-mark molding defects to improve an appearance of molded articles, and as a means for achieving the object, a propylene-based block copolymer is used as an appearance improver, the copolymer comprising 80 to 60% by weight of crystalline propylene polymer portion which has an intrinsic viscosity [η]p of 0.90 dL/g or less and 20 to 40% by weight of propylene/ethylene random copolymer portion which has an ethylene content of 35 to 50% by weight and an intrinsic viscosity [η]c of 7.0 dL/g or higher ([η]c/[η]p being 7.5 to 30), in which the propylene-based block copolymer has a MFR of 10 to 50 g/10 min.
摘要:
Provided is a polypropylene-based resin composition which gives uniform and fine cells and from which a foamed sheet and thermoform excellent in appearance, thermoformability, impact resistance, lightness, stiffness, heat resistance, heat insulating properties, oil resistance and the like can be produced. A polypropylene-based resin composition comprising (X) 5 to 99% by weight of a polypropylene resin having a structure with long chain branches, and (Y) 1 to 95% by weight of a propylene-based block copolymer produced by sequential polymerization, which block copolymer comprises (Y-1) a propylene (co)polymer and (Y-2) a propylene-ethylene copolymer, said resin (X) having properties (X-i) to (X-iv) and said block copolymer (Y) having properties (Y-i) to (Y-v), and the like.
摘要:
The present invention relates to a polar group-containing olefin copolymer (A′) which is produced through polymerization using a transition metal catalyst, which has a weight-average molecular weight falling within a specific range and which contains a polar group-containing monomer within a specific range; a multinary polar olefin copolymer (A″) indispensably containing a polar monomer component that has a norbornene skeleton and a carboxyl group or an acid anhydride group and having three or more types of monomer units; and a resin composition (C) containing a specific amount of a polar group-containing olefin copolymer (A) and a specific amount of an olefin resin (B).
摘要:
Provided is a thermoplastic resin composition that is free of discoloration defects, is resistant to the staining and deterioration caused by urine, fecal matter, detergents and so forth, exhibits an excellent tactile sensation, and also exhibits an excellent marring resistance and that is thus well suited for toilet components. Toilet components comprising this thermoplastic resin composition are also provided.The thermoplastic resin composition comprises (A) a thermoplastic resin and, per 100 weight parts thereof, (B) 2 to 40 weight parts of an organic flame retardant, 0.1 to 2 weight parts of a component (D), and as desired, (C) 0.1 to 20 weight parts of a flame retardant synergist, wherein the component (D) satisfies the following condition:condition: the component (D) is at least one compound selected from the group consisting of polyolefin-based waxes, alcohols, carboxylic acids, and esters, and having a melting point of not more than 100° C. and an HLB value of not more than 5.The toilet components and so forth comprise this thermoplastic resin composition.