摘要:
To provide a perovskite-type composite oxide which has stable quality in which a solid solution of Pd is formed at a high rate, a method for producing the perovskite-type composite oxide, and a catalyst composition containing the perovskite-type composite oxide, the perovskite-type composite oxide is produced by formulating materials in accordance with each atomic ratio of a perovskite-type composite oxide represented by the following general formula (1): AxB(1-y)PdyO3+δ (1) wherein A represents at least one element selected from rare earth elements and alkaline earth metals; B represents at least one element selected from transition elements (excluding rare earth elements, and Pd), Al and Si; x represents an atomic ratio satisfying the following condition: 1
摘要:
To provide a perovskite-type composite oxide which has stable quality in which a solid solution of Pd is formed at a high rate, a method for producing the perovskite-type composite oxide, and a catalyst composition containing the perovskite-type composite oxide, the perovskite-type composite oxide is produced by formulating materials in accordance with each atomic ratio of a perovskite-type composite oxide represented by the following general formula (1): AxB(1-y)PdyO3+δ (1) wherein A represents at least one element selected from rare earth elements and alkaline earth metals; B represents at least one element selected from transition elements (excluding rare earth elements, and Pd), Al and Si; x represents an atomic ratio satisfying the following condition: 1
摘要:
An object of the present invention is to provide a catalyst composition containing a perovskite-type composite oxide which exhibits a satisfactory catalytic performance over a long time even in a high temperature atmosphere and has a stable quality in which Rh and/or Pt dissolves to form a solid solution at a high rate.To achieve the object described above, in the present invention the catalyst composition is prepared to comprise an Rh-containing perovskite-type composite oxide represented by the following general formula (I) and/or a Pt-containing perovskite-type composite oxide represented by the following general formula (II) and a thermostable oxide optionally containing a noble metal. A1xA2wB11−(y+z)B2yRhzO3±δ (I) A3rA4sB31−(t+u)B4tPtuO3±δ′ (II)
摘要:
To provide an exhaust gas purifying catalyst which can maintain the catalytic activity at a high level over a long time and can achieve satisfactory emission control performance, an exhaust gas purifying catalyst is prepared so as to contain a noble metal, a perovskite-type composite oxide represented by the following general formula (3), and theta-alumina and/or alpha-alumina: AB1-mNmO3 (3) wherein A represents at least one element selected from rare-earth elements and alkaline earth metals; B represents at least one element selected from Al and transition elements excluding rare-earth elements and noble metals; N represents a noble metal; and m represents an atomic ratio of N satisfying the following relation: 0
摘要:
To provide a method for industrially efficiently producing an exhaust gas purifying catalyst containing a perovskite-type composite oxide which is stable and has a less reduced specific surface area and is also effectively prevented from decreasing in its catalytic performance even in endurance in high temperature oxidative reducing atmospheres, a pre-crystallization composition containing elementary components constituting a perovskite-type composite oxide containing a noble metal is prepared, is mixed with a powder of theta-alumina and/or alpha-alumina to prepare a mixture, and the mixture is heat treated. Thus, the resulting perovskite-type composite oxide supported by the powder of theta-alumina and/or alpha-alumina can keep its thermostability at a sufficient level thereby to effectively prevent the catalytic performance from decreasing. This method can industrially efficiently produce the exhaust gas purifying catalyst.
摘要:
To provide an exhaust gas purifying catalyst which can maintain the catalytic activity at a high level over a long time and can achieve satisfactory emission control performance, an exhaust gas purifying catalyst is prepared so as to contain a noble metal, a perovskite-type composite oxide represented by the following general formula (3), and theta-alumina and/or alpha-alumina: AB1−mNmO3 (3) wherein A represents at least one element selected from rare-earth elements and alkaline earth metals; B represents at least one element selected from Al and transition elements excluding rare-earth elements and noble metals; N represents a noble metal; and m represents an atomic ratio of N satisfying the following relation: 0
摘要:
An excellent oxygen storage capacity is achieved even in the case used for a long period of time under high temperature conditions. An oxygen storage material contains a first particle made of a composite oxide of cerium and zirconium or a composite oxide of cerium, a rare-earth element other than cerium and zirconium, a second particle including a composite oxide of a rare-earth element, an alkaline-earth element and zirconium, and a precious metal. A part of the precious metal forms a solid solution with the composite oxide included in the second particle.
摘要:
An exhaust gas-purifying catalyst (1) contains a rare-earth element, an alkaline-earth element, zirconium and a precious metal, wherein an atomic ratio of the alkaline-earth element with respect to a sum of the rare-earth element and the zirconium is 10 atomic % or more, a part of the rare-earth element and a part of zirconium form a composite oxide with at least a part of the alkaline-earth element, and the composite oxide and a part of the precious metal form a solid solution.
摘要:
An excellent oxygen storage capacity is achieved even in the case used for a long period of time under high temperature conditions. An oxygen storage material contains a first particle made of a composite oxide of cerium and zirconium or a composite oxide of cerium, a rare-earth element other than cerium and zirconium, a second particle including a composite oxide of a rare-earth element, an alkaline-earth element and zirconium, and a precious metal. A part of the precious metal forms a solid solution with the composite oxide included in the second particle.
摘要:
Provided is a catalyst with a noble metal efficiently supported on the surfacemost thereof. A composite oxide-containing layer is formed on a catalyst carrier so as to contain a perovskite-type composite oxide represented by the following general formula (1) and an other composite oxide, and a noble metal layer is further formed on the catalyst carrier so as to be supported on the surfacemost of the catalyst carrier by immersing the catalyst carrier formed with the composite oxide-containing layer in an aqueous noble metal salt solution to impregnate the catalyst carrier with the aqueous noble metal salt solution: AxByO3±δ (1) (wherein A represents at least one element selected from rare earth elements and alkaline earth metals; B represents at least one element selected from transition elements (excluding rare earth elements); x represents an atomic ratio of less than 1; y represents an atomic ratio of 1.0; and δ represents an oxygen excess or an oxygen deficiency.)