Stable support for Fischer-Tropsch catalyst
    5.
    发明授权
    Stable support for Fischer-Tropsch catalyst 有权
    稳定支持费 - 托催化剂

    公开(公告)号:US09233360B1

    公开(公告)日:2016-01-12

    申请号:US14482313

    申请日:2014-09-10

    摘要: A process has been developed for preparing a Fischer-Tropsch catalyst precursor and a Fischer-Tropsch catalyst made from the precursor. The process includes contacting a gamma alumina catalyst support material with a first solution containing a compound containing zinc and optionally containing P, Ti, V, Co, Ga, Ge, Mo, W and/or Pr to obtain a modified catalyst support material. The modified catalyst support material is calcined at a temperature of at least 500° C. The calcined modified catalyst support has a pore volume of at least 0.4 cc/g. The modified catalyst support is less soluble in acid solutions than an equivalent unmodified catalyst support. The modified catalyst support is contacted with a second solution which includes a precursor compound of an active cobalt catalyst component to obtain a catalyst precursor. The catalyst precursor is reduced to activate the catalyst precursor to obtain the Fischer-Tropsch catalyst. The catalyst has enhanced hydrothermal stability as measured by losing no more than 20% of its pore volume when exposed to water vapor.

    摘要翻译: 已经开发了制备费 - 托催化剂前体和由前体制备的费 - 托催化剂的方法。 该方法包括使γ氧化铝催化剂载体材料与含有锌化合物和任选地含有P,Ti,V,Co,Ga,Ge,Mo,W和/或Pr的第一溶液接触,以获得改性的催化剂载体材料。 改性的催化剂载体材料在至少500℃的温度下煅烧。煅烧的改性催化剂载体的孔体积至少为0.4cc / g。 改性的催化剂载体在酸溶液中比相当的未改性的催化剂载体更难溶解。 将改性的催化剂载体与包含活性钴催化剂组分的前体化合物的第二溶液接触以获得催化剂前体。 催化剂前体被还原以活化催化剂前体以获得费 - 托催化剂。 催化剂具有增强的水热稳定性,当暴露于水蒸气时,其通过损失其不超过其孔体积的20%来测量。