摘要:
Process for producing biaxially oriented PET film for use in film capacitors with SMD capabilities and its use for SMD-technology film capacitors The invention describes a process for producing a biaxially oriented film of thickness 0.1% and transversely by >3%, where the edges of the film are held during the longitudinal and transverse relaxation and the film is wound up.
摘要:
The invention relates to a biaxially oriented polyester film having one or more layers and a thickness of .ltoreq.10 .mu.m, where the mechanical consolidation coefficient MC, given by the following equation, lies within the ranges given below:MC here is .gtoreq.-2, preferably >0 and in particular >0.5, particularly preferably .gtoreq.1, and is .ltoreq.50, preferably .ltoreq.30 and particularly preferably
摘要:
Biaxially stretched film with polymeric constituents formed mainly of polyester in which the film includes at least one copper salt and one halide, with the resulting film having an AC (alternating current) dielectric strength of at least 100 kV/mm at 23° C. and 50 Hz. The invention further relates to the use of the film of the invention, in particular in solar modules, and also to a process for its production.
摘要:
Biaxially stretched film with polymeric constituents formed mainly of polyester in which the film includes at least one copper salt and one halide, with the resulting film having an AC (alternating current) dielectric strength of at least 100 kV/mm at 23° C. and 50 Hz. The invention further relates to the use of the film of the invention, in particular in solar modules, and also to a process for its production.
摘要:
The present invention relates to a single or multilayer biaxially oriented film having a thickness of ≦12 &mgr;m, in which Ts (TD) is ≧160° C., S 200 (TD) is ≦5%, S 200 (MD) is 2-5%, the shrinkage force ratio Ns 220/Ns 160 is ≧4.5; the film fixing peak is ≧210° C.; the film density is 1.39-1.41 g/cm3, and Ts (TD) is the temperature at which the transverse shrinkage begins, S 200 (TD) is the shrinkage in the transverse direction (in %) at 200° C., S 200 (MD) is the shrinkage in the machine direction (in %) at 200° C., Ns 220 is the shrinkage force (in N) at 220° C. and Ns 160 is the shrinkage force (in N) at 160° C. in the transverse direction. The invention also relates to a method for forming the film.
摘要:
The invention relates to biaxially oriented polyester films which contain 0.1-5.0% by weight (based on the weight of the film) of a hydrolysis stabilizer based on epoxidized fatty acid esters and 0.2-10% by weight (based on the weight of the film) of epoxidized fatty acid glycerides, the epoxidized fatty acid esters having a mean molecular weight of at least 425 g/mol. Such films find use in outdoor applications, as a ribbon cable, as a backside laminate of solar modules and in electrical insulation applications.
摘要:
The invention relates to biaxially oriented polyester films which contain 0.1-5.0% by weight (based on the weight of the film) of a hydrolysis stabilizer based on epoxidized fatty acid esters and 0.2-10% by weight (based on the weight of the film) of epoxidized fatty acid glycerides, the epoxidized fatty acid esters having a mean molecular weight of at least 425 g/mol. Such films find use in outdoor applications, as a ribbon cable, as a backside laminate of solar modules and in electrical insulation applications.
摘要:
The invention relates to a biaxially oriented film containing at least one black pigment. The film is predominantly formed from a polyester whose diol component includes at least 80 mol-% of 1,4-cyclohexanedimethanol (CHDM), and whose the dicarboxylic acid component includes at least 80 mol-% of one or more benzenedicarboxylic acid(s) and/or one or more naphthalene dicarboxylic acid(s). The dicarboxylic acid component includes a main dicarboxylic acid component forming an at least 55 mol-% portion, chosen from either 2,6-naphthalene dicarboxylic acid or terephthalic acid. The dicarboxylic acid component further includes a secondary dicarboxylic acid component, present in an amount of at least 18 mol-%, with the secondary dicarboxylic acid component differing from the main dicarboxylic acid component. The invention further relates to a method for producing the film and its use.
摘要:
The invention relates to a biaxially oriented polyester film having a roughness, on at least one film surface, of R.sub.z greater than 1.0 .mu.m (Ra is greater than 0.1 .mu.m), a dielectric strength (AC) greater than 220 kV/mm (the DC dielectric strength is greater than 500 kV/mm) and a migrating fraction in the film of less than 18 .mu.S/cm based on a mass of added particles in a polyester volume of 100 cm.sup.3. The film is particularly suitable for oil-impregnated capacitors.
摘要:
The invention relates to a biaxially oriented film, predominantly formed from a polyester whose diol component includes at least 80 mol-% of 1,4-cyclohexanedimethanol (CHDM), and whose dicarboxylic acid component includes at least 80 mol-% of one or more benzenedicarboxylic acid(s) and/or one or more naphthalene dicarboxylic acid(s). The dicarboxylic acid component includes a main dicarboxylic acid component forming an at least 55 mol-% portion, chosen from either 2,6-naphthalene dicarboxylic acid or terephthalic acid. The dicarboxylic acid component further includes a secondary dicarboxylic acid component, present in an amount of at least 18 mol-%, with the secondary dicarboxylic acid component differing from the main dicarboxylic acid component. The invention further relates to a method for producing the film and its use.