摘要:
A polyethylene molding composition having a multimodal molecular mass distribution and comprising from 45 to 55% by weight of a low molecular weight ethylene homopolymer A, from 20 to 40% by weight of a high molecular weight copolymer B comprising ethylene and another olefin having from 4 to 8 carbon atoms and from 15 to 30% by weight of an ultrahigh molecular weight ethylene copolymer C can be prepared in the presence of a Ziegler catalyst in a three-stage process and is highly suitable for producing pipes having excellent mechanical properties.
摘要:
The invention relates to a polyethylene molding composition which has a multimodal molar mass distribution and is particularly suitable for producing external sheathing of electric or information transmission cables. The molding composition has a density at a temperature of 23° C. in the range from 0.94 to 0.95 g/cm3 and an MFI190/5 in the range from 1.2 to 2.1 dg/min. It comprises from 45 to 55% by weight of a low molecular weight ethylene homopolymer A, from 30 to 40% by weight of a high molecular weight copolymer B of ethylene and another olefin having from 4 to 8 carbon atoms and from 10 to 20% by weight of an ultra high molecular weight ethylene copolymer C. The invention also relates to an electric or information transmission cable having an external sheath of the polyethylene molding composition which has a thickness in the range from 0.2 to 3 cm.
摘要:
The invention relates to a polyethylene molding composition which has a multimodal molecular mass distribution and comprises a low molecular weight ethylene homopolymer A, a high molecular weight ethylene copolymer B and an ultrahigh molecular weight ethylene copolymer C. The molding composition has a density at a temperature of 23° C. in the range from 0.940 to 0.957 g/cm3, an MFR (190° C./2.16 kg) in the range from 0.5 to 4 dg/min and a viscosity number VN3 of the mixture of ethylene homopolymer A, copolymer B and ethylene copolymer C, measured in accordance with ISO/R 1191 in decalin at a temperature of 135° C., in the range from 150 to 300 cm3/g. The invention further relates to the use of such a molding composition for producing injection-molded finished parts, and to finished parts produced by injection molding.
摘要:
A polyethylene molding composition having a multimodal molecular mass distribution and comprising from 45 to 55% by weight of a low molecular weight ethylene homopolymer A, from 20 to 40% by weight of a high molecular weight copolymer B comprising ethylene and another olefin having from 4 to 8 carbon atoms and from 15 to 30% by weight of an ultrahigh molecular weight ethylene copolymer C can be prepared in the presence of a Ziegler catalyst in a three-stage process and is highly suitable for producing pipes having excellent mechanical properties.
摘要:
A novel adhesive composition suitable for composing multilayered coatings onto large, industrial equipment such as pipeline tubes is devised. The composition is a blend based on a polyethylene which determines the blend's favorable properties, which polyethylene itself can be used further in coating cables and for producing moldings, especially rotomoulded articles.
摘要:
The invention relates to a polyethylene molding composition which has a multimodal molar mass distribution and is particularly suitable for producing protective coatings on steel pipes. The molding composition has a density at a temperature of 23° C. in the range from 0.94 to 0.95 g/cm3 and an MFI190/5 in the range from 1.2 to 2.1 dg/min. It comprises from 45 to 55% by weight of a low molecular weight ethylene homopolymer A, from 30 to 40% by weight of a high molecular weight copolymer B of ethylene and another olefin having from 4 to 8 carbon atoms and from 10 to 20% by weight of an ultra high molecular weight ethylene copolymer C.
摘要:
The invention relates to a polyethylene molding composition which has a multimodal molecular mass distribution and comprises a low molecular weight ethylene homopolymer A, a high molecular weight ethylene copolymer B and an ultrahigh molecular weight ethylene copolymer C. The molding composition has a density at a temperature of 23° C. in the range from 0.940 to 0.957 g/cm3, an MFR (190° C./2.16 kg) in the range from 0.5 to 4 dg/min and a viscosity number VN3 of the mixture of ethylene homopolymer A, copolymer B and ethylene copolymer C, measured in accordance with ISO/R 1191 in decalin at a temperature of 135° C., in the range from 150 to 300 cm3/g. The invention further relates to the use of such a molding composition for producing injection-molded finished parts, and to finished parts produced by injection molding.
摘要:
A novel adhesive composition suitable for composing multilayered coatings onto large, industrial equipment such as pipeline tubes is devised. The composition is a blend based on a polyethylene which determines the blend's favorable properties, which polyethylene itself can be used further in coating cables and for producing mouldings, especially rotomoulded articles.