摘要:
Various embodiments of a polyetherimide film and multilayer structure are provided. In one embodiment the polyetherimide film has a glass transition temperature that ranges from about 260° C. to about 350° C. and the polyetherimide has a melt viscosity range from about 200 to about 10,000 Pascal-seconds at 425° C. as measured by ASTM method D3835.
摘要:
Various embodiments of a polymer composition are provided. In one embodiment the polymer composition includes, by weight, from about 50% to about 95% polyetherimide resin and from about 5% to about 50% inorganic substance. The polymer composition when formed into a film has a coefficient of thermal expansion of less than about 50 ppm/° C.
摘要:
Disclosed is a biaxially oriented multilayer film comprising at least two layers A-B, wherein A and B represent separate layers at least one of which layers comprises a polyimide having a Tg of greater than about 200° C., wherein the film has a CTE of less than 35 ppm/° C., and wherein A comprises 60 wt. %-100 wt. % of amorphous polymer with 0 wt. %-40 wt. % of crystallizable polymer, and B comprises 60 wt. %-100 wt. % crystallizable polymer with 0 wt. %-40 wt. % amorphous polymer, the relative thicknesses of layer A to layer B are in a ratio in a range of between 1:5 and 1:100, and the thickness of the film is in a range of between 5 μm and 125 μm. Also disclosed is a biaxially oriented monolithic film comprising a polyimide with structural units formally derived from 3,4-diaminodiphenylether and 4,4-oxydiphthalic anhydride. Laminates comprising the films and methods for making film and laminate are also disclosed. Articles comprising a film or laminate of the invention are also disclosed.
摘要:
Various embodiments of polymer fibers comprising a high heat polymer and process for making the polymer fibers are provided. In one embodiment, synthetic polymer fibers comprise polyetherimide polymer that is substantially free of foreign particulate matter greater than about 100 microns in size. A process for producing polymer fiber includes melting polymer comprising polyetherimide to a melt temperature that ranges from about 180-500° C. to form a molten polymer; passing the polyetherimide that is substantially free of foreign particulate matter above about 100 microns in size, through a spinneret comprising a plurality of hole openings to produce a fiber bundle; and cooling the fiber bundle with a cooling medium having a temperature that ranges from about 0° C. to about 80° C.
摘要:
In one aspect the present invention provides a storage medium for data, the storage medium comprising: a) a substrate, a physical portion of which comprises at least one polyimide, and b) at least one data layer on the substrate. The substrate comprising a polyimide exhibits low axial displacement and beneficial damping characteristics.
摘要:
Polymer blends suitable for use in optical article. The polymer blends comprise a first and second polycarbonate and have properties particularly suited for use in high density optical data storage media.
摘要:
The invention relates to substantially single phase silicone copolycarbonates suitable for use in optical articles such as digital versatile disks. The silicone copolycarbonates contain residues of silicone containing and nonsilicone containing bisphenols and have properties particularly suited for use in high density optical data storage media. The invention further relates to the preparation and properties of substantially single phase silicone copolycarbonates having either a blocky or a random structure. The structure of the compositions of the invention is determined by the method of preparation used and may be used to control physical properties.
摘要:
This disclosure relates to a data storage medium, and in particular to a data storage medium comprising at least one high modulus layer. In one embodiment, an asymmetric optical storage medium can comprise: a substrate layer comprising polyarylene ether, a high modulus layer comprising a thermoset, and a data layer disposed between the modulus layer and the substrate layer. The high modulus layer has a tensile modulus that is greater than a substrate layer tensile modulus. In another embodiment, an asymmetric optical storage medium can comprise: a substrate layer comprising polyarylene ether and having surface features and a high modulus layer disposed on the side of the substrate comprising the surface features. The surface features can comprise pits. The high modulus layer can comprise a thermoset, and can have a tensile modulus that is greater than a substrate layer tensile modulus.
摘要:
This disclosure relates to a data storage medium, and in particular to a data storage medium comprising at least one high modulus layer. An asymmetric optical storage medium can comprise: at least one substrate layer comprising polyarylene ether, at least one high modulus layer comprising a thermoset, and at least one data layer disposed between the modulus layer and the substrate layer.
摘要:
A disk substrate prepared from a blend of poly(arylene ether) resin and poly(alkenyl aromatic) resin is disclosed. The substrate can be used in data storage media having dimensional stability and good molded-in features.