摘要:
The amount of residual carbon and hydroxyl groups in a synthetic quartz powder made by a wet process is reduced by baking the synthetic quartz powder in a low pressure atmosphere. Quartz glass crucibles made using the synthetic quartz powder have low bubble contents, and are particularly suited for growing single crystals.
摘要:
The amount of residual carbon and hydroxyl groups in a synthetic quartz powder made by a wet process is reduced by baking the synthetic quartz powder in a low pressure atmosphere. Quartz glass crucibles made using the synthetic quartz powder have low bubble contents, and are particularly suited for growing single crystals.
摘要:
An amorphous luminous material, which is substantially composed of only rare earth complex compounds, wherein the compounds are two or more kinds of rare earth complexes, and rare earth metal ions, which are center ions of the two or more kinds of rare earth complexes, are different ions.
摘要:
A semiconductor device includes a gate electrode; a gate insulating film over the gate electrode; an oxide semiconductor film in contact with the gate insulating film and including a channel formation region which overlaps with the gate electrode; a source electrode and a drain electrode over the oxide semiconductor film; and an oxide insulating film over the oxide semiconductor film, the source electrode, and the drain electrode. The source electrode and the drain electrode each include a first metal film having an end portion at the end of the channel formation region, a second metal film over the first metal film and containing copper, and a third metal film over the second metal film. The second metal film is formed on the inner side than the end portion of the first metal film.
摘要:
Disclosed are a method of forming a back reflection layer in a solar cell, a composition used therefor, and a solar cell having a back reflection layer formed by the method, which layer has superior heat-resistance and various types of durabilities, and can contribute to improving the conversion rate of solar cells and reliability during long-term use, and which method can form a back reflection layer in a solar cell easily and at low cost. The polyimide resin composition for use in forming a back reflection layer in a solar cell includes an organic solvent, a polyimide resin dissolved in the organic solvent, and light-reflecting particles dispersed in the organic solvent.
摘要:
A weldment includes metal materials that are welded to each other. At least one of the metal materials includes pure copper including an inevitable impurity, more than 2 mass ppm of oxygen, and an additive element selected from the group consisting of Mg, Zr, Nb, Fe, Si, Al, Ca, V, Ni, Mn, Ti and Cr. A method of manufacturing a weldment includes melting a dilute copper alloy material by SCR continuous casting and rolling at a molten copper temperature of not less than 1100° C. and not more than 1320° C. to make a molten metal, forming a cast bar from the molten metal, forming a dilute copper alloy member by hot-rolling the cast bar, and welding the dilute copper alloy member to a metal material. The dilute copper alloy material includes the pure copper, more than 2 mass ppm of oxygen, and the additive element,?
摘要:
A catalyst for exhaust gas purification having superior exhaust gas purification performance is provided. Disclosed is a catalyst containing, as a catalyst support, a composite phosphate containing yttrium and phosphorus and having a composition ratio of yttrium to phosphorus (Y/P) of greater than 1 as a molar ratio.
摘要:
The purified air discharge device comprises a push hood (2) comprising an air flow discharge surface (23) discharging a uniform purified air flow. The push hood (2) is provided with a lateral air discharger (28) for creating a purified air flow that collides against a surrounding wall that is formed as the push hood (2) is installed and that is situated close along the circumferential direction of the air flow discharge surface (23) of the push hood (2).
摘要:
A local air cleaning apparatus (1) is provided with a push hood (2) having an air flow opening face (23) for blowing out a cleaned uniform air flow and a guide (3) provided on a side of the push hood (2) having the air flow opening face (23), the guide (3) extending from the side thereof having the air flow opening face (23) toward a downstream side of the uniform air flow to form an opening face (31) at a downstream end portion thereof. The push hood (2) is arranged such that the uniform air flow blown out from the air flow opening face (23) passes through the inside of the guide (3) and then collides with an air collision face (W) on a downstream side of the opening face (31). The opening face (31) of the guide (3) is spaced apart from and opposed to the air collision face (W) to form an open region between the opening face (3) and the air collision face (W). The cleaned uniform air flow blown out from the air flow opening face (23) collides with the air collision face (W) and flows out of the opening region, thereby allowing the inside of the guide (3) and the inside of the open region to have higher cleanliness than other regions.
摘要:
In the laminated coil component, the grain diameter of the coil conductors is 10 μm to 22 μm after baking is completed. When the grain diameter of the coil conductors is set to be 10 μm or larger after baking is completed, surface roughness of the coil conductors can be reduced to such an extent that a satisfactory Q value can be obtained at a high frequency. In addition, when the grain diameter of the coil conductors is set to be 22 μm or smaller after baking is completed, metal of the coil conductors can be refrained from being rapidly melted down during baking. Accordingly, a high Q value can be obtained while a high quality is ensured.