Multilayer coil component
    1.
    发明授权
    Multilayer coil component 有权
    多层线圈组件

    公开(公告)号:US07378931B2

    公开(公告)日:2008-05-27

    申请号:US11844483

    申请日:2007-08-24

    IPC分类号: H01F5/00

    CPC分类号: H01F17/0013 H01F2017/002

    摘要: A multilayer coil component is formed such that ceramic green sheets having coil conductors and via hole conductors are laminated. The multilayer coil component includes therein a spiral coil in which the coil conductors are connected in series through the via hole conductors. In plan view in a lamination direction, the via hole conductors are located in positions spaced toward the outer side of the spiral coil, the positions being located near end surfaces in a long side direction of a multilayer body.

    摘要翻译: 形成多层线圈部件,使得具有线圈导体和通孔导体的陶瓷生片层压。 多层线圈组件包括螺旋线圈,其中线圈导体通过通孔导体串联连接。 在层叠方向的平面图中,通孔导体位于与螺旋线圈的外侧隔开的位置,该位置位于多层体的长边方向的端面附近。

    Fuel pump and fuel supply system of internal combustion engine
    2.
    发明授权
    Fuel pump and fuel supply system of internal combustion engine 有权
    燃油泵和内燃机燃油供应系统

    公开(公告)号:US09188096B2

    公开(公告)日:2015-11-17

    申请号:US13581698

    申请日:2011-09-06

    摘要: A fuel pump which can suppress fuel bubbles from being sucked into a fuel pressure chamber, and can achieve a stable fuel pressure property. The fuel pump has a pump body formed with a suction passage and a pump operation chamber, and a pressure pump mechanism to pressurize and discharge fuel. The pump body has a lower side wall portion and an upper side wall portion respectively at the vertically lower and upper sides of the inner wall portion forming a suction gallery chamber partly forming the suction passage. The pressure pump mechanism has a valve retaining member having an insertion portion inserted into the suction gallery chamber. The insertion portion has internal suction inlets through which the fuel is sucked from the suction gallery chamber into the pump operation chamber, the internal suction inlets being positioned in the intermediate height area in the suction gallery chamber.

    摘要翻译: 一种能够抑制燃料气泡被吸入燃料压力室的燃料泵,能够实现稳定的燃料压力特性。 燃料泵具有形成有吸入通道和泵操作室的泵体,以及用于对燃料进行加压和排出的压力泵机构。 泵体在内壁部分的垂直下下侧分别具有下侧壁部分和上侧壁部分,形成部分地形成吸入通道的抽吸腔室。 压力泵机构具有阀保持构件,该阀保持构件具有插入吸入腔室中的插入部分。 插入部分具有内部吸入口,燃料通过该吸入口从抽吸腔室吸入泵操作室,内部吸入口位于抽吸腔室中的中间高度区域。

    METHOD FOR MANUFACTURING COPPER FOIL FOR NEGATIVE ELECTRODE CURRENT COLLECTOR
    3.
    发明申请
    METHOD FOR MANUFACTURING COPPER FOIL FOR NEGATIVE ELECTRODE CURRENT COLLECTOR 审中-公开
    用于制造负极电流集电器的铜箔的方法

    公开(公告)号:US20130306486A1

    公开(公告)日:2013-11-21

    申请号:US13807091

    申请日:2011-06-29

    IPC分类号: H01M4/04

    摘要: An object of the present invention is to provide a method for manufacturing a copper foil for a negative electrode current collector (specifically, copper foil for a negative electrode current collector of a lithium ion secondary battery) more excellent in discoloration resistance to improve charge/discharge cycle life of a secondary battery. To achieve the object, a method for manufacturing a copper foil for a negative electrode current collector of a secondary battery subjecting the copper foil to rust-proofing treatment, the method characterized in that the copper foil is rust-proofing treated with a chromate-treatment solution having pH in the range from 3.5 to 7.0 to form a chromate film on the surface of the copper foil is employed.

    摘要翻译: 本发明的目的是提供一种用于制造耐变色性优异的负极集电体(特别是锂离子二次电池用负极集电体用铜箔)的铜箔的制造方法,以提高充放电性 二次电池的循环寿命。 为了实现该目的,提供了一种用于制造用于对铜箔进行防锈处理的二次电池的负极集电体的铜箔的方法,其特征在于,所述铜箔用铬酸盐处理进行防锈处理 使用pH为3.5〜7.0的溶液,在铜箔的表面形成铬酸盐膜。

    Magnetic recording medium, method for manufacturing recording medium and magnetic recording apparatus
    5.
    发明授权
    Magnetic recording medium, method for manufacturing recording medium and magnetic recording apparatus 有权
    磁记录介质,记录介质的制造方法和磁记录装置

    公开(公告)号:US07494725B2

    公开(公告)日:2009-02-24

    申请号:US11085622

    申请日:2005-03-22

    IPC分类号: G11B5/66

    CPC分类号: G11B5/667 G11B5/65 G11B5/7325

    摘要: A grain diameter controlling crystalline layer comprising crystalline grains of a metal selected from the group consisting essentially of Cu, Ni, Rh and Pt was formed on a substrate. Then, deposited atom layer of at least one element selected from the group consisting of oxygen and carbon was formed on the surface of the grain diameter control layer. A magnetic recording layer was deposited on the atoms deposited grain diameter controlling crystalline layer. Then a magnetic recording medium in which the magnetic crystalline grains has small grain diameter and small grain diameter distribution, and the magnetic recording medium shows increased signal to noise ratio at high recording density.

    摘要翻译: 在基板上形成包含选自Cu,Ni,Rh和Pt中的金属的晶粒的晶粒直径控制晶体层。 然后,在粒径控制层的表面上形成从由氧和碳组成的组中选出的至少一种元素的沉积原子层。 在原子沉积粒径控制晶体层上沉积磁记录层。 然后是其中磁晶粒具有小的粒径和小的粒径分布的磁记录介质,并且磁记录介质在高记录密度下显示增加的信噪比。

    PERPENDICULAR MAGNETIC RECORDING MEDIUM AND MAGNETIC RECORDING APPARATUS
    6.
    发明申请
    PERPENDICULAR MAGNETIC RECORDING MEDIUM AND MAGNETIC RECORDING APPARATUS 失效
    全磁记录介质和磁记录装置

    公开(公告)号:US20090011281A1

    公开(公告)日:2009-01-08

    申请号:US12166592

    申请日:2008-07-02

    IPC分类号: G11B5/33

    摘要: According to one embodiment, a perpendicular magnetic recording medium includes a substrate, and a first magnetic layer and a second magnetic layer formed on the substrate, in which supposing that, for the first and second magnetic layers, respectively, uniaxial magnetic anisotropy constants are Ku1 and Ku2, saturation magnetizations are Ms1 and Ms2, anisotropic magnetic fields are Hk1 and Hk2 and the thicknesses are t1 and t2, then following conditions are satisfied that Ku1 and Ku2 are 3×106 erg/cc or more, Ms1 is smaller than Ms2, Hk1 is larger than Hk2 and t1 is larger than t2.

    摘要翻译: 根据一个实施例,垂直磁记录介质包括基板,以及形成在基板上的第一磁性层和第二磁性层,其中,对于第一和第二磁性层,单轴磁各向异性常数分别为Ku1 和Ku2,饱和磁化为Ms1和Ms2,各向异性磁场为Hk1和Hk2,厚度为t1和t2,则满足以下条件:Ku1和Ku2为3×106erg / cc或更大,Ms1小于Ms2,Hk1为 大于Hk2和t1大于t2。