Sealing Ring for Reciprocating Motion
    1.
    发明申请
    Sealing Ring for Reciprocating Motion 有权
    密封圈用于往复运动

    公开(公告)号:US20090166979A1

    公开(公告)日:2009-07-02

    申请号:US12223667

    申请日:2007-02-02

    IPC分类号: F16J15/18

    CPC分类号: F16J15/3204 F16J15/164

    摘要: A sealing ring (21) used for reciprocating motion and having low friction characteristics. The sealing ring is held at one of two members that move relative to each other and slidably in intimate contact with the other. The sealing ring (21) has an end sliding part (21a) having an arcuate cross section and slidably in intimate contact with the other and also has a recessed surface (21c, 21d, 21e) formed in at least either a rear face or both side faces in an axial direction. The sealing ring (21) satisfies the relationships of A/2 and 0.5A

    摘要翻译: 用于往复运动并具有低摩擦特性的密封环(21)。 密封环保持在相对于彼此移动并且可滑动地彼此紧密接触的两个构件中的一个构件中。 密封环(21)具有端部滑动部分(21a),其具有弓形横截面并且可滑动地彼此紧密接触,并且还具有形成在至少后面或两者中的至少一个或两个的凹面(21c,21d,21e) 侧面沿轴向。 密封环(21)满足A / 2 和0.5A

    Sealing ring for reciprocating motion
    2.
    发明授权
    Sealing ring for reciprocating motion 有权
    用于往复运动的密封圈

    公开(公告)号:US07954823B2

    公开(公告)日:2011-06-07

    申请号:US12223667

    申请日:2007-02-02

    IPC分类号: F16J9/20 F16J15/18 F16J15/32

    CPC分类号: F16J15/3204 F16J15/164

    摘要: A sealing ring used for reciprocating motion and having low friction characteristics. The sealing ring is held at one of two members that move relative to each other and slidably in intimate contact with the other. The sealing ring has an end sliding part having an arcuate cross section and slidably in intimate contact with the other and also has a recessed surface formed in at least either a rear face or both side faces in an axial direction. The sealing ring satisfies the relationships of A/2

    摘要翻译: 用于往复运动并具有低摩擦特性的密封环。 密封环保持在相对于彼此移动并且可滑动地彼此紧密接触的两个构件中的一个构件中。 密封环具有端部滑动部分,其具有弓形横截面并且可滑动地彼此紧密接触,并且还具有形成在轴向方向上的至少任一个后表面或两个侧面中的凹陷表面。 密封圈满足A / 2

    RUBBER COMPOSITION
    4.
    发明申请
    RUBBER COMPOSITION 有权
    橡胶组合物

    公开(公告)号:US20140142235A1

    公开(公告)日:2014-05-22

    申请号:US14114252

    申请日:2012-04-27

    IPC分类号: C08K3/36 C08K5/548

    摘要: The present invention provides a rubber composition containing: (A) a rubber component containing from 90 to 100% by mass of at least one kind of diene rubber synthesized by solution polymerization and from 0 to 10% by mass of another kind of diene rubber; (B) silica having a n-hexadecyltrimethylammonium bromide (CTAB) adsorption specific surface area of 140 m2/g or more and less than 180 m2/g measured according to a method described in ASTM D3765-92; (C) at least one silane coupling agent selected from a polysulfide compound and a thioester compound; and (D) a vulcanization accelerator, the rubber composition after vulcanization having an average aggregated aggregate area (nm2) of the silica of 2,200 or less, and thus provides a rubber composition that is improved in low-heat-generation property.

    摘要翻译: 本发明提供一种橡胶组合物,其含有:(A)含有90〜100质量%的通过溶液聚合合成的至少一种二烯系橡胶和0〜10质量%的其他二烯系橡胶的橡胶成分; (B)根据ASTM D3765-92中描述的方法测量的具有140m 2 / g以上且小于180m 2 / g的正十六烷基三甲基溴化铵(CTAB)吸附比表面积的二氧化硅; (C)选自多硫化物化合物和硫酯化合物的至少一种硅烷偶联剂; 和(D)硫化促进剂,硫化后的橡胶组合物的二氧化硅的平均凝集聚集面积(nm2)为2200以下,由此提供低发热性提高的橡胶组合物。

    RUBBER COMPOSITION
    5.
    发明申请
    RUBBER COMPOSITION 有权
    橡胶组合物

    公开(公告)号:US20140051792A1

    公开(公告)日:2014-02-20

    申请号:US14113499

    申请日:2012-04-27

    摘要: The present invention provides a rubber composition containing: (A) a rubber component containing from 90 to 100% by mass of at least one kind of diene rubber synthesized by solution polymerization and from 0 to 10% by mass of another kind of diene rubber; (B) a silica having a n-hexadecyltrimethylammonium bromide (CTAB) adsorption specific surface area of 180 m2/g or more measured according to a method described in ASTM D3765-92; (C) at least one silane coupling agent selected from a polysulfide compound and a thioester compound; and (D) a vulcanization accelerator, the rubber composition after vulcanization having an average aggregated aggregate area (nm2) of the silica of 1,700 or less, and thus provides a rubber composition that is improved in low-heat-generation property.

    摘要翻译: 本发明提供一种橡胶组合物,其含有:(A)含有90〜100质量%的通过溶液聚合合成的至少一种二烯系橡胶和0〜10质量%的其他二烯系橡胶的橡胶成分; (B)根据ASTM D3765-92中记载的方法测定的具有正十六烷基三甲基溴化铵(CTAB)吸附比表面积为180m 2 / g以上的二氧化硅; (C)选自多硫化物化合物和硫酯化合物的至少一种硅烷偶联剂; 和(D)硫化促进剂,硫化后的橡胶组合物的二氧化硅的平均凝集聚集面积(nm2)为1700以下,由此提供了低发热性提高的橡胶组合物。

    METHOD FOR MANUFACTURING RUBBER COMPOSITION
    6.
    发明申请
    METHOD FOR MANUFACTURING RUBBER COMPOSITION 有权
    制造橡胶组合物的方法

    公开(公告)号:US20130296463A1

    公开(公告)日:2013-11-07

    申请号:US13876983

    申请日:2011-10-03

    IPC分类号: C08J3/22

    摘要: The present invention relates to a method for producing a rubber composition containing a rubber component (A) of at least one selected from natural rubbers and synthetic dienic rubbers, a filler containing an inorganic filler (B), a silane coupling agent (C) and at least one vulcanization promoter (D) selected from guanidines, sulfenamides, thiazoles, thiurams, dithiocarbamate salts, thioureas and xanthate salts, wherein the rubber composition is kneaded in at least three stages, in the first stage (X) of kneading, the rubber component (A), all or a part of the inorganic filler (B), and all or a part of the silane coupling agent (C) are kneaded, then in the stage (Y) on and after the second stage of kneading but before the final stage, the vulcanization promoter (D) is added and kneaded, and in the final stage (Z) of kneading, a vulcanizing agent is added and kneaded.

    摘要翻译: 本发明涉及一种橡胶组合物的制造方法,该橡胶组合物含有选自天然橡胶和合成二烯橡胶中的至少一种的橡胶组分(A),含有无机填料(B),硅烷偶联剂(C)和 至少一种选自胍胺,次磺酰胺,噻唑,秋兰姆,二硫代氨基甲酸盐,硫脲和黄原酸盐的硫化促进剂(D),其中橡胶组合物在至少三个阶段中捏合,在捏合的第一阶段(Ⅹ)中, 组分(A),全部或部分无机填料(B)和全部或部分硅烷偶联剂(C)进行混炼,然后在第二阶段揉合之前和之后的阶段(Y) 在最终阶段,加入硫化促进剂(D)并捏合,在捏合的最后阶段(Z)中,加入硫化剂并捏合。

    Epdm composition
    8.
    发明申请
    Epdm composition 审中-公开
    Epdm组成

    公开(公告)号:US20070021565A1

    公开(公告)日:2007-01-25

    申请号:US10569348

    申请日:2004-09-29

    IPC分类号: C08F8/00

    摘要: An EPDM composition, which comprises a blend rubber comprising 100 parts by weight of blend rubber consisting of 20-80% by weight of EPDM containing 5-ethylidene-2-norbornene [ENB] as one type of diene component and 80-20% by weight of EPDM containing dicyclopentadiene [DCPD] as another type of diene component, and 0.5-10 parts by weight of an organic peroxide. Seal parts obtained by vulcanization molding of the EPDM composition show well balanced characteristics, even if dipped in hot water at high temperatures such as 200° C. for 500 hours or 300° C. for 24 hours, particularly with improved compression set characteristics.

    摘要翻译: 一种EPDM组合物,其包含混合橡胶,其包含100重量份由20-80重量%的含有5-亚乙基-2-降冰片烯[ENB]的EPDM组成的共混橡胶作为一种二烯组分和80-20%由 含有二环戊二烯[DCPD]作为另一种二烯成分的EPDM的重量和0.5-10重量份的有机过氧化物。 即使在高温如200℃,500小时或300℃的热水中浸渍24小时,特别是具有改进的压缩永久变形特性,通过EPDM组合物的硫化成型获得的密封部件显示均匀的特性。

    Rubber composition
    9.
    发明授权
    Rubber composition 有权
    橡胶组成

    公开(公告)号:US08980990B2

    公开(公告)日:2015-03-17

    申请号:US14114258

    申请日:2012-04-27

    摘要: The present invention provides a rubber composition containing: (A) a rubber component containing 10% by mass or more of at least one kind of rubber selected from diene rubber synthesized by emulsion polymerization and natural rubber and 90% by mass or less of another kind of diene rubber; (B) silica having a n-hexadecyltrimethylammonium bromide (CTAB) adsorption specific surface area of 140 m2/g or more and less than 180 m2/g measured according to a method described in ASTM D3765-92; (C) at least one silane coupling agent selected from a polysulfide compound and a thioester compound; and (D) a vulcanization accelerator, the rubber composition after vulcanization having an average aggregated aggregate area (nm2) of the silica of 2,300 or less, and thus provides a rubber composition that is improved in low-heat-generation property.

    摘要翻译: 本发明提供一种橡胶组合物,其含有:(A)含有10质量%以上的选自通过乳液聚合和天然橡胶合成的二烯橡胶中的至少一种橡胶的橡胶组分和90质量%以下的其他橡胶组合物 的二烯橡胶; (B)根据ASTM D3765-92中描述的方法测量的具有140m 2 / g以上且小于180m 2 / g的正十六烷基三甲基溴化铵(CTAB)吸附比表面积的二氧化硅; (C)选自多硫化物化合物和硫酯化合物的至少一种硅烷偶联剂; 和(D)硫化促进剂,硫化后的橡胶组合物的二氧化硅的平均凝集聚集面积(nm2)为2300以下,因此提供了低发热性提高的橡胶组合物。

    Rubber composition
    10.
    发明授权
    Rubber composition 有权
    橡胶组成

    公开(公告)号:US08980988B2

    公开(公告)日:2015-03-17

    申请号:US14113499

    申请日:2012-04-27

    摘要: The present invention provides a rubber composition containing: (A) a rubber component containing from 90 to 100% by mass of at least one kind of diene rubber synthesized by solution polymerization and from 0 to 10% by mass of another kind of diene rubber; (B) a silica having a n-hexadecyltrimethylammonium bromide (CTAB) adsorption specific surface area of 180 m2/g or more measured according to a method described in ASTM D3765-92; (C) at least one silane coupling agent selected from a polysulfide compound and a thioester compound; and (D) a vulcanization accelerator, the rubber composition after vulcanization having an average aggregated aggregate area (nm2) of the silica of 1,700 or less, and thus provides a rubber composition that is improved in low-heat-generation property.

    摘要翻译: 本发明提供一种橡胶组合物,其含有:(A)含有90〜100质量%的通过溶液聚合合成的至少一种二烯系橡胶和0〜10质量%的其他二烯系橡胶的橡胶成分; (B)根据ASTM D3765-92中记载的方法测定的具有正十六烷基三甲基溴化铵(CTAB)吸附比表面积为180m 2 / g以上的二氧化硅; (C)选自多硫化物化合物和硫酯化合物的至少一种硅烷偶联剂; 和(D)硫化促进剂,硫化后的橡胶组合物的二氧化硅的平均凝集聚集面积(nm2)为1700以下,由此提供了低发热性提高的橡胶组合物。