An object of the invention is to find out intermediates usful for the synthesis of pyrazol-fused ring derivatives (such as 7-phenylpyrazolo[1,5-a]pyridine derivatives) and a method for producing the same. A method for producing compound represented by the general formula (II), wherein Z1 and Z2 each independently represents a methine group or a nitrogen atom; R1 represents an ethyl group or the like; R5 represents a hydrogen atom or the like; R2 and R3 each independently represents a C1-6 alkyl group or the like, salts thereof, or solvates of both, comprising the step of: reacting a compound represented by the general formula (I), wherein Z1, Z2, R5, R1, R2 and R3 each has the same definition as described above, with an organometallic reagent; and then reacting the resulting product with pentafluoroiodobenzene.
摘要翻译:本发明的目的是找出有用于合成吡唑稠合环衍生物(如7-苯基吡唑并[1,5-a]吡啶衍生物)的中间体及其制备方法。 由通式(II)表示的化合物,其中Z 1和Z 2各自独立地表示次甲基或氮原子的方法; R 1表示乙基等; R 5表示氢原子等; R 2和R 3各自独立地表示C 1-6烷基等,其盐或两者的溶剂合物,包括 步骤:使通式(I)表示的化合物,其中Z 1,Z 2,R 5,R 5, 1,R 2和R 3各自具有与上述相同的定义与有机金属试剂; 然后使所得产物与五氟碘苯反应。
摘要:
A steel for an induction hardening including, by mass %, C: more than 0.75% to 1.20%, Si: 0.002 to 3.00%, Mn: 0.20 to 2.00%, S: 0.002 to 0.100%, Al: more than 0.050% to 3.00%, P: limited to 0.050% or less, N: limited to 0.0200% or less, O: limited to: 0.0030% or less, and the balance composing of iron and unavoidable impurities, wherein an Al content and a N content satisfy, by mass %, Al−(27/14)×N>0.050%.
摘要:
This steel for a machine structure contains, in mass %: C: 0.40% to less than 0.75%; Si: 0.01% to 3.0%; Mn: 0.1% to 1.8%; S: 0.001% to 0.1%; Al: more than 0.1% and not more than 1.0%; N: 0.001% to 0.02%; and P: limited to not more than 0.05%, with a balance including Fe and inevitable impurities, in which the steel satisfies 139.38 ≦214×[C]+30.6×[Si]+42.8×[Mn]−14.7×[Al]≦177 and 0.72≦[C]+1/7×[Si]+1/5×[Mn]
摘要:
The present invention provides a steel for nitriding with a composition including, by mass %: C: 0.10% to 0.20%; Si: 0.01% to 0.7%; Mn: 0.2% to 2.0%; Cr: 0.2% to 2.5%; Al: 0.01% to less than 0.19%; V: over 0.2% to 1.0%; Mo: 0% to 0.54%; N: 0.001% to 0.01%; P limited to not more than 0.05%; S limited to not less than 0.2%; and a balance including Fe and inevitable impurities, the composition satisfying 2≦[V]/[C]≦10, where [V] is an amount of V by mass % and [C] is an amount of C by mass %, in which the steel for nitriding has a microstructure containing bainite of 50% or more in terms of an area percentage.
摘要:
Steel for induction hardening wherein coarsening of austenite crystal grains can be prevented even at a high temperature of over 1100° C. such as which occurs at projecting parts of steel parts at the time of induction hardening, the steel for induction hardening characterized by containing, by mass %, C: 0.35 to 0.6%, Si: 0.01 to 1%, Mn: 0.2 to 1.8%, S: 0.001 to 0.15%, Al: 0.001 to 1%, Ti: 0.05 to 0.2%, and Nb: 0.001 to 0.04%, restricting N: 0.0060% or less, P: 0.025% or less, and O: 0.0025% or less, satisfying Nb/Ti≧0.015, and having a balance of iron and unavoidable impurities.
摘要:
A communication system includes a first communication device that transmits transmission data containing user data and control data, and a second communication device that receives the transmission data from the first communication device. The second communication device includes a temporary storing unit that temporarily stores therein the received transmission data, and a space-insufficient-information transmitting unit that transmits, when an amount of the transmission data stored in the temporary storing unit exceeds a first threshold, space insufficient information indicating that available storage space of the temporary storing unit is insufficient to the first communication device. The first communication device includes a transmission control unit that transmits, when receiving the space insufficient information from the second communication device, transmission data excluding the user data from the transmission data to the second communication device, and that resumes, when receiving space-insufficient dissolution information from the second communication device, transmission of the user data.
摘要:
This case hardening steel has a chemical composition including, by mass %: C: 0.1 to 0.6%; Si: 0.02 to 1.5%; Mn: 0.3 to 1.8%; P: 0.025% or less; S: 0.001 to 0.15%; Al: over 0.05 to 1.0%; Ti: 0.05 to 0.2%; N: 0.01% or less; and O: 0.0025% or less, and further including, by mass %, one or more of Cr: 0.4 to 2.0%, Mo: 0.02 to 1.5%, Ni: 0.1 to 3.5%, V: 0.02 to 0.5%, and B: 0.0002 to 0.005%, and the balance consisting of iron and unavoidable impurities.
摘要:
A steel for a carburizing and a carburized steel component having a steel portion and a carburized layer with a thickness of more than 0.4 mm to less than 2 mm which is formed on an outside of the steel portion. A chemical composition of the steel for the carburizing and the steel portion of the carburized steel component satisfies simultaneously equations of a hardness parameter, a hardenability parameter, and a TiC precipitation parameter.
摘要:
The present invention provides a spring steel, which is finally formed into a spring, by making use of, at a maximum, the temper softening resistance effect due to alloying elements while suppressing the formation of hard inclusions of SiO2 and the generation of decarburization, which may cause deterioration of fatigue characteristics of the spring. The spring steel is characterized by comprising, in % by mass, C: 0.50 to 0.70%, Si: 1.00 to 5.00%, Mn: 0.30 to 2.00%, P: 0.0002 to 0.0500%, S: 0.0002 to 0.0500%, Cr: 0.10 to 3.50%, Al: 0.0005 to 0.0500%, and N: 0.0020 to 0.0100%, with the balance being Fe and inevitable impurities, wherein the H-value defined by the following equation (a) is 160 or more, and the C-value defined by the following equation (b) is 3.25 or less: H=33.6[C]+10.0[Si]+5.95[Mn]+11.1[Cr]+90.0 (a), and C=[Si]/[Mn] (b).
摘要:
The present invention provides a steel product for gas carburizing used for manufacturing a carburized steel part. In the above steel product for gas carburizing, a composition of a base metal contains, in mass %, C: 0.1 to 0.4%, Si: exceeding 1.2 to 4.0%, Mn: 0.2 to 3.0%, Cr: 0.5 to 5.0%, Al: 0.005 to 0.1%, S: 0.001 to 0.3%, N: 0.003 to 0.03%, and O: limited to 0.0050% or less, and P: limited to 0.025% or less, and when the contents of Si, Mn, and Cr (mass %) are set to [Si %], [Mn %], and [Cr %], Expression (1) below is satisfied, and an alloy shortage layer satisfying Expression (2) below exists in a range from its surface to 2 to 50 μm in depth. 32≧3.5[Si %]+[Mn %]+3[Cr %]>9 (1) 3.5[Si %]+[Mn %]+3[Cr %]≦9 (2)