COATED POLYESTER FILM
    1.
    发明申请
    COATED POLYESTER FILM 审中-公开
    涂层聚酯薄膜

    公开(公告)号:US20110209901A1

    公开(公告)日:2011-09-01

    申请号:US12671648

    申请日:2008-08-01

    摘要: A method of improving the flexibility of a coated polyester substrate for an electronic device comprising a coated polyester substrate layer and an electrode layer comprising conductive material, said method comprising: (a) providing a polyester film; and (b) disposing an organic/inorganic hybrid coating on one or both surfaces of said polyester film, wherein said coating is derived from a coating composition comprising a low molecular weight reactive component selected from monomeric acrylates and/or an unsaturated oligomeric component selected from acrylates, polyether acrylates, epoxy acrylates and polyester acrylates; a solvent; and inorganic particles, and optionally further comprising a photoinitiator.

    摘要翻译: 一种提高包含涂覆聚酯基底层和包含导电材料的电极层的电子器件的涂覆聚酯基底的柔性的方法,所述方法包括:(a)提供聚酯薄膜; 和(b)在所述聚酯膜的一个或两个表面上设置有机/无机混合涂层,其中所述涂层衍生自包含选自单体丙烯酸酯和/或不饱和低聚组分的低分子量反应性组分的涂料组合物, 丙烯酸酯,聚醚丙烯酸酯,环氧丙烯酸酯和聚酯丙烯酸酯; 溶剂; 和无机颗粒,并且任选地还包含光引发剂。

    Manufacturing process for coated polyester film
    5.
    发明授权
    Manufacturing process for coated polyester film 有权
    涂层聚酯薄膜的制造工艺

    公开(公告)号:US08802226B2

    公开(公告)日:2014-08-12

    申请号:US12278819

    申请日:2007-02-09

    摘要: A method of preventing or minimizing the formation of haze in a biaxially oriented polyester film during the annealing of said film above its glass transition temperature, said method comprising: (a) selecting a biaxially oriented polyester film having glass transition temperature (Tg (° C.)); (b) disposing a coating on one or both surfaces of said biaxially oriented film; (c) annealing said coated biaxially oriented polyester film at a temperature above its glass transition temperature, wherein said coating composition is selected from: (i) an organic coating comprising a low molecular weight reactive diluent; an unsaturated oligomer; a solvent; and a photoinitiator; (ii) an organic/inorganic hybrid coating comprising a low molecular weight reactive component and/or an unsaturated oligomeric component; a solvent; and inorganic particles, and optionally further comprising a photoinitiator; (iii) a predominantly inorganic hardcoat comprising inorganic particles contained in a polymerisable predominantly inorganic matrix; and (iv) a composition comprising a cross-linkable organic polymer selected from polyethylene imine (PEI), polyester and polyinylalcohol (PVOH), and a cross-linking agent.

    摘要翻译: 一种防止或最小化在所述膜退火温度以上的玻璃化转变温度下在双轴取向聚酯膜中形成雾度的方法,所述方法包括:(a)选择具有玻璃化转变温度(Tg(℃) 。)); (b)在所述双轴取向膜的一个或两个表面上设置涂层; (c)在高于其玻璃化转变温度的温度下退火所述涂覆的双轴取向聚酯膜,其中所述涂料组合物选自:(i)包含低分子量反应性稀释剂的有机涂层; 不饱和低聚物 溶剂; 和光引发剂; (ii)包含低分子量反应性组分和/或不饱和低聚组分的有机/无机混合涂层; 溶剂; 和无机颗粒,并且任选地还包含光引发剂; (iii)主要为无机硬质涂层,其包含可聚合的主要为无机基质中的无机颗粒; 和(iv)包含选自聚乙烯亚胺(PEI),聚酯和聚乙烯醇(PVOH))和交联剂的可交联有机聚合物的组合物。

    Conformable copolyester film
    7.
    发明授权
    Conformable copolyester film 有权
    合适的共聚酯膜

    公开(公告)号:US07078105B2

    公开(公告)日:2006-07-18

    申请号:US10485680

    申请日:2002-07-10

    摘要: A conformable oriented polymeric film comprising a layer of copolyester derived from: (i) one or more diol(s); (ii) an aromatic dicarboxylic acid; and (iii) one or more aliphatic dicarboxylic acid(s) of the general formula CnH2n(COOH)2 wherein n is 2 to 8, wherein the aromatic dicarboxylic acid is present in the copolyester in an amount of from 60 to 85 mole % based on the total amount of dicarboxylic acid components in the copolyester, wherein the copolyester is a random or alternating copolyester, and wherein after deformation by subjecting and maintaining the film to 7% strain, the stress within the film immediately after deformation dissipates to a residual value of less than 60% of the original value within 10 minutes of said deformation; and use thereof as a conformable medium for signage, advertising, graphic art and other display applications or as an overlaminate for such media.

    摘要翻译: 包含衍生自(i)一种或多种二醇的共聚酯层的适形取向聚合物膜; (ii)芳族二羧酸; 和(iii)一种或多种通式为C n H 2n(COOH)2的脂族二羧酸,其中n为2 至8,其中所述芳族二羧酸以所述共聚酯中二羧酸组分的总量计为60至85摩尔%的量存在于所述共聚酯中,其中所述共聚酯是无规或交替的共聚酯,并且其中在变形后 通过使膜保持7%的应变,立即变形后的膜内的应力在所述变形的10分钟内消失至小于原值的60%的残值; 并将其用作标牌,广告,图形艺术和其他显示应用的合适介质,或作为此类介质的叠层。

    MANUFACTURING PROCESS FOR COATED POLYESTER FILM
    10.
    发明申请
    MANUFACTURING PROCESS FOR COATED POLYESTER FILM 有权
    涂层聚酯薄膜的制造工艺

    公开(公告)号:US20090011228A1

    公开(公告)日:2009-01-08

    申请号:US12278819

    申请日:2007-02-09

    IPC分类号: B32B27/08 B05D3/00

    摘要: A method of preventing or minimising the formation of haze in a biaxially oriented polyester film during the annealing of said film above its glass transition temperature, said method comprising: (a) selecting a biaxially oriented polyester film having glass transition temperature (Tg (° C.)); (b) disposing a coating on one or both surfaces of said biaxially oriented film; (c) annealing said coated biaxially oriented polyester film at a temperature above its glass transition temperature, wherein said coating composition is selected from: (i) an organic coating comprising a low molecular weight reactive diluent; an unsaturated oligomer; a solvent; and a photoinitiator; (ii) an organic/inorganic hybrid coating comprising a low molecular weight reactive component and/or an unsaturated oligomeric component; a solvent; and inorganic particles, and optionally further comprising a photoinitiator; (iii) a predominantly inorganic hardcoat comprising inorganic particles contained in a polymerisable predominantly inorganic matrix; and (iv) a composition comprising a cross-linkable organic polymer selected from polyethylene imine (PEI), polyester and polyinylalcohol (PVOH), and a cross-linking agent.

    摘要翻译: 一种防止或最小化在所述膜退火温度以上的玻璃化转变温度下在双轴取向聚酯膜中形成雾度的方法,所述方法包括:(a)选择具有玻璃化转变温度(Tg(℃) 。)); (b)在所述双轴取向膜的一个或两个表面上设置涂层; (c)在高于其玻璃化转变温度的温度下退火所述涂覆的双轴取向聚酯膜,其中所述涂料组合物选自:(i)包含低分子量反应性稀释剂的有机涂层; 不饱和低聚物 溶剂; 和光引发剂; (ii)包含低分子量反应性组分和/或不饱和低聚组分的有机/无机混合涂层; 溶剂; 和无机颗粒,并且任选地还包含光引发剂; (iii)主要为无机硬质涂层,其包含可聚合的主要为无机基质中的无机颗粒; 和(iv)包含选自聚乙烯亚胺(PEI),聚酯和聚乙烯醇(PVOH))和交联剂的可交联有机聚合物的组合物。