Vascular stents
    1.
    发明授权
    Vascular stents 有权
    血管支架

    公开(公告)号:US08911857B2

    公开(公告)日:2014-12-16

    申请号:US13362477

    申请日:2012-01-31

    申请人: Carlo Civelli

    发明人: Carlo Civelli

    摘要: The disclosure describes a coating for medical implants, in particular, vascular stents, said coating comprising silicon dioxide, towards medical implants with a coating containing silicon dioxide and towards a method for their production. The coating can contain additional admixtures and have functionalization coats. The substrate of the coating is produced from a durable material, preferably from a stainless steel.

    摘要翻译: 本公开描述了用于医疗植入物的涂层,特别是血管支架,所述涂层包含二氧化硅,朝向具有包含二氧化硅的涂层的医疗植入物并朝向其生产方法。 涂层可以含有额外的混合物并具有官能化涂层。 涂层的基材由耐用材料制成,优选由不锈钢制成。

    Bone repair material and method for producing the same
    3.
    发明授权
    Bone repair material and method for producing the same 有权
    骨修复材料及其制造方法

    公开(公告)号:US08784864B2

    公开(公告)日:2014-07-22

    申请号:US13147082

    申请日:2010-01-29

    IPC分类号: A61K33/24 A61K9/00

    摘要: Bone repair materials are disclosed, from which ions are hardly eluted in living body and which are superior in apatite-forming ability and resistance to apatite peeling and have a scratch resistance high enough for practical use. The material comprises a substrate made of titanium or titanium alloys, and a surface layer, made substantially of titanium oxide, along the surface of the substrate. The substrate has on the surface thereof irregularities of from 1 nm to 10 μm in average in both width and depth. The layer has a zeta potential of +4.5 mV or more under an aqueous solution environment of pH 6 to 8, and a critical scratch resistance of 35 mN or more when vibration 100 μm in amplitude is added to a stylus with a spring constant of 200 g/mm on the surface layer and the stylus is moved at a rate of 10 mm/sec under a load increasing at a rate of 100 mN/min.

    摘要翻译: 公开了骨修复材料,其中离子几乎不在生物体中洗脱,并且磷灰石形成能力和磷灰石剥离性都优异,并且具有足够高的实用用途的耐擦伤性。 该材料包括由钛或钛合金制成的基材,以及基本上由氧化钛制成的表面层。 基板在表面上的宽度和深度均匀地具有1nm至10μm的不规则性。 在pH6〜8的水溶液环境下,该层的ζ电位为+4.5mV以上,当振幅为100μm的振幅加入弹簧常数为200的触针时,临界耐擦伤性为35mN以上 表面层上的g / mm和触针以10毫米/秒的速率移动,负载以100毫微米/分钟的速率增加。

    Nanosurface
    5.
    发明授权
    Nanosurface 有权
    纳米表面

    公开(公告)号:US08632836B2

    公开(公告)日:2014-01-21

    申请号:US12298884

    申请日:2008-07-08

    IPC分类号: B05D3/10 C25C3/00

    摘要: The invention relates to a method for modification of a biocompatible component comprising the steps of a) providing a biocompatible component at least partly covered by metallic oxide; and b) treating at least a part of said component, which part is covered by said metallic oxide, with an aqueous composition comprising oxalic acid; whereby a modified metallic oxide is obtained. The invention also relates to a biocompatible component comprising a substrate having a surface comprising a) a microstructure comprising pits separated by plateus and/or ridges; and b) a primary nanostructure being superimposed on said microstructure, said primary nanostructure comprising depressions arranged in a wave-like formation.