摘要:
Provided are a method of producing a titanium-containing rare earth-iron-nitrogen anisotropic magnetic powder having good magnetic properties, and secondary particles for a titanium-containing anisotropic magnetic powder. The method includes: obtaining a first precipitate containing R, iron, and titanium by mixing a first precipitating agent with a solution containing R, iron, and titanium, wherein R is at least one selected from Sc, Y, Pr, Nd, Pm, Sm, Gd, Tb, Dy, Ho, Er, Tm, and Lu; obtaining a second precipitate containing R and iron by mixing, in the presence of the first precipitate, a second precipitating agent with a solution containing R and iron; obtaining an oxide containing R, iron, and titanium by calcining the second precipitate; obtaining a partial oxide by heat treating the oxide in a reducing gas atmosphere; obtaining alloy particles by reducing the partial oxide; and obtaining an anisotropic magnetic powder by nitriding the alloy particles.
摘要:
An anisotropic rare earth sintered magnet represented by the formula (R1-aZra)x(Fe1-b COb)100-x-y(M11-cM2c)y where R is at least one element selected from rare earth elements and Sm is essential; M1 is at least one of V, Cr, Mn, Ni, Cu, Zn, Ga, Al, and Si; M2 is at least one of Ti, Nb, Mo, Hf, Ta, and W; and x, y, a, b, and c each satisfy certain conditions. The anisotropic rare earth sintered magnet includes 80% by volume or more of a main phase composed of a compound of a ThMn12 type crystal, the main phase having an average crystal grain size of 1 μm or more, and containing an R-rich phase and an R(Fe,Co)2 phase in a grain boundary portion. A method for producing the anisotropic rare earth sintered magnet is also described.
摘要:
A shaped body of anisotropic magnetic material based on the Sm-Fe-N system which has a crystalline, hard magnetic phase with a Th.sub.2 Zn.sub.17 crystal structure, wherein N atoms are incorporated in the crystal lattice, is produced by compacting a powder Sm-Fe preliminary product with an Sm-Fe phase having a magnetically isotropic structure, followed by hot-shaping to provide an intermediate product with a Sm-Fe phase having a magnetically anisotropic structure, followed by heat treating the intermediate product in a nitrogen atmosphere to provide a Sm-Fe-N hard magnetic phase.
摘要:
A magnetic powder and a method for fabricating the same according to an embodiment of the present disclosure are provided. The magnetic powder is powder particles synthesized using a mixture of a rare earth oxide, a raw material, a metal, a metal oxide and a reducing agent, wherein the powder particles are single-phase, the raw material includes at least one of Fe and Co, the metal includes at least one of Ti, Zr, Mn, Mo, V and Si, and the metal oxide includes at least one of MnO2, MoO3, V2O5, SiO2, ZrO2 and TiO2.
摘要:
New magnetic materials containing cerium, iron, and small additions of a third element are disclosed. These materials comprise compounds Ce(Fe12−xMx) where x=1-4, having the ThMn12 tetragonal crystal structure (space group I4/mmm, #139). Compounds with M=B, Al, Si, P, S, Sc, Co, Ni, Zn, Ga, Ge, Zr, Nb, Hf, Ta, and W are identified theoretically, and one class of compounds based on M=Si has been synthesized. The Si cognates are characterized by large magnetic moments (4πMs greater than 1.27 Tesla) and high Curie temperatures (264≦Tc≦305° C.). The Ce(Fe12−xMx) compound may contain one or more of Ti, V, Cr, and Mo in combination with an M element. Further enhancement in Tc is obtained by nitriding the Ce compounds through heat treatment in N2 gas while retaining the ThMn12 tetragonal crystal structure; for example CeFe10Si2N1.29 has Tc=426° C.
摘要:
Provided is a magnetic compound represented by the formula (R(1-x)Zrx)a(Fe(1-y)Coy)bTcMdAe (wherein R represents one or more rare earth elements, T represents one or more elements selected from the group consisting of Ti, V, Mo, and W, M represents one or more elements selected from the group consisting of unavoidable impurity elements, Al, Cr, Cu, Ga, Ag, and Au, A represents one or more elements selected from the group consisting of N, C, H, and P, 0≦x≦0.5, 0≦y≦0.6, 4≦a≦20, b=100−a−c−d, 0
摘要:
A magnetic material is expressed by a composition formula: (R1-xZx)aMbTc, and includes a main phase having a ThMn12 crystal structure. In the ThMn12 crystal structure, when an amount of the element Z occupying 2a site is Z2a atomic percent, an amount of the element Z occupying 8i site is Z8i atomic percent, an amount of the element Z occupying 8j site is Z8j atomic percent, and an amount of the element Z occupying 8f site is Z8f atomic percent, Z2a, Z8i, Z8j, and Z8f satisfy (Z8i+Z8j+Z8f)/(Z2a+Z8i+Z8j+Z8f)
摘要:
An magnetic material is a magnetic material expressed by a composition formula: (R1-xYx)aMbTcAd, which includes a main phase consisting of a ThMn12 type crystal phase. 30 atomic percent or more of the element M in the composition formula is Fe.
摘要:
Disclosed is a magnetic material for a high frequency wave which has high magnetic permeability and small eddy-current loss, particularly a magnetic material for a high frequency wave which can be used suitably in an information device which works in a high frequency field of 1 GHz or higher. Specifically disclosed is a composite magnetic material for a high frequency wave, which comprises a (rare earth element)-(iron)-(nitrogen)-based magnetic material and a (rare earth element)-(iron)-(nitrogen)-based magnetic material whose surface is coated with a ferrite magnetic material.
摘要:
A single phase consisting of a ThMn12 phase can be obtained by having the composition thereof represented by a general formula R(Fe100-y-wCowTiy)xSizAv (in the general formula, R is at least one element selected from rare earth elements (here the rare earth elements signify a concept inclusive of Y), Nd accounts for 50 mol % or more of R, and A is N and/or C) in which the molar ratios in the general formula are such that x=10 to 12.5, y=(8.3−1.7×z) to 12.3, z=0.1 to 2.3, v=0.1 to 3 and w=0 to 30, and the relation (Fe+Co+Ti+Si)/R>12 is satisfied.
摘要翻译:由ThMn 12相组成的单相可以通过使其组成由通式R(Fe)100-y w / Co (在通式中,R是选自至少一个元素) 来自稀土元素(这里的稀土元素表示包括Y的概念),Nd占R的50mol%以上,A是N和/或C),其中通式中的摩尔比使得 x = 10〜12.5,y =(8.3-1.7×z)〜12.3,z = 0.1〜2.3,v = 0.1〜3,w = 0〜30,关系式(Fe + Co + Ti + Si) 12满足。