公开(公告)号:US11753500B2
公开(公告)日:2023-09-12
申请号:US17426228
申请日:2020-01-21
Applicant: UNITIKA LTD.
Inventor: Ayumi Yanaka , Yumeto Fukubayashi , Takatoshi Murakami
IPC: C08G59/40 , C08G59/42 , C08L63/00 , C08J5/24 , B32B27/38 , C08G59/02 , C08G59/22 , C08G59/32 , C08J5/04
CPC classification number: C08G59/4042 , C08G59/022 , C08G59/22 , C08G59/32 , C08G59/4238 , C08J5/04 , C08J5/249 , C08L63/00 , C08J2367/00 , C08L2201/08 , C08L2203/20
Abstract: The present invention provides an epoxy resin solution, from which an epoxy resin-cured product adequately excellent in heat-resisting properties and dielectric properties can be obtained with adequately good working properties ensured. The present invention relates to an epoxy resin solution containing at least a curing agent and an epoxy resin mixed in an organic solvent, wherein the curing agent comprises an imide group-containing curing agent having 1-4 imide groups and 2-4 glycidyl group-reactive functional groups in a molecule.
-
公开(公告)号:US20220195187A1
公开(公告)日:2022-06-23
申请号:US17603399
申请日:2020-04-17
Applicant: UNITIKA LTD.
Inventor: Miho Asai , Junichi Mii
Abstract: A polyamide resin composition including a semi-aromatic polyamide (A) having a melting point of 290 to 330° C. and a fibrous reinforcing material (B), wherein the polyamide resin composition has an amount of creep strain of 2.0% or less in the flow direction after a lapse of 100 hours under the measurement conditions of a temperature of 100° C. and a tensile load of 75 MPa.
-
公开(公告)号:US11254814B2
公开(公告)日:2022-02-22
申请号:US17051943
申请日:2020-04-21
Applicant: UNITIKA LTD.
Inventor: Yutaka Nabeshima
Abstract: The present invention is to provide a resin composition capable of producing a molded product sufficiently excellent in hydrolysis resistance and mold release characteristics and having an excellent balance between heat resistance and fluidity, even if a heat stabilizer and a mold release agent are contained.
The present invention relates to a resin composition, comprising: (A) a polyarylate resin; (B) a melt-polymerized polycarbonate resin; (C) a specific phosphite compound; and (D) a dipentaerythritol fatty acid ester, a mass ratio (A/B) of the (A) polyarylate resin and the (B) melt-polymerized polycarbonate resin being from 2/98 to 98/2, and the resin composition having a Vicat softening point of 140° C. or higher.-
公开(公告)号:US20220033584A1
公开(公告)日:2022-02-03
申请号:US17276216
申请日:2019-10-23
Applicant: UNITIKA LTD.
Inventor: Makoto Nakai , Yuki Takubo , Yusuke Yagi
IPC: C08G69/28
Abstract: A flexible polyamide including a unit formed from an aliphatic dicarboxylic acid (A1) having 18 or more carbon atoms and/or a unit formed from an aliphatic diamine (B1) having 18 or more carbon atoms, wherein the polyamide has a total content of 10 to 90% by mass of the unit formed from (A1) and the unit formed from (B1) and has a melting point of 240° C. or higher.
-
公开(公告)号:US20210403710A1
公开(公告)日:2021-12-30
申请号:US17289669
申请日:2019-10-28
Applicant: UNITIKA LTD.
Inventor: Yukinari NEGI , Yoshihito KISARA , Masako TANAKA
Abstract: The present invention provides a thermoplastic resin pellet capable of obtaining a molded body which is excellent in metallic coloring properties, surface smoothness property, and flow mark suppressing properties, and has a sufficient metallic appearance. The present invention relates a metallic-tone thermoplastic resin pellet comprising 100 parts by weight of a thermoplastic resin (A), 0.5 to 10 parts by mass of metallic particles (B), and 0 to 10 parts by mass of plate-like, fibrous and/or granular filler (C), wherein the pellet has a cylindrical shape having a circular or elliptical cross section perpendicular to the longitudinal direction, and the pellet has a length of 0.5 to 2.8 mm and a cross-sectional major diameter of 0.5 to 2.8 mm.
-
公开(公告)号:US11040515B2
公开(公告)日:2021-06-22
申请号:US16333711
申请日:2017-09-20
Applicant: UNITIKA LTD.
Inventor: Mari Shimizu , Kouhei Tanaka , Nobuyasu Okumura
IPC: B32B7/06 , B29C55/02 , B29C55/14 , B29C55/12 , B32B27/30 , B32B27/36 , B32B27/00 , B32B27/26 , C08J5/18 , B29K29/00 , B29K67/00 , B29K33/00
Abstract: There is provided a release film comprising a substrate film and a resin layer provided on at least one surface of a substrate film, wherein the resin layer comprises 100 parts by mass of an acid-modified polyolefin resin, 1 to 20 parts by mass of a crosslinking agent and 10 to 1,000 parts by mass of a polyvinyl alcohol having a saponification rate of 99% or lower.
-
公开(公告)号:US10954396B2
公开(公告)日:2021-03-23
申请号:US16753569
申请日:2018-10-01
Applicant: UNITIKA LTD.
Inventor: Hirotaka Takeda , Chikako Yamada
Abstract: The present invention provides a nickel nanowires-containing paste having an adequately high thermal curing rate even under comparatively low temperature, which is excellent in functional properties such as an electrical conductivity, strength properties (in particular, a bending property), a water-resisting property, a salt water-resisting property and electromagnetic-wave shielding properties, from which a cured structure excellent in an electrical conductivity can be obtained even if it is stored for a long time. The present invention relates to a paste comprising nickel nanowires, an alkoxy-alkylated polyamide and a glycol.
-
公开(公告)号:US20200317911A1
公开(公告)日:2020-10-08
申请号:US16303911
申请日:2017-05-18
Applicant: UNITIKA LTD.
Inventor: Yutaka NABESHIMA
Abstract: The present invention provides a resin composition excellent in a molding stability, which can be molded into a molded article excellent in a dust generation resistance, a heat resistance, a dimensional stability, and an external appearance, and a molded article obtained by molding the same. The present invention relates to a resin composition comprising a polyarylate resin, a polycarbonate resin, silica particles having an average particle diameter of 0.5 to 10 μm and a phosphite ester compound shown by a general formula (I), wherein a mass ratio of the polyarylate resin and the polycarbonate resin is 25/75 to 90/10, a content of the silica particles is 5 to 60 parts by mass with respect to 100 parts by mass of a total amount of the polyarylate resin and the polycarbonate resin and a content of the phosphite ester compound is 0.01 to 1 part by mass with respect to 100 parts by mass of a total amount of the polyarylate resin and the polycarbonate resin: (wherein m1 and m2 respectively and independently are an integer of 0 to 5; R1 and R2 respectively and independently represent an alkyl group having 1 to 12 carbon atoms, which may have a substituent group; four R3s respectively and independently represent an alkylene group having 1 to 5 carbon atoms).
-
公开(公告)号:US10400446B2
公开(公告)日:2019-09-03
申请号:US14914045
申请日:2014-08-26
Applicant: UNITIKA LTD.
Inventor: Nobutaka Takeuchi , Hitoshi Kourogi , Yuki Horikoshi
IPC: D06M15/233 , D06M15/263 , B32B5/02 , B32B5/26 , G01N21/59 , B32B27/30 , E04B1/94 , A47H23/08 , B32B27/12 , D06M15/327 , G01N21/84 , D06M101/00
Abstract: The present invention addresses the problem of providing a transparent, noncombustible sheet having excellent transparency but minimized blurring and color bleeding. The means for addressing the problem is a transparent noncombustible sheet including a glass fiber fabric and a cured resin composition layer impregnated into the glass fiber fabric; wherein, the cured resin composition layer is formed by curing a resin composition including a curable resin and a bifunctional (meth)acrylate, total light transmittance of the transparent noncombustible sheet being no less than 80%, and haze of the transparent noncombustible sheet being no more than 30%.
-
公开(公告)号:US20190144329A1
公开(公告)日:2019-05-16
申请号:US16097033
申请日:2016-11-01
Inventor: Yoshiyuki INAKA , Takaharu MIYAZAKI , Yoshito NAWA , Daisuke NISHINAKA , Tomoki SEKIDA
Abstract: A glass composition of the present disclosure includes, in wt %, 50≤SiO2≤54, 25≤B2O3≤30, 12≤Al2O3≤15, 0.5≤MgO≤1.9, 3.0≤CaO≤5.5, 0≤ZnO≤3.5, 0.1≤Li2O≤0.5, and 0.1≤Na2O≤0.3, and has a permittivity of less than 5.0 at a frequency of 1 MHz. The glass composition of the present disclosure has a low permittivity. The use of this glass composition can reduce the occurrence of devitrification and the inclusion of bubbles in glass fibers to be formed or in a shaped glass material to be formed even when the glass fibers have a small fiber diameter or the shaped glass material has a small thickness.
-
-
-
-
-
-
-
-
-