FABRIC FOR AIRBAG
    94.
    发明申请
    FABRIC FOR AIRBAG 审中-公开
    安全气囊布

    公开(公告)号:US20160273157A1

    公开(公告)日:2016-09-22

    申请号:US14777828

    申请日:2014-03-18

    申请人: TOYOBO CO., LTD.

    发明人: Tsutomu Akechi

    IPC分类号: D06M15/59 D03D1/02 B60R21/235

    摘要: The purpose of the present invention is to provide a base fabric for an airbag which has a low initial air permeability, an excellent flammability, and in addition a small amount of thread fraying when the fabric is cut with a knife or sewn, even with a small amount of coating,[Solution] Provided is a base fabric for an airbag comprising a coated fabric wherein resin compositions are applied to at least one side of a textile, wherein the coating amount of the resin composition applied to the one side of the textile is 0.1 to 10 g/m2 in terms of a mass after drying, an air permeability under a differential pressure of 100 kPa is 0.05 L/cm2/min or less, a flammability measured in accordance with FMVSS302 is self-extinguishing, and the number of frayed thread at the end part after 100 repetitions of a scrub test in accordance with ISO5981 is 5 or less.

    摘要翻译: [解决方案]提供一种用于气囊的底布,其包括涂布织物,其中将树脂组合物施加到织物的至少一侧,其中施加到织物一侧的树脂组合物的涂布量为0.1至10g / m2,干燥后的空气透过率为100kPa的压差为0.05L / cm 2 / min以下,根据FMVSS302测定的可燃性为自熄性,在 根据ISO5981的100次重复擦洗试验后的末端部分为5以下。

    METALLIZED TEXTILES AND PROCESS FOR MANUFACTURING SAME
    95.
    发明申请
    METALLIZED TEXTILES AND PROCESS FOR MANUFACTURING SAME 审中-公开
    金属纺织品和制造方法

    公开(公告)号:US20160273155A1

    公开(公告)日:2016-09-22

    申请号:US15034958

    申请日:2014-11-17

    申请人: MERMET

    摘要: The present invention provides a textile metallized on at least one of its faces comprising a textile layer of inorganic fibers and a metallic layer, the textile being characterized in that the connection between the textile layer and the metallic layer is provided by a polymeric intermediate layer formed by a matrix having at least one coupling polymer in which at least one flame retardant agent is distributed, said coupling polymer being bonded by chemical bonds firstly to the textile layer and secondly to the metallic layer. The present invention also provides the method of fabricating this metallized textile.

    摘要翻译: 本发明提供一种在其至少一个表面上金属化的织物,其中包含无机纤维和金属层的织物层,该织物的特征在于织物层和金属层之间的连接由形成的聚合物中间层 通过具有至少一种其中分布有至少一种阻燃剂的偶联聚合物的基质,所述偶联聚合物首先通过化学键键合到织物层,其次是结合到金属层。 本发明还提供了制造这种金属化织物的方法。

    BIOCIDE-FREE PREWETTED SPONGE CLOTH
    96.
    发明申请
    BIOCIDE-FREE PREWETTED SPONGE CLOTH 审中-公开
    无生物无纺布海绵布

    公开(公告)号:US20160174564A1

    公开(公告)日:2016-06-23

    申请号:US14967566

    申请日:2015-12-14

    申请人: Kalle GmbH

    IPC分类号: A01N59/06 A01N25/34

    摘要: A biocide-free sponge cloth prewetted with a hygroscopically acting inorganic salt is provided. The spone cloth is based on regenerated cellulose which is mechanically reinforced with fibres and/or a web and includes a hygroscopically acting salt. The sponge cloth has an aw value of less than 0.80. On account of the low aw value, the sponge cloth has an antibacterial, bacteriostatic, fungicidal and/or fungistatic effect. The hygroscopically acting salt is preferably magnesium chloride. It can be combined with further inorganic salts, with low molecular weight, mono- or polyhydric alcohols, with sugars, sugar esters, mono- or polybasic carboxylic acids, esters of mono- or polybasic carboxylic acids and/or with hydrophilic polymers. The sponge cloth is preferably produced by the viscose process.

    摘要翻译: 提供了预湿润吸湿作用的无机盐的无杀生物剂的海绵布。 螺旋布基于再生纤维素,其被纤维和/或纤维网机械增强,并且包括吸湿作用盐。 海绵布的aw值小于0.80。 由于低aw值,海绵布具有抗菌,抑菌,杀真菌和/或抑菌作用。 吸湿作用盐优选为氯化镁。 它可与另外的无机盐,低分子量的一元醇或多元醇与糖,糖酯,单羧酸或多元羧酸,单羧酸或多元羧酸的酯和/或亲水性聚合物结合。 海绵布优选通过粘胶工艺制造。

    Sizing agent for reinforcement fibers, and application thereof
    100.
    发明授权
    Sizing agent for reinforcement fibers, and application thereof 有权
    增强纤维上浆剂及其应用

    公开(公告)号:US09234312B2

    公开(公告)日:2016-01-12

    申请号:US14381357

    申请日:2013-02-27

    摘要: A sizing agent for a reinforcement fiber is used for reinforcing thermoplastic matrix resins and spreads on the reinforcement fiber surface and imparts both excellent splittability and bonding performance to thermoplastic matrix resins. The sizing agent includes essentially an ester compound (A) having a vinyl ester group, acrylate group or methacrylate group bonded to at least one of the chain ends of the main chain of the ester compound (A), and of a polyoxyalkylene alkyl ether (B) which is an adduct between an alkylene oxide and a C4-14 monohydric alcohol. When water is added to the sizing agent thereby producing a mixture with a nonvolatile content of 1 weight %, the mixture exhibits a dynamic surface tension ranging from 40 to 55 mN/m determined by the maximum bubble pressure method when bubbles are blown into the mixture at the rate of one bubble per 100 milliseconds.

    摘要翻译: 用于增强纤维的上浆剂用于增强热塑性基质树脂并在增强纤维表面上扩散,并赋予热塑性基质树脂优异的分裂性和粘结性能。 上浆剂基本上包括与酯化合物(A)的主链的至少一个链端连接的聚乙烯基酯基,丙烯酸酯基或甲基丙烯酸酯基和聚氧化烯烷基醚(A)的酯化合物(A) B),其是环氧烷和C4-14一元醇之间的加合物。 当向施胶剂中加入水,从而制成不挥发成分为1重量%的混合物时,当将气泡吹入混合物时,通过最大气泡压力法确定的混合物表现出40至55mN / m的动态表面张力 以每100毫秒一个气泡的速率。