Method and apparatus for paint curing
    171.
    发明授权
    Method and apparatus for paint curing 有权
    油漆固化方法和设备

    公开(公告)号:US08524330B2

    公开(公告)日:2013-09-03

    申请号:US12705685

    申请日:2010-02-15

    CPC classification number: B05D3/067 B05B16/00 B05D3/0209 B05D3/0263 B05D3/0406

    Abstract: A method for curing a paint coating applied to a workpiece includes applying radiant light energy to cure the paint coating on surfaces of the workpiece within a line of sight of a radiant light energy source, and applying ambient air to the workpiece to cure the paint coating on surfaces of the workpiece not within the line of sight of the radiant light energy source.

    Abstract translation: 用于固化施加到工件上的涂料涂层的方法包括施加辐射光能量以在辐射光能源的视线范围内固化工件表面上的涂料涂层,并且将环境空气施加到工件以固化涂料涂层 在工件的表面上不在辐射光能量源的视线范围内。

    Methods and systems for coating and sealing inside of piping systems
    173.
    发明授权
    Methods and systems for coating and sealing inside of piping systems 有权
    管道系统内部涂层和密封的方法和系统

    公开(公告)号:US08343579B2

    公开(公告)日:2013-01-01

    申请号:US12813873

    申请日:2010-06-11

    Abstract: Methods, processes and systems for cleaning, coating and sealing leaks in existing pipes, in a single operation. A process can include isolating, draining, drying, cleaning and sealing a piping system. Air can be forced and pulled throughout the piping system by a generator and a vacuum. Pipes can be protected from water corrosion, erosion and electrolysis, extending the life of pipes such as copper, steel, lead, brass, cast iron piping and composite materials. Coatings can be applied to pipes having diameters up to approximately 6″. Leak sealants of at least approximately 4 mils thick can cover insides of pipes, and can include novel mixtures of fillers and epoxy materials, and viscosity levels. A positive pressure can be maintained within the pipes during applications. Piping systems can be returned to service within approximately 96 hours.

    Abstract translation: 在单一操作中清洁,涂覆和密封现有管道泄漏的方法,过程和系统。 一个过程可以包括隔离,排水,干燥,清洁和密封管道系统。 可以通过发电机和真空将空气强制并拉过管道系统。 管道可以防止水腐蚀,腐蚀和电解,延长铜,钢,铅,黄铜,铸铁管和复合材料等管道的使用寿命。 涂层可以应用于直径大约6“的管道。 至少约4密耳厚的泄漏密封剂可以覆盖管道的内部,并且可以包括填充剂和环氧材料的新型混合物和粘度水平。 在施工过程中,管内可保持正压。 管道系统可在大约96小时内恢复使用。

    Information-recording medium and method for producing the same

    公开(公告)号:US20040126534A1

    公开(公告)日:2004-07-01

    申请号:US10734165

    申请日:2003-12-15

    Inventor: Yoshihisa Usami

    CPC classification number: G11B7/24 B05C11/08 B05D1/005 B05D3/0406 G11B7/26

    Abstract: Disclosed is a method for producing an information-recording medium comprising, on a substrate, a dye recording layer capable of recording information, the method comprising the step of drying the substrate formed with the dye recording layer by allowing clean air to flow while rotating the substrate at a high speed; wherein an intake for introducing the clean air is narrowed by arranging a lid having a circular opening at a central portion, at an opening disposed at an upper portion of an apparatus for rotating the substrate at the high speed.

    Chemical liquid processing apparatus for processing a substrate and the method thereof
    177.
    发明授权
    Chemical liquid processing apparatus for processing a substrate and the method thereof 失效
    用于处理基板的化学液处理装置及其方法

    公开(公告)号:US06579382B2

    公开(公告)日:2003-06-17

    申请号:US09784200

    申请日:2001-02-16

    Applicant: Shinichi Ito

    Inventor: Shinichi Ito

    Abstract: In this disclosure, air flow is formed above chemical liquid film and a move of the chemical liquid is generated by making the air flow into a contact with the surface of chemical liquid. Further, a negative pressure is generated in a space between a processing object substrate and a plate by rotating the plate. Consequently, uniformity of processing of chemical liquid is improved, so that liquid removing step can be carried out effectively. As a result, yield rate of chemical liquid treatment can be improved.

    Abstract translation: 在本公开中,在化学液膜上方形成空气流,并且通过使空气流与化学液体的表面接触而产生化学液体的移动。 此外,通过旋转板在处理对象基板和板之间的空间中产生负压。 因此,提高了液体的处理均匀性,能够有效地进行液体除去工序。 结果,可以提高化学液体处理的产率。

    Chemical liquid processing apparatus for processing a substrate and the method thereof
    178.
    发明申请
    Chemical liquid processing apparatus for processing a substrate and the method thereof 失效
    用于处理基板的化学液处理装置及其方法

    公开(公告)号:US20010028920A1

    公开(公告)日:2001-10-11

    申请号:US09784200

    申请日:2001-02-16

    Abstract: In this disclosure, air flow is formed above chemical liquid film and a move of the chemical liquid is generated by making the air flow into a contact with the surface of chemical liquid. Further, a negative pressure is generated in a space between a processing object substrate and a plate by rotating the plate. Consequently, uniformity of processing of chemical liquid is improved, so that liquid removing step can be carried out effectively. As a result, yield rate of chemical liquid treatment can be improved.

    Abstract translation: 在本公开中,在化学液膜上方形成空气流,并且通过使空气流与化学液体的表面接触而产生化学液体的移动。 此外,通过旋转板在处理对象基板和板之间的空间中产生负压。 因此,提高了液体的处理均匀性,能够有效地进行液体除去工序。 结果,可以提高化学液体处理的产率。

    Method for applying a composite coating having a polychromatic effect onto a substrate
    179.
    发明授权
    Method for applying a composite coating having a polychromatic effect onto a substrate 有权
    将具有多色效应的复合涂层施加到基材上的方法

    公开(公告)号:US06291018B1

    公开(公告)日:2001-09-18

    申请号:US09440610

    申请日:1999-11-15

    Abstract: A method of forming a composite coating having a polychromatic effect over a substrate is provided in which a first liquid basecoat material is exposed to air having a temperature of about 50° F. to about 90° F. (10-32.5° C.), a relative humidity of about 40% to about 80% and an air vilocity of about 20 FPM to about 150 FPM (0.10-0.76 m/s) at the surface of the first basecoat material for a peroid of about 10 to about 180 seconds. A second liquid basecoat material comprising effect pigment is then applied over the set first basecoat material by a bell applicator to produce the composite coating.

    Abstract translation: 提供了一种在衬底上形成具有多色效应的复合涂层的方法,其中将第一液体底涂层材料暴露于温度为约50°F至约90°F(10-32.5℃)的空气中。 ,相对湿度为约40%至约80%,空气速度为约20FPM至约150FPM(0.10-0.76m / s),在第一底涂层材料的表面为约10至约180秒 。 然后通过钟形施加器将包含效果颜料的第二液体底漆材料施加在所述第一底漆材料上以产生复合涂层。