Liquid inks comprising stabilizing plastisols
    15.
    发明授权
    Liquid inks comprising stabilizing plastisols 失效
    包含稳定增塑溶胶的液体油墨

    公开(公告)号:US06806013B2

    公开(公告)日:2004-10-19

    申请号:US10177640

    申请日:2002-06-20

    CPC classification number: C09D11/36 C09D11/03 C09D11/033 C09D11/101

    Abstract: This invention relates to a liquid ink for developing electrophotographic images comprising: a) a carrier liquid having a Kauri-Butanol number less than 30; b) a plastisol; c) a dispersant; and d) a charge director wherein: a. for a positive charge director, the dispersant has amine groups and the plastisol comprises polymeric particles having acid groups and an acid value between 30 and 150 mg KOH/g such that the mole ratio of the amine groups to the acid groups is between 0.075 and 0.3; and b. for a negative charge director, the plastisol comprises a polymer having an amine value between 5 and 200 mg KOH/g and the dispersant has acid groups such that the mole ratio of the acid groups to the amine groups is between 0.075 and 0.3.

    Abstract translation: 本发明涉及一种用于显影电子照相图像的液体油墨,包括:a)具有小于30的贝壳杉脂丁醇值的载液; b)增塑溶胶; c)分散剂; andd)a charge director wherein:a。 对于正电荷导向剂,分散剂具有胺基,增塑溶胶包含具有酸基和酸值在30至150mg KOH / g之间的聚合物颗粒,使得胺基与酸基的摩尔比在0.075和0.3之间 ; 安布 对于负电荷导向剂,增塑溶胶包含具有5至200mg KOH / g的胺值的聚合物,并且分散剂具有酸基,使得酸基与胺基的摩尔比为0.075至0.3。

    Epoxy coating compositions with metal-containing stabilizers
    17.
    发明授权
    Epoxy coating compositions with metal-containing stabilizers 失效
    具有含金属稳定剂的环氧涂料组合物

    公开(公告)号:US5314980A

    公开(公告)日:1994-05-24

    申请号:US5597

    申请日:1993-01-19

    Inventor: Eric D. Morrison

    Abstract: A coating composition comprises an epoxy silane, an amine hardener that can react with the epoxy silane to form a cross-linked coating, and a stabilizer that includes a sufficient amount of a metal component to delay cross-linking between the epoxy silane and the amine hardener. The coating composition has a shelf life of at least 3 days.

    Abstract translation: 涂料组合物包含环氧硅烷,可与环氧硅烷反应以形成交联涂层的胺固化剂,以及包含足够量的金属组分以延迟环氧硅烷和胺之间的交联的稳定剂 硬化剂 涂料组合物的保质期至少为3天。