A POLYOLEFIN COMPOSITION
    27.
    发明申请
    A POLYOLEFIN COMPOSITION 审中-公开
    聚烯烃组合物

    公开(公告)号:US20150344681A1

    公开(公告)日:2015-12-03

    申请号:US14653329

    申请日:2013-12-27

    Abstract: The instant invention provides a polyolefin composition suitable for injection molding applications, and method of making such injection molded articles. The polyolefin composition suitable for injection molding applications comprises: an ethylene/α-olefin interpolymer composition comprising: (a) from 25 to 50 percent by weight of a first ethylene/α-olefin copolymer fraction having a density in the range of from 0.924 to 0.937 g/cm3, a melt index (I2) in the range of from 0.03 to 0.3 g/10 min, (b) from 50 to 75 percent by weight of a second ethylene homopolymer fraction having a density in the range of from greater than 0.960 g/cm3, a melt index (I2) in the range of from 100 to 180 g/10 minutes, wherein said ethylene/α-olefin interpolymer composition has a density in the range of from 0.950 to 0.958 g/cm3, a melt index (I2) in the range of from 1.0 g/10 min to 3.5 g/10 min, a zero shear viscosity ratio (ZSVR) in the range of from 1.01 to 2.5, a molecular weight distribution (Mw/Mn) in the range of from 2.0 to 4.0, and tan delta at 0.1 radian/second and 190° C. in the range of from 9 to 50.

    Abstract translation: 本发明提供了适用于注塑应用的聚烯烃组合物,以及制备这种注模制品的方法。 适用于注塑应用的聚烯烃组合物包括:乙烯/α-烯烃互聚物组合物,其包含:(a)25至50重量%的第一乙烯/α-烯烃共聚物部分,其密度范围为0.924至 0.937g / cm 3,熔体指数(I 2)在0.03至0.3g / 10min的范围内,(b)50至75重量%的第二乙烯均聚物部分,其密度在大于 0.960g / cm 3,熔体指数(I 2)在100至180g / 10分钟的范围内,其中所述乙烯/α-烯烃互聚物组合物的密度范围为0.950至0.958g / cm 3,熔体 指数(I 2)在1.0g / 10min至3.5g / 10min的范围内,零剪切粘度比(ZSVR)在1.01至2.5范围内,分子量分布(Mw / Mn)在该范围内 为2.0〜4.0,tanδ为0.1弧度/秒,190℃为9〜50。

Patent Agency Ranking