METHOD FOR MAINTAINING THE OPTIMAL AMOUNT OF INERT GAS BEING INJECTED INTO CAST STEEL

    公开(公告)号:US20230201919A1

    公开(公告)日:2023-06-29

    申请号:US17919824

    申请日:2020-04-20

    Applicant: ArcelorMittal

    CPC classification number: B22D41/58 B22D11/117 B22D41/42

    Abstract: A method for maintaining the optimal argon injection flow rate which will result in production of steel slab of a chosen alloy having optimal cleanliness. The steel is cast using an argon injected slide gate. The selected steel has a known optimal argon injection flow rate Qb* for casting steel of optimal cleanliness. The method involves calculating the present steel pressure and determining the present injection flow rate conductance Gb′ of the argon injected slide gate during either of 1) a steel pressure change event; or 2) an argon flow change event. The measurements are used to calculate present argon pressure required to insure the required injection flow rate of argon into the steel for optimal cleanliness of the cast steel.

    Lamination device and process thereof

    公开(公告)号:US11623436B2

    公开(公告)日:2023-04-11

    申请号:US17299477

    申请日:2019-12-10

    Applicant: ArcelorMittal

    Abstract: A lamination device for laminating a photovoltaic stack on a profiled metallic panel, the lamination device including a lid covered on its underside with an upper flexible pressure membrane so as to form an airtight upper chamber that may be ventilated or evacuated and/or including an upper heating device whose bottom side has a crenellated profile, the device also including a chassis covered on its top with a lower flexible pressure membrane so as to form an airtight lower chamber that may be ventilated or evacuated and/or including a lower heating device whose upper side has a cross-section which differs from the crenellated profile of the bottom side of the upper heating device, wherein the lid is capable of sealably laying on the chassis so that the cavity thus formed is airtight and may be ventilated or evacuated. A corresponding process is also provided.

    Method for producing a high strength steel sheet having improved strength, ductility and formability

    公开(公告)号:US11618931B2

    公开(公告)日:2023-04-04

    申请号:US15322947

    申请日:2015-07-03

    Applicant: ArcelorMittal

    Abstract: A method for producing a high strength steel sheet having a yield strength YS of at least 850 MPa, a tensile strength TS of at least 1180 MPa, a total elongation of at least 14% and a hole expansion ratio HER of at least 30%. The chemical composition of the steel contains: 0.15%≤C≤0.25%, 1.2%≤Si≤1.8%, 2%≤Mn≤2.4%, 0.1%≤Cr≤0.25%, Nb≤0.05%, Ti≤0.05%, Al≤0.50%, the remainder being Fe and unavoidable impurities. The sheet is annealed at an annealing temperature TA higher than Ac3 but less than 1000° C. for more than 30 s, by cooling it to a quenching temperature QT between 275° C. and 325° C., at a cooling speed sufficient to have, just after quenching, a structure consisting of austenite and at least 50% of martensite, the austenite content en.) being such that the final structure can contain between 3% and 15% of residual austenite and between 85 and 97% of the sum of martensite and bainite, without ferrite, heated to a partitioning temperature PT between 420° C. and 470° C. and maintained at this temperature for time between 50 s and 150 s and cooled to the room temperature.