摘要:
The present invention provides: proteins suppressing or promoting the aggregation or deposition of amyloid-β protein; polynucleotides encoding the proteins; a method for screening a compound suppressing or promoting the aggregation or deposition of amyloid-β protein; and therapeutic agents for treating or preventing Alzheimer's diseases comprising a compound that regulates the activity of a protein suppressing or promoting the aggregation or deposition of amyloid-β protein.
摘要:
A martensitic stainless steel sheet which is hard to be softened by tempering caused by heating during the use of a disk brake, can maintain the predetermined hardness, and has excellent punching workability, bending workability before quenching, and a particularly small shear drop, and in which a predetermined hardness after quenching is constantly achieved, in a low carbon martensitic stainless steel sheet used only after quenching. Specifically, the sheet contains, on the basis of mass percent, 0.030% to 0.100% C; 0.50% or less of Si; 1.00% to 2.50% Mn; more than 10.00% to 15.00% Cr; at least one selected from the group consisting of 0.01% to 0.50% Ti, 0.01% to 0.50% V, 0.01% to 1.00% Nb, and 0.01% to 1.00% Zr; N in an amount defined by the following expression, N: 0.005% to (Ti+V)×14/50+(Nb+Zr)×14/90; and the balance being Fe and incidental impurities.
摘要:
Ferritic stainless steel comprising all three of Co, V, and B, having a Co content of about 0.01 mass % to about 0.3 mass %, a V content of about 0.01 mass % to about 0.3 mass %, and a B content of about 0.0002 mass % to about 0.0050 mass %, and having superior secondary working embrittleness resistance and superior high temperature fatigue characteristics.
摘要:
The present invention provides a BA-finished stainless steel product having superior antibacterial properties and corrosion resistance and a method for producing the same. Specifically, after a stainless steel product is subjected to BA treatment, the stainless steel product is immersed in a solution containing Ag ions having a concentration of 0.0001 to 1.0 mol/l so that a BA film contains, in area percentage, 0.0002 to 0.05% of Ag particles and Ag compounds, and further, stainless steel product contains 0.001 to 0.10% by weight of Ag and optionally further contains 0.001 to 0.30% by weight of V.
摘要:
An optical disk is made up of a disk-shaped substrate having a surface, a first track and a second track provided on the surface of the substrate, where the first and second tracks are two mutually adjacent concentric tracks or two mutually adjacent track turns of a single spiral track, the first track extends along a first center line and the second track extends along a second center line, and an identification signal recording part extending along a third center line and prerecorded with an identification signal including at least a sector number and a track number for identifying a position on the optical disk. The third center line is arranged between the first and second center lines, and the identification signal prerecorded in the identification signal recording part is common to the first and second tracks on both sides of the identification signal recording part.
摘要:
A steel sheet for porcelain enameling having improved press formability and enameling properties comprises particular amounts of C, Mn, B, Cu, Al, O, N, and P or further Ti and Nb and the balance being Fe and inevitable impurities and is produced by hot rolling a slab of steel having a chemical composition as mentioned above as a starting material, cold rolling the resulting hot rolled sheet at a reduction of not less than 70%, and then subjecting the resulting cold rolled sheet to a continuous annealing at a heating temperature of not lower than 800.degree. C. but not higher than A.sub.c3 transformation point.
摘要:
A method of manufacturing a steel sheet having excellent deep-drawability. A steel blank is rolled into a steel sheet having a predetermined thickness. The steel contains C: not more than 0.008 wt %, Si: not more than 0.5 wt %, Mn: not more than 1.0 wt %, P: not more than 0.15 wt %, S: not more than 0.02 wt %, Al: 0.010 to 0.10 wt %, N: not more than 0.008 wt %, and at least one element selected from the group consisting of Ti and Nb which is contained in an amount satisfying the relationship of 1.2 (C/12+N/14).ltoreq.(Ti/48+Nb/93). In at least one pass, rolling is conducted within a temperatures range lower than the Ar3 transformation point but not lower than 500.degree. C., in such a manner that the roll radius R (mm) and the blank thickness t (mm) before rolling by rolls satisfy the relationships of R.ltoreq.200 and R.sup.2 .times..sqroot.t.ltoreq.100000, and the total rolling reduction at temperature lower than the Ar3 transformation point is not lower than 60%. The hot-rolled steel sheet possesses a high level of Lankford value, and is free from cold-working embrittlement. The method may include the step of obtaining, after the rolling, pickling, annealing and hot dip galvanizing under certain conditions, a surface-treated steel sheet having excellent deep-drawability.
摘要:
A method of manufacturing formable as-rolled thin steel sheets having excellent ridging resistance and other properties is disclosed, which comprises rolling a low carbon steel to a given thickness without cold rolling and recrystallization annealing steps. In this rolling, at least one rolling pass is carried out within a given temperature range at high draft and high strain rate.
摘要:
A composition for percutaneous administration containing a nicotinic ester represented by formula (I) ##STR1## or an isonicotinic ester represented by formula (II) ##STR2## wherein R and R' each represents an alkyl group having 5 or more carbon atoms,with or without a specific polar compound. The composition improves percutaneous absorption of an active ingredient.
摘要:
Thin steel sheets having an improved processability are produced when a steel sheet or cast strip obtained through a continuous casting or strip caster process is subjected to a lubrication rolling step at a temperature of from Ar.sub.3 transformation point to 300.degree. C. and a rolling speed of not less than 1,500 m/min. By this method, the cold rolling step or cold rolling-annealing step can be omitted.