A glass antenna with improved reception sensitivity was provided. A glass antenna formed on a surface of a window of a motor vehicle includes: an FM antenna element; and a heater that is capacitively coupled to the FM antenna element, and includes a plurality of heating wires, wherein a distance S between the FM antenna element and the heater is more than 40 mm.
摘要:
The reduced pressure double glazed glass panel of the present invention includes an outside glass sheet, an inside glass sheet, and a gap portion that are joined together, with the gap portion being formed between the glass sheets and sealed under reduced pressure. Here, the outside glass sheet has a first glass surface disposed to face the outdoor space and a second glass surface disposed to face the gap portion. A Low-E film is formed on the second glass surface. The following relations hold: (Emissivity of Low-E film ∈)≦0.067; 31%≦(Solar reflectance on First glass surface RG(solar))≦40%; (48−RG(solar))%≦(Solar absorptance on First glass surface AG(solar))≦17%; (AG(solar))≦{18.3−(0.07×RG(solar))+(20×∈)}%; (Solar heat gain coefficient SHGC)≦0.50; and (Thermal transmittance U value)≦1.2 W/m2·K or less. According to the present invention, it is possible to provide a reduced pressure double glazed glass panel having sufficient heat insulating and heat shielding properties and being less susceptible to bending when exposed to solar radiation.
摘要:
The present invention provides a glass composition containing, in mass %: 59.0 to 63.0% SiO2; 4.0 to 10.0% TiO2; 8.0 to 12.0% Al2O3; 1.0 to 5.0% MgO; 0 to 4.0% CaO; 4.0 to 14.0% SrO; 4.0 to 11.0% Na2O; and 0 to 1.0% K2O. According to the present invention, it is possible to provide a glass composition having excellent heat resistance, being suitable for production by the float process, and being suitable for chemical strengthening.
摘要:
A cover glass of the present invention for photoelectric conversion devices includes a glass sheet having surface asperities and a reflection-reducing film formed over the surface asperities of the glass sheet. The surface asperities of the glass sheet have an average spacing Sm of 0.3 mm or more and 2.5 mm or less and an arithmetic average roughness Ra of 0.3 μm to 5 μm. The reflection-reducing film includes fine silica particles having an average particle diameter of 50 to 200 nm and a binder for the fine silica particles, and the fine silica particles are uniformly arranged in a single layer on peak portions of the surface asperities in such a manner that a filling fraction F is 35 to 65%. A transmittance gain is 2.37% or more, the transmittance gain being obtained by subtracting an average transmittance of the glass sheet as measured when light having wavelengths ranging from 380 to 1100 nm are incident on a face of the glass sheet that has the surface asperities, from an average transmittance of the cover glass as measured when light having the wavelengths are incident on a reflection-reducing film side of the cover glass. Thus, a cover glass for photoelectric conversion devices that exhibits a high transmittance gain is provided.
摘要:
The method of the present invention for producing a granular material containing a metal oxide includes the steps of feeding a metal oxide sol that contains colloidal particles of a metal oxide as a dispersoid and water as a dispersion medium and that has a pH of 7 or higher, into an aqueous electrolyte solution, so as to aggregate the colloidal particles of the metal oxide, form aggregates containing the metal oxide in the aqueous electrolyte solution, and make the aggregates settle out in the aqueous electrolyte solution; and separating the aggregates from the aqueous electrolyte solution after formation of the aggregates. Thus, a highly productive method for producing a granular material containing a metal oxide can be provided.
摘要:
A bright pigment of the present invention includes a scaly inorganic base 10, a silver-containing coating 11 that covers the inorganic base 10 and contains silver or a silver alloy, and a yellowing-suppressing coating 2 that covers the inorganic base 10 from outside of the silver-containing coating 11 and contains a metal compound functioning as an oxidizing agent. The metal compound is preferably at least one selected from the group consisting of a hydroxide of metal, an oxide hydrate of metal, and a salt of an oxide hydrate of metal, and the metal is at least one selected from the group consisting of tungsten, molybdenum, bismuth, vanadium, or cerium.
摘要:
A window glass with a conductive ceramic fired body includes at least one glass plate having main surfaces, and the conductive ceramic fired body including a feeding point and a linear portion which is disposed on either one of the main surfaces of the glass plate, at least a part of the linear portion being placed in a visible region of the window glass and formed by successively laminating a first colored layer, a conductor layer and a second colored layer on the main surface, wherein the first colored layer and the second colored layer each include a pigment and a glass component, and the conductor layer includes silver and the glass component.
摘要:
The reinforcing cord of the present invention includes at least one strand. The strand includes a bundle of filaments that are bundled and twisted together in one direction, and a coating layer that is formed on at least the surface of the bundle. The bundle consists essentially of carbon fiber filaments. The coating layer is a coating layer that is formed from an aqueous treatment agent containing a rubber latex and a crosslinking agent as essential components and a filler as an optional component. In the aqueous treatment agent, the total of the mass of the crosslinking agent and the mass of the filler is in a range of 1 to 50% of the mass of rubber in the rubber latex.
摘要:
Provided is a glass composition suitable for production using large-scale sheet glass mass production facilities by the float process or the like, having high heat resistance, and suitable for chemical strengthening. Specifically, provided is a glass composition containing, in mass %: 60 to 66% SiO2; 10 to 16% Al2O3; 0 to 1% B2O3; 3 to 10% MgO; 0 to 1% CaO; 1 to 9% SrO; O to 4% BaO; 0 to 2% ZnO; 0 to 1% Li2O; 10 to 20% Na2O; 0 to 5% K2O; O to 2% TiO2; 0 to 0.1% ZrO2; and 0 to 2% total iron oxide in terms of Fe2O3. In this glass composition, a total content of MgO, CaO, SrO, and BaO is in a range of 10 to 20%, a total content of Li2O, Na2O, and K2O is in a range of 14 to 20%, and a content of SrO is higher than a content of CaO.
摘要:
It is an object of the present invention to provide a method of detoxifying a methyl compound comprising arsenic etc., effectively and systematically. The method of detoxifying a methyl compound according to the present invention is characterized in that an organic halogenated compound is reacted with a methyl compound comprising at least one element selected from the groups comprising arsenic, antimony and selenium to convert the methyl compound into more harmless substances. Furthermore, in a preferred embodiment of the method of detoxifying a methyl compound according to the present invention, the method is characterized in that the element is arsenic.