摘要:
A two-component coating composition is disclosed wherein the binder components comprise: (a) an amino component comprising an aqueous solution and/or dispersion of at least one polyacrylate containing amino groups in a quantity sufficient to make said polyacrylate soluble and/or dispersible in water upon neutralization with acid; and (b) a polyisocyanate component containing free isocyanate groups. Also disclosed is the method of emulsifying component (b) into component (a).
摘要:
The present invention relates to a coating composition having an improved pot life without a corresponding increase in dry time when cured under ambient conditions which containsa) a polyisocyanate component,b) an aldimine based on the reaction product of a polyamine having 2 or more primary amino groups with an aldehyde corresponding to the formula:O=CHCH(R.sub.1)(R.sub.2) wherein R.sub.1 and R.sub.2 may be the same or different and represent optionally substituted hydrocarbon radicals, or R.sub.1 and R.sub.2 together with the .beta.-carbon atom form a cycloaliphatic or heterocyclic ring andc) 0.001 to 5 weight percent, based on the weight of components a) and b), of a tin(IV) compound which is a catalyst for the reaction between isocyanate groups and hydroxyl groups,wherein components a) and b) are present in an amount sufficient to provide an equivalent ratio of isocyanate groups to aldimine groups of 0.5:1 to 20:1.
摘要:
The present invention relates to a coating composition for the preparation of a polyurea coating which containsa) a polyisocyanate component containing one or more aliphatic polyisocyanates,b) at least one polaspartic acid esterc) 0.05 to 5% by weight, based on the total weight of the coating composition, of an organic acid,wherein components a) and b) are present in amounts sufficient to provide an equivalent ratio of isocyanate groups of component a) to isocyanate-reactive groups of component b) of 0.5:1 to 20:1.
摘要:
The present disclosure describes a method of manufacturing a one-component coating composition. The method can include combining a water-containing additive with a non-reactive resin to form a grinding dispersion. The method can also include grinding the grinding dispersion to a Hegman value of at least 4 to form a ground dispersion. A drying agent can then be added to form a dried slurry. A silane-modified polyurea can be added to the dried slurry to form a one-component coating composition.
摘要:
Methods of printing a three-dimensional object using co-reactive components are disclosed. Thermosetting compositions for three-dimensional printing are also disclosed.
摘要:
A conductive composition for conductive coatings, gap fillers, caulks and fairing compounds that are useful for EMI shielding, electrical grounding, lightning strike protection, and reduced radar cross-section for low observability (LO), with improved resistance to exposure to water, oil and other fluids contains at least one aspartic ester, at least one isocyanate and a conductive filler.
摘要:
Durable polyurea copolymer coatings can be applied to surfaces that come in contact with fluids, such as biological fluids, thereby passivating the surface. Polyurea copolymer coating compositions comprise a reaction product of (a) a diamine composition that includes a polyethylene glycol diamine, and optionally, a dipiperidyl alkane; and (b) a diisocyanate. Solutions containing polyurea copolymers, coated surfaces and methods are also described.
摘要:
Provided is a protective material that protects a wireless communication portion for wireless communication, comprising a substrate formed of a foam synthetic resin and a coating layer of a polyurea resin covering at least a front side surface of the substrate. The wireless communication device includes a wireless communication portion for wireless communication and a protective material.
摘要:
A polyisocyanate resin can include from 25 wt % to 50 wt % of a first cycloaliphatic polyisocyanate and from 50 wt % to 75 wt % of a flexibilizing component based on a total weight of the polyisocyanate resin. The flexibilizing component can include a linear aliphatic polyisocyanate having a number average isocyanate functionality of from 2 to 3 based on gel permeation chromatography and an isocyanate-terminated reaction product of a second cycloaliphatic polyisocyanate and an isocyanate-reactive material, the reaction product having a Tg of less than −30° C. based on a Differential Scanning calorimetry (2nd Heating) temperature scan from −100° C. to 150° C. using 20° C./min heating and cooling ramps. The isocyanate-terminated reaction product and the linear aliphatic polyisocyanate can be present at a weight ratio of from 0.5 to 2.5.