Tire with innerliner containing talc and epichlorohydrin rubber
    2.
    发明授权
    Tire with innerliner containing talc and epichlorohydrin rubber 失效
    含有滑石粉和表氯醇橡胶的内衬轮胎

    公开(公告)号:US08397776B2

    公开(公告)日:2013-03-19

    申请号:US12331735

    申请日:2008-12-10

    Abstract: The present invention is directed to a pneumatic tire comprising a carcass and an innerliner in direct contact with the carcass, the innerliner comprising a rubber composition comprising: at least one elastomer selected from the group consisting of butyl rubber, chlorinated butyl rubber, brominated butyl rubber, synthetic polyisoprene, natural rubber, styrene butadiene rubber, polybutadiene, copolymer of isobutylene and paramethylstyrene, and brominated copolymer of isobutylene and paramethylstyrene; epichlorohydrin rubber; and at least one delaminated talc having a BET surface area according to DIN 66131 of 10-40 m2/g, an average particle size (D50) of 4-8 microns, determined by laser diffraction measurement, and a lamellarity index of 3-15.

    Abstract translation: 本发明涉及一种充气轮胎,其包括与胎体直接接触的胎体和内衬层,所述衬里包括橡胶组合物,所述橡胶组合物包含:至少一种选自丁基橡胶,氯化丁基橡胶,溴化丁基橡胶 ,合成聚异戊二烯,天然橡胶,丁苯橡胶,聚丁二烯,异丁烯和对甲基苯乙烯的共聚物,异丁烯和对甲基苯乙烯的溴化共聚物; 表氯醇橡胶; 并且根据DIN 66131具有10-40m 2 / g的BET表面积的至少一种脱层滑石,通过激光衍射测量确定的平均粒径(D50)为4-8微米,层厚指数为3-15 。

    METHOD OF PROCESSING RUBBER COMPOSITION, RUBBER COMPOSITION AND PNEUMATIC TIRE
    5.
    发明申请
    METHOD OF PROCESSING RUBBER COMPOSITION, RUBBER COMPOSITION AND PNEUMATIC TIRE 失效
    加工橡胶组合物,橡胶组合物和气动轮胎的方法

    公开(公告)号:US20110034619A1

    公开(公告)日:2011-02-10

    申请号:US12535762

    申请日:2009-08-05

    Abstract: The present invention is directed to a method of processing a rubber composition, comprising the steps of mixing at least one diene base elastomer with at least one additive selected from the group consisting of fillers, to a final temperature of about 150 to about 160° C. in a first non-productive mix step to form a first non-productive mix; cooling the first non-productive mix to a temperature of about 60 to about 90° C.; mixing the first non-productive mix with 0.1 to 10 parts by weight, per 100 parts by weight of elastomer, of a treated short aramid fiber having a length ranging from 1 to 10 mm and having a thickness ranging from 5 to 15 microns and comprising 3 to 40 percent by weight of a peroxide radical initiator in a second non-productive mix step to a final temperature of about 150 to about 160° C. to form a second non-productive mix; and mixing the second non-productive mix with curatives in a productive mix step to form a productive mix.

    Abstract translation: 本发明涉及一种处理橡胶组合物的方法,包括以下步骤:将至少一种二烯基基弹性体与至少一种选自填料的添加剂混合至最终温度约150至约160℃ 在第一个非生产性混合步骤中形成第一个非生产性混合物; 将第一非生产性混合物冷却至约60至约90℃的温度; 将第一非生产性混合物按每100重量份弹性体0.1至10重量份混合,长度范围为1至10毫米且厚度范围为5至15微米的处理过的短芳族聚酰胺纤维,其包含 3至40重量%的过氧化物自由基引发剂,在第二非生产性混合步骤中至约150至约160℃的最终温度以形成第二非生产性混合物; 并在生产混合步骤中将第二非生产性混合物与固化剂混合以形成生产性混合物。

    Method of processing rubber composition, rubber composition and pneumatic tire
    7.
    发明授权
    Method of processing rubber composition, rubber composition and pneumatic tire 失效
    加工橡胶组合物,橡胶组合物和充气轮胎的方法

    公开(公告)号:US08168709B2

    公开(公告)日:2012-05-01

    申请号:US12535762

    申请日:2009-08-05

    Abstract: The present invention is directed to a method of processing a rubber composition, comprising the steps of mixing at least one diene base elastomer with at least one additive selected from the group consisting of fillers, to a final temperature of about 150 to about 160° C. in a first non-productive mix step to form a first non-productive mix; cooling the first non-productive mix to a temperature of about 60 to about 90° C.; mixing the first non-productive mix with 0.1 to 10 parts by weight, per 100 parts by weight of elastomer, of a treated short aramid fiber having a length ranging from 1 to 10 mm and having a thickness ranging from 5 to 15 microns and comprising 3 to 40 percent by weight of a peroxide radical initiator in a second non-productive mix step to a final temperature of about 150 to about 160° C. to form a second non-productive mix; and mixing the second non-productive mix with curatives in a productive mix step to form a productive mix.

    Abstract translation: 本发明涉及一种处理橡胶组合物的方法,包括以下步骤:将至少一种二烯基基弹性体与至少一种选自填料的添加剂混合至最终温度约150至约160℃ 在第一个非生产性混合步骤中形成第一个非生产性混合物; 将第一非生产性混合物冷却至约60至约90℃的温度; 将第一非生产性混合物按每100重量份弹性体0.1至10重量份混合,长度范围为1至10毫米且厚度范围为5至15微米的处理过的短芳族聚酰胺纤维,其包含 3至40重量%的过氧化物自由基引发剂,在第二非生产性混合步骤中至约150至约160℃的最终温度以形成第二非生产性混合物; 并在生产混合步骤中将第二非生产性混合物与固化剂混合以形成生产性混合物。

    TIRE WITH INNERLINER CONTAINING TALC AND EPICHLOROHYDRIN RUBBER
    8.
    发明申请
    TIRE WITH INNERLINER CONTAINING TALC AND EPICHLOROHYDRIN RUBBER 失效
    带有内胆的TALC和硫酸橡胶的轮胎

    公开(公告)号:US20100139829A1

    公开(公告)日:2010-06-10

    申请号:US12331735

    申请日:2008-12-10

    Abstract: The present invention is directed to a pneumatic tire comprising a carcass and an innerliner in direct contact with the carcass, the innerliner comprising a rubber composition comprising: at least one elastomer selected from the group consisting of butyl rubber, chlorinated butyl rubber, brominated butyl rubber, synthetic polyisoprene, natural rubber, styrene butadiene rubber, polybutadiene, copolymer of isobutylene and paramethylstyrene, and brominated copolymer of isobutylene and paramethylstyrene; epichlorohydrin rubber; and at least one delaminated talc having a BET surface area according to DIN 66131 of 10-40 m2/g, an average particle size (D50) of 4-8 microns, determined by laser diffraction measurement, and a lamellarity index of 3-15.

    Abstract translation: 本发明涉及一种充气轮胎,其包括与胎体直接接触的胎体和内衬层,所述衬里包括橡胶组合物,所述橡胶组合物包含:至少一种选自丁基橡胶,氯化丁基橡胶,溴化丁基橡胶 ,合成聚异戊二烯,天然橡胶,丁苯橡胶,聚丁二烯,异丁烯和对甲基苯乙烯的共聚物,异丁烯和对甲基苯乙烯的溴化共聚物; 表氯醇橡胶; 并且根据DIN 66131具有10-40m 2 / g的BET表面积的至少一种脱层滑石,通过激光衍射测量确定的平均粒径(D50)为4-8微米,层厚指数为3-15 。

Patent Agency Ranking