Multilayer printed circuit board
    2.
    发明授权
    Multilayer printed circuit board 有权
    多层印刷电路板

    公开(公告)号:US08164001B2

    公开(公告)日:2012-04-24

    申请号:US11986432

    申请日:2007-11-21

    IPC分类号: H05K1/03

    摘要: A multilayer printed circuit board includes an inner magnetic layer essentially consisting of magnetic material. The inner magnetic layer may be formed by an action of chemical bond or van der Waals force. The inner magnetic layer may comprise a plurality of magnetic units, each of which provides magnetism, and may be formed by magnetically coupling the magnetic units with each other by using a strong interaction. The inner magnetic layer may essentially consist of a ferrite film. The ferrite film may be formed directly on the inner conductive layer by means of an electroless plating method. The ferrite film may essentially consist of an oxide metal composition, the metal composition being represented by the formula of FeaNibZncCod, where: a+b+c+d=3.0; 2.1≦a≦2.7; 0.1≦b≦0.3; 0.1≦c≦0.7; and 0≦d≦0.15.

    摘要翻译: 多层印刷电路板包括基本由磁性材料组成的内部磁性层。 内部磁性层可以通过化学键或范德华力的作用形成。 内磁性层可以包括多个磁性单元,每个磁性单元提供磁性,并且可以通过使用强相互作用将磁性单元彼此磁耦合而形成。 内部磁性层可以基本上由铁氧体膜组成。 铁氧体膜可以通过化学镀方法直接形成在内导电层上。 铁氧体膜可以基本上由氧化物金属组合物组成,金属组成由式FeaNibZncCod表示,其中:a + b + c + d = 3.0; 2.1≦̸ a≦̸ 2.7; 0.1≦̸ b≦̸ 0.3; 0.1≦̸ c≦̸ 0.7; 和0≦̸ d≦̸ 0.15。

    Ferrite material, ferrite film formed thereof, and radio frequency identification tag with ferrite film
    4.
    发明申请
    Ferrite material, ferrite film formed thereof, and radio frequency identification tag with ferrite film 审中-公开
    铁氧体材料,由其形成的铁氧体膜和具有铁氧体膜的射频识别标签

    公开(公告)号:US20070231614A1

    公开(公告)日:2007-10-04

    申请号:US11717386

    申请日:2007-03-13

    IPC分类号: G11B5/708 G08B13/14

    CPC分类号: C22C38/105 C22C38/002

    摘要: A ferrite material is disclosed, consisting of an oxide metal composition, the metal composition having the formula of FeaNibZncCod, where: a+b+c+d=3.0; 2.1≦a≦2.7; 0≦b≦0.4; 0≦c≦0.4; and 0.1≦d≦0.5. A ferrite film is made of the ferrite material. Preferably, the ferrite film is formed by a ferrite plating method to have a thickness of 30 μm or less and an aspect ratio of 30 or more. The ferrite film is arranged or provided in the vicinity of an antenna conductor of a radio frequency identification tag. The ferrite film may be in direct contact with the antenna conductor.

    摘要翻译: 公开了一种铁氧体材料,其由氧化物金属组合物组成,该金属组合物具有下式的金属组成:具有下式的金属组成: > d ,其中:a + b + c + d = 3.0; 2.1 <= a <= 2.7; 0 <= b <= 0.4; 0 <= c <= 0.4; 和0.1 <= d <= 0.5。 铁氧体膜由铁氧体材料制成。 优选地,通过铁素体电镀法形成厚度为30μm以下,纵横比为30以上的铁氧体膜。 铁氧体膜被布置或设置在射频识别标签的天线导体附近。 铁氧体膜可以与天线导体直接接触。