摘要:
A semiconductor device and a method thereof are disclosed. In the example method, a mold layer having an opening may be formed on a substrate. A conductive etchable pattern (e.g., a preliminary conductive pattern, a lower electrode pattern, etc.) may be formed within the opening. The mold layer may be reduced so as to expose a portion of the conductive etchable pattern and less than all of the exposed portion of the conductive etchable pattern may be etched such that the etched conductive etchable pattern has a reduced thickness. The example semiconductor device may include the etched conductive etchable pattern as above-described with respect to the example method.
摘要:
A semiconductor structure may be formed by a wet etching process using an etchant containing water. The semiconductor structure may include a plurality of patterns having an increased or higher aspect ratio and may be arranged closer to one another. A dry cleaning process may be performed using hydrogen fluoride gas on the semiconductor structure.
摘要:
A semiconductor structure may be formed by a wet etching process using an etchant containing water. The semiconductor structure may include a plurality of patterns having an increased or higher aspect ratio and may be arranged closer to one another. A dry cleaning process may be performed using hydrogen fluoride gas on the semiconductor structure.
摘要:
In a method of processing a semiconductor structure and a method of forming a capacitor for a semiconductor device using the same, a semiconductor structure may be cleaned using a cleaning solution having a surface tension lower than that of water. The semiconductor structure may be dried in an isopropyl alcohol vapor atmosphere.
摘要:
A corrosion-inhibiting cleaning composition for semiconductor wafer processing includes an aqueous admixture of at least water, a surfactant and a corrosion-inhibiting compound selected from a group consisting of amino phosphonates, polyamines and polycarboxylic acids. The quantity of the corrosion-inhibiting compound in the admixture is preferably in a range from about 0.0001 wt % to about 0.1 wt % and the quantity of the surfactant is preferably in a range from about 0.001 wt % to about 1.0 wt %. The aqueous admixture may also include sulfuric acid and a fluoride, which act as oxide etchants, and a peroxide, which acts as a metal etchant.
摘要:
Provided herein are methods for using corrosion-inhibiting cleaning compositions for semiconductor wafer processing that include an aqueous admixture of at least water, a surfactant and a corrosion-inhibiting compound selected from a group consisting of amino phosphonates, polyamines and polycarboxylic acids. The quantity of the corrosion-inhibiting compound in the admixture is preferably in a range from about 0.0001 wt % to about 0.1 wt % and the quantity of the surfactant is preferably in a range from about 0.001 wt % to about 1.0 wt %. The aqueous admixture may also include sulfuric acid and a fluoride, which act as oxide etchants, and a peroxide, which acts as a metal etchant.
摘要:
Disclosed is an organic stripping composition and a method of etching a semiconductor device in which the generation of an Si pitting phenomenon can be prevented. The composition includes a compound including a hydroxyl ion (OH−), a compound including a fluorine ion (F−) and a sufficient amount of an oxidizing agent to control the pH of the composition within the range of from about 6.5 to about 8.0. The method includes dry etching an oxide by a dry etching using a plasma, and then ashing the etched oxide using an ashing process to remove an organic material. The method further includes supplying the organic stripping composition to remove residues including any residual organic material, a metal polymer, and an oxide type polymer. The stripping composition is stable onto various metals and does not induce the Si pitting phenomenon.
摘要:
Cleaning solutions for integrated circuit devices and methods of cleaning integrated circuit devices using the same are disclosed. The cleaning solution includes about 30% aqueous ammonia solution, acetic acid by a volume percent higher then a volume percent of the aqueous ammonia solution, and deionized water by a volume percent higher then the volume percent of the acetic acid. Additionally, disclosed are methods wherein the cleaning solution is formed on integrated circuit substrates having an exposed metal pattern formed thereon, and further providing mega-sonic energy to the film of the cleaning solution.
摘要:
Example embodiments of the present invention relate to an etching solution, a method of forming a pattern using the same, a method of manufacturing a multiple gate oxide layer using the same and a method of manufacturing a flash memory device using the same. Other example embodiments of the present invention relate to an etching solution having an etching selectivity between a polysilicon layer and an oxide layer, a method of forming a pattern using an etching solution using the same, a method of manufacturing a multiple gate oxide layer using the same, and a method of manufacturing a flash memory device using the same. An etching solution including hydrogen peroxide (H2O2) and ammonium hydroxide (NH4OH) by a volume ratio of about 1:2 to about 1:10 mixed in water. In a method of forming a pattern and methods of manufacturing a multiple gate oxide layer and a flash memory device, a polysilicon layer may be formed on a substrate. An insulation layer pattern including an opening exposing the polysilicon layer may be formed on the polysilicon layer. The polysilicon layer exposed by the insulation layer pattern may be etched using the etching solution. A polysilicon layer pattern may be formed on the substrate using the etching solution.
摘要:
Methods of forming non-volatile memory devices include the steps of forming a semiconductor substrate having first and second floating gate electrodes thereon and an electrically insulating region extending between the first and second floating gate electrodes. A step is then performed to etch back the electrically insulating region to expose upper corners of the first and second floating gate electrodes. Another etching step is then performed. This etching step includes exposing upper surfaces and the exposed upper corners of the first and second floating gate electrodes to an etchant that rounds the exposed upper corners of the first and second floating gate electrodes. The step of etching back the electrically insulating region includes etching back the electrically insulating region to expose sidewalls of the first and second floating gate electrodes having heights ranging from about 30 Å to about 200 Å. The step of exposing the upper corners of the first and second floating gate electrodes to an etchant is followed by the step of etching back the electrically insulating region to expose entire sidewalls of the first and second floating gate electrodes.