Low contrast anti-reflection articles with reduced scratch and fingerprint visibility

    公开(公告)号:US12092793B2

    公开(公告)日:2024-09-17

    申请号:US17983527

    申请日:2022-11-09

    IPC分类号: G02B1/11 C03C17/34 G02B1/115

    摘要: Embodiments of articles including a low-contrast anti-reflection coating are disclosed. The coated surface of such articles exhibits a reduced difference in reflectance between a pristine state and when a surface defect is present. In one or more embodiments, the coated surface of such articles exhibits a first average reflectance in the range from about 0.6% to about 6.0% in a pristine condition and a second average reflectance of about 8% or less after removal of a surface thickness of the anti-reflection coating. In other embodiments, the coated substrate exhibits a second average reflectance of about 10% or less, when the coated surface comprises a contaminant. In some embodiments, the coated substrate exhibits a first color coordinate (a*1, b*1) in a pristine condition and a second color coordinate (a*2, b*2) after the presence of a surface defect such that Δa*b* is about 6 or less.

    Low contrast anti-reflection articles with reduced scratch and fingerprint visibility

    公开(公告)号:US11531141B2

    公开(公告)日:2022-12-20

    申请号:US16821121

    申请日:2020-03-17

    IPC分类号: G02B1/11 G02B1/115 C03C17/34

    摘要: Embodiments of articles including a low-contrast anti-reflection coating are disclosed. The coated surface of such articles exhibits a reduced difference in reflectance between a pristine state and when a surface defect is present. In one or more embodiments, the coated surface of such articles exhibits a first average reflectance in the range from about 0.6% to about 6.0% in a pristine condition and a second average reflectance of about 8% or less after removal of a surface thickness of the anti-reflection coating. In other embodiments, the coated substrate exhibits a second average reflectance of about 10% or less, when the coated surface comprises a contaminant. In some embodiments, the coated substrate exhibits a first color coordinate (a*1, b*1) in a pristine condition and a second color coordinate (a*2, b*2) after the presence of a surface defect such that Δa*b* is about 6 or less.