    发明申请
    Molding method and apparatus of resin molded article 审中-公开
    树脂成型品的成型方法和装置

    公开(公告)号:US20070187859A1

    公开(公告)日:2007-08-16

    申请号:US11648630

    申请日:2007-01-03

    IPC分类号: B29C44/02

    摘要: A foaming molten resin containing reinforcement fibers and super critical fluid is injected into a cavity with a short shot (a), the foaming molten resin is made self-foam and flow in the cavity (b), and a volume of the cavity is increased by expanding molds so as to expand the foaming molten resin in the cavity (c). During the expansion step (c), the expansion of the foaming molten resin is assisted by gas vent, vacuum suction, partial pressure adding with gas or resin, or a spring back force of the reinforcement fiber in the foaming molten resin. Accordingly, there can be provided a resin foam molded article that has no improperly large air voids therein, a sufficient volume expansion thereof, and a superior transferability function.

    摘要翻译: 将含有增强纤维和超临界流体的发泡熔融树脂注入到短腔(a)的空腔中,发泡熔融树脂自发泡沫并在空腔(b)中流动,并且空腔体积增加 通过膨胀模具以使空腔(c)中的发泡熔融树脂膨胀。 在膨胀步骤(c)期间,发泡熔融树脂的膨胀由发泡熔融树脂中的排气,真空抽吸,气体或树脂的分压添加或增强纤维的回弹力辅助。 因此,可以提供一种树脂发泡成型体,其中没有不适当的大的空气空隙,其充分的体积膨胀和优异的转移性功能。

    Molding method and apparatus of fiber filler reinforced resin molded article
    6.
    发明申请
    Molding method and apparatus of fiber filler reinforced resin molded article 审中-公开
    纤维增强树脂成型制品的成型方法和装置

    公开(公告)号:US20070182048A1

    公开(公告)日:2007-08-09

    申请号:US11636648

    申请日:2006-12-11

    IPC分类号: B29C44/12

    摘要: There are provided a plasticizing-kneading step of plasticizing a reinforcement fiber and a resin in a cylinder having a screw, and a metering-injecting step of supplying a physical foaming agent to the resin and injecting them into a cavity of a mold, after metering the necessary amount of resin for molding, a foaming-agent supplying step of supplying the physical foaming agent to the resin passed through a nozzle after being plasticized, and a mixing-dispersion promoting step of promoting mixing and dispersion of the physical foaming agent in the resin in a resin flow path from a supply portion of the physical foaming agent to the cavity of the mold. Accordingly, any breakage of reinforcement fiber is prevented and the mixing and dispersion of the physical foaming agent is improved.

    摘要翻译: 提供了一种在具有螺杆的圆筒中增塑纤维和树脂增塑的增塑捏合步骤,以及计量注射步骤,在物理发泡剂供给物质发泡剂之后将其注入到模具的空腔中 必要量的用于成型的树脂,将经过塑化后通过喷嘴的树脂供给物理发泡剂的发泡剂供给步骤和促进物理发泡剂的混合分散的混合分散促进步骤 树脂从物理发泡剂的供给部分到模具的空腔的树脂流动路径中。 因此,防止了增强纤维的断裂,改善了物理发泡剂的混合和分散。

    Long fiber-reinforced polypropylene resin composition
    10.
    发明授权
    Long fiber-reinforced polypropylene resin composition 有权
    长纤维增强聚丙烯树脂组合物

    公开(公告)号:US06586517B2

    公开(公告)日:2003-07-01

    申请号:US10073254

    申请日:2002-02-13

    IPC分类号: C08J300

    摘要: The present invention provides a long fiber-reinforced polypropylene resin composition for a molded article which is improved in all of a mechanical strength, a rigidity and an impact resistance and excellent as well in a durability, in which the long fiber-reinforced polypropylene resin composition comprises a long fiber-reinforced propylene polymer composition comprising a propylene polymer modified with unsaturated carboxylic acid or an anhydride thereof and having an isotactic pentad ratio of 96% or more and a melt flow rate of 100 to 500 g/10 min, an alkaline earth metal compound, and a glass fiber; and a propylene-ethylene copolymer composition comprising a propylene-ethylene copolymer having a melt flow rate of 10 to 60 g/10 min and a nucleating agent.

    摘要翻译: 本发明提供一种模塑制品的长纤维增强聚丙烯树脂组合物,其全部机械强度,刚性和抗冲击性以及耐久性优异,其中长纤维增强聚丙烯树脂组合物 包括长纤维增强丙烯聚合物组合物,其包含用不饱和羧酸或其酸酐改性的丙烯聚合物,其全同立构五价比为96%以上,熔体流动速率为100〜500g / 10min,碱土 金属化合物和玻璃纤维; 和包含熔体流动速率为10至60g / 10min的丙烯 - 乙烯共聚物和成核剂的丙烯 - 乙烯共聚物组合物。