摘要:
The instant invention provides nonwoven fabrics and staple or binder fibers prepared from an ethylene-based polymer having a Comonomer Distribution Constant in the range of from greater than from 100 to 400, a vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of the ethylene-based polymer composition; a zero shear viscosity ratio (ZSVR) in the range from 1 to less than 2; a density in the range of 0.930 to 0.970 g/cm3, a melt index (12) in the range of from 15 to 30 or from 10 to 50 g/10 minutes, a molecular weight distribution (Mw/Mn) in the range of from 2 to 3.5, and a molecular weight distribution (Mz/Mw) in the range of from less than 2.
摘要:
The instant invention provides nonwoven fabrics and staple or binder fibres prepared from an ethylene-based polymer having a Comonomer Distribution Constant in the range of from greater than from 100 to 400, a vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of the ethylene-based polymer composition; a zero shear viscosity ratio (ZSVR) in the range from 1 to less than 2; a density in the range of 0.930 to 0. 970 g/cm3, a melt index (12) in the range of from 15 to 30 or from 10 to 50 g/10 minutes, a molecular weight distribution (Mw/Mn) in the range of from 2 to 3.5, and a molecular weight distribution (Mz/Mw) in the range of from less than 2.
摘要:
The present invention provides bicomponent fibers, a method of producing bicomponent fibers, nonwoven materials comprising one or more such bicomponent fibers, and a method for making such nonwoven materials. The bicomponent fibers according to the present invention comprise (a) a first component comprising a polymeric material selected from the group consisting of polypropylene, polyester, and polyamide; and (b) a second component comprising a polyethylene composition comprising less than or equal to 100 percent by weight of the units derived from ethylene; and less than 20 percent by weight of units derived from one or more α-olefin comonomers; wherein the polyethylene composition has a density in the range of from 0.945 to 0. 965 g/cm3, a molecular weight distribution (Mw/Mn) in the range of from 1.70 to 3.5, a melt index (I2) in the range of from 0.2 to 150 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of from less than 2.5, vinyl unsaturation in the range of from less than 0.1 vinyls per one thousand carbon atoms present in the backbone of said composition.
摘要:
The present invention relates to particular ethylene-based polymer compositions suitable for use in binder fiber applications. The materials are characterized in having a peak recrystallization temperature in the range of from 85° C. to 110 C, and a Comonomer Distribution Constant (“CDC”) of 55 or greater. The materials are also characterized by having a tan delta value at 0.1 rad/sec from about 15 to 50, and a complex viscosity at 0.1 rad/second of 1400 Pa·sec or less.
摘要:
A bicomponent fiber is obtainable from or comprises an ethylene/α-olefin interpolymer characterized by an elastic recovery, Re, in percent at 300 percent strain and 1 cycle and a density, d, in grams/cubic centimeter, wherein the elastic recovery and the density satisfy the following relationship: Re>1481−1629(d). Such interpolymer can also be characterized by other properties. The fibers made therefrom have a relatively high elastic recovery and a relatively low coefficient of friction. The fibers can be cross-linked, if desired. Woven or non-woven fabrics, such as spunbond, melt blown and spun-laced fabrics or webs can be made from such fibers.
摘要:
A composite structure including a substrate and a fluid in contact with the substrate, wherein the substrate comprises a non-woven, a foam, or combinations thereof and is characterized by having a basis weight of 15 to 500 grams per square meter.
摘要:
The present invention relates to propylene-based nonwoven layers made by the meltblown process, and laminates incorporating such layers. The meltblown layers of the present invention comprise propylene copolymers characterized by having less than 50 percent crystallinity. The meltblown layers of the present invention show an improved combination of extensibility and tensile strength. The laminate structures of the present invention are characterized by a combination of low bending modulus with high peel strength.
摘要:
A polypropylene impact copolymer is disclosed. The propylene impact copolymer composition comprises from 60 to 90 percent by weight of the impact copolymer composition of a matrix phase, which can be a homopolymer polypropylene or random polypropylene copolymer having from 0.1 to 7 mol percent of units derived from ethylene or C4-C10 alpha olefins. The propylene impact copolymer composition also comprises from 10 to 40 percent by weight of the impact copolymer composition of a dispersed phase, which comprises a propylene/alpha-olefin copolymer having from 6 to 40 mol percent of units derived from ethylene or C4-C10 alpha olefins, wherein the dispersed phase has a comonomer content which is greater than the comonomer content in the matrix phase. The propylene impact copolymer composition is further characterized by having the ratio of the dispersed phase intrinsic viscosity (IV) to the matrix phase IV being 0.95 or less. The polypropylene impact copolymers of the present invention are well suited for making spunbond fibers which can be used to make nonwoven fabrics having good haptics.
摘要:
The present disclosure provides for a tape or monofilament of a polyethylene composition comprising less than or equal to 100 percent by weight of the polyethylene composition derived from ethylene monomers, and less than 20 percent by weight of the polyethylene composition derived from one or more α-olefin monomers, where the polyethylene composition of the tape or monofilament has a density in the range of 0.920 to 0.970 g/cm3, a molecular weight distribution (Mw/Mn) in the range of 1.70 to 3.5, a melt index (I2) in the range of 0.2 to 50 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of less than 2.5, vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of the polyethylene composition, where the tape or monofilament has a decitex of greater than 500 g/10,000 m.
摘要:
Fabricated articles are disclosed which comprise a polypropylene impact copolymer. The propylene impact copolymer composition comprises from 60 to 90 percent by weight of the impact copolymer composition of a matrix phase, which can be a homopolymer polypropylene or random polypropylene copolymer having from 0.1 to 7 mol percent of units derived from ethylene or C4-C10 alpha olefins. The propylene impact copolymer composition also comprises from 10 to 40 percent by weight of the impact copolymer composition of a dispersed phase, which comprises a propylene/alpha-olefin copolymer having from 6 to 40 mol percent of units derived from ethylene or C4-C10 alpha olefins, wherein the dispersed phase has a comonomer content which is greater than the comonomer content in the matrix phase. The propylene impact copolymer composition is further characterized by having the ratio of the matrix MFR to the dispersed phase MFR being 1.2 or less. The fabricated articles of the present invention cane be made at high speeds and are characterized by their soft feel, as compared to fabricated articles made from other propylene impact copolymers.