Process for production of polyamide composite material
    4.
    发明授权
    Process for production of polyamide composite material 有权
    聚酰胺复合材料生产工艺

    公开(公告)号:US07265187B2

    公开(公告)日:2007-09-04

    申请号:US10675951

    申请日:2003-10-02

    Abstract: In the process of the present invention, a polyamide A1 and an organized clay B are mixed mainly by dispersive mixing, and after added with a polyamide A2, mixed mainly by distributive mixing in a corotating intermeshing twin-screw extruder so designed as to effect the dispersive mixing and the distributive mixing. The organized clay B is completely and finely dispersed and distributed throughout the resultant polyamide composite material. Shaped articles such as films and sheets made of the polyamide composite material exhibit excellent gas barrier properties and transparency with little malodor mainly attributable to the decomposed products of the organizing agent for preparing the organized clay B.

    Abstract translation: 在本发明的方法中,主要通过分散混合将聚酰胺A1和有机粘土B混合,并且在加入聚酰胺A2之后,主要通过分配混合在相互啮合的双螺杆挤出机中进行混合, 分散混合和分配混合。 有机粘土B完全精细地分散并分布在所得的聚酰胺复合材料中。 由聚酰胺复合材料制成的薄膜和薄片等成型体,具有优异的阻气性和透明性,主要是由于用于制备有机粘土B的组织剂的分解产物而产生的恶臭。

    Thin-wall article
    7.
    发明授权
    Thin-wall article 有权
    薄壁文章

    公开(公告)号:US09096714B2

    公开(公告)日:2015-08-04

    申请号:US13824027

    申请日:2012-08-07

    Abstract: Provided is a thin-wall article formed from a polyamide resin which can be stably produced with little variation in mechanical properties such as flexural strength, flexural modulus and impact resistance. A thin-wall article formed by molding a polyamide resin (C) obtained by polycondensing a diamine (A) and a dicarboxylic acid (B) or a polyamide resin composition containing the polyamide resin, wherein 70 mol % or more of a diamine structural unit is derived from xylylenediamine and the polyamide resin has a melt viscosity (i) of 50 to 200 Pa·s as measured at a temperature of the melting point plus 10° C. for a holding time of 6 minutes at a shear rate of 122 sec−1.

    Abstract translation: 本发明提供一种由聚酰胺树脂形成的薄壁制品,其可以稳定地制造,其弯曲强度,弯曲模量和抗冲击性等机械性能几乎不变化。 通过将通过使二胺(A)和二羧酸(B)缩聚得到的聚酰胺树脂(C)或含有聚酰胺树脂的聚酰胺树脂组合物成型而形成的薄壁制品,其中,70mol%以上的二胺结构单元 衍生自苯二甲胺,聚酰胺树脂的熔融粘度(i)在熔点加10℃保温6分钟,剪切速度为122秒时的熔融粘度(i)为50〜200Pa·s -1。

    Polyamide resins and processes for molding them
    8.
    发明授权
    Polyamide resins and processes for molding them 有权
    聚酰胺树脂及其成型方法

    公开(公告)号:US08841407B2

    公开(公告)日:2014-09-23

    申请号:US13824695

    申请日:2011-11-08

    CPC classification number: C08G69/265 C08G69/26 C08L77/06

    Abstract: Provided is a polyamide resin having high heat resistance, excellent moldability and excellent mechanical properties. The polyamide resin comprises a diamine unit containing 70 mol % or more of a xylylenediamine unit and a dicarboxylic acid unit containing 70 mol % or more of a straight chain aliphatic dicarboxylic acid unit, wherein the xylylenediamine unit is composed of 50 to 95 mol % of p-xylylenediamine and 50 to 5 mol % of m-xylylenediamine; the straight chain aliphatic dicarboxylic acid unit is composed of 50 to 100 mol % of adipic acid and 0 to less than 50 mol % of sebacic acid or other straight chain aliphatic dicarboxylic acids; the molar ratio of reacted diamine units to reacted dicarboxylic acid units (the number of moles of reacted diamine units/the number of moles of reacted dicarboxylic acid units) is less than 0.994; and the polyamide resin has a number average molecular weight of 10,000 to 25,000 and a melting point of 285° C. or more.

    Abstract translation: 提供耐热性高,成型性优异,机械特性优异的聚酰胺树脂。 聚酰胺树脂包含含有70摩尔%以上的苯二甲胺单元的二胺单元和含有70摩尔%以上的直链脂肪族二羧酸单元的二羧酸单元,其中,所述苯二甲胺单元为50〜95摩尔% 对苯二甲胺和50〜5摩尔间苯二甲胺; 直链脂肪族二羧酸单元由50〜100摩尔%的己二酸和0〜小于50摩尔%的癸二酸或其它直链脂肪族二羧酸组成, 反应的二胺单元与反应的二羧酸单元的摩尔比(反应的二胺单元的摩尔数/反应的二羧酸单元的摩尔数)小于0.994; 聚酰胺树脂的数均分子量为10,000〜25,000,熔点为285℃以上。

    THIN-WALL ARTICLE
    9.
    发明申请
    THIN-WALL ARTICLE 有权
    薄壁文章

    公开(公告)号:US20140194569A1

    公开(公告)日:2014-07-10

    申请号:US13824027

    申请日:2012-08-07

    Abstract: Provided is a thin-wall article formed from a polyamide resin which can be stably produced with little variation in mechanical properties such as flexural strength, flexural modulus and impact resistance. A thin-wall article formed by molding a polyamide resin (C) obtained by polycondensing a diamine (A) and a dicarboxylic acid (B) or a polyamide resin composition containing the polyamide resin, wherein 70 mol % or more of a diamine structural unit is derived from xylylenediamine and the polyamide resin has a melt viscosity (i) of 50 to 200 Pa·s as measured at a temperature of the melting point plus 10° C. for a holding time of 6 minutes at a shear rate of 122 sec−1.

    Abstract translation: 本发明提供一种由聚酰胺树脂形成的薄壁制品,其可以稳定地制造,其弯曲强度,弯曲模量和抗冲击性等机械性能几乎不变化。 通过将通过使二胺(A)和二羧酸(B)缩聚得到的聚酰胺树脂(C)或含有聚酰胺树脂的聚酰胺树脂组合物成型而形成的薄壁制品,其中,70mol%以上的二胺结构单元 衍生自苯二甲胺,聚酰胺树脂的熔融粘度(i)在熔点加10℃保温6分钟,剪切速度为122秒时的熔融粘度(i)为50〜200Pa·s -1。

    POLYAMIDE RESIN-TYPE COMPOSITE MATERIAL AND METHOD OF PRODUCING SAME
    10.
    发明申请
    POLYAMIDE RESIN-TYPE COMPOSITE MATERIAL AND METHOD OF PRODUCING SAME 审中-公开
    聚酰胺树脂类复合材料及其生产方法

    公开(公告)号:US20130062806A1

    公开(公告)日:2013-03-14

    申请号:US13518651

    申请日:2011-04-28

    Applicant: Jun Mitadera

    Inventor: Jun Mitadera

    Abstract: A xylylenediamine-based polyamide resin/fiber composite material and molding are provided that do not exhibit a decline in properties under high temperatures and high humidities, and that exhibit a high elastic modulus and present little warping, and exhibit better recycle characteristics, a better moldability, and a better productivity than for thermosetting resins.The polyamide resin-type composite material comprises a fibrous material (B) impregnated with a polyamide resin (A) wherein at least 50 mole % of diamine structural units derived from xylylenediamine, and having a number-average molecular weight (Mn) of 6,000 to 30,000, and containing a component of a molecular weight of not more than 1,000 at 0.5 to 5 mass %.

    Abstract translation: 提供了一种苯二甲胺类聚酰胺树脂/纤维复合材料,并且在高温和高湿度下不显示性能下降的成型体,并且表现出高的弹性模量并且几乎没有翘曲,并且表现出更好的回收特性,更好的成型性 ,并且比热固性树脂具有更好的生产率。 聚酰胺树脂型复合材料包括浸渍有聚酰胺树脂(A)的纤维材料(B),其中至少50摩尔%来源于苯二甲胺的二胺结构单元,数均分子量(Mn)为6,000至 并且在0.5〜5质量%的范围内含有分子量为1000以下的成分。