Methods of dry etching silicon-containing dielectric films are described. The methods include maintaining a relatively high temperature of the dielectric films while etching in order to achieve reduced solid residue on the etched surface. Partially or completely avoiding the accumulation of solid residue increases the etch rate.
摘要:
Methods of dry etching silicon-containing dielectric films are described. The methods include maintaining a relatively high temperature of the dielectric films while etching in order to achieve reduced solid residue on the etched surface. Partially or completely avoiding the accumulation of solid residue increases the etch rate.
摘要:
A method of etching silicon oxide from a multiple trenches is described which allows more homogeneous etch rates among trenches. The surfaces of the etched silicon oxide within the trench following the etch may also be smoother. The method includes two dry etch stages followed by a sublimation step. The first dry etch stage removes silicon oxide quickly and produces large solid residue granules. The second dry etch stage remove silicon oxide slowly and produces small solid residue granules in amongst the large solid residue granules. Both the small and large solid residue are removed in the ensuing sublimation step. There is no sublimation step between the two dry etch stages.
摘要:
A method of etching silicon oxide from a multiple trenches is described which allows more homogeneous etch rates among trenches. The surfaces of the etched silicon oxide within the trench following the etch may also be smoother. The method includes two dry etch stages followed by a sublimation step. The first dry etch stage removes silicon oxide quickly and produces large solid residue granules. The second dry etch stage remove silicon oxide slowly and produces small solid residue granules in amongst the large solid residue granules. Both the small and large solid residue are removed in the ensuing sublimation step. There is no sublimation step between the two dry etch stages.
摘要:
A method of etching silicon-containing material is described and includes a SiConi™ etch having a greater or lesser flow ratio of hydrogen compared to fluorine than that found in the prior art. Modifying the flow rate ratios in this way has been found to reduce roughness of the post-etch surface and to reduce the difference in etch-rate between densely and sparsely patterned areas. Alternative means of reducing post-etch surface roughness include pulsing the flows of the precursors and/or the plasma power, maintaining a relatively high substrate temperature and performing the SiConi™ in multiple steps. Each of these approaches, either alone or in combination, serve to reduce the roughness of the etched surface by limiting solid residue grain size.
摘要:
A method of etching silicon-containing material is described and includes a SiConi™ etch having a greater or lesser flow ratio of hydrogen compared to fluorine than that found in the prior art. Modifying the flow rate ratios in this way has been found to reduce roughness of the post-etch surface and to reduce the difference in etch-rate between densely and sparsely patterned areas. Alternative means of reducing post-etch surface roughness include pulsing the flows of the precursors and/or the plasma power, maintaining a relatively high substrate temperature and performing the SiConi™ in multiple steps. Each of these approaches, either alone or in combination, serve to reduce the roughness of the etched surface by limiting solid residue grain size.
摘要:
A method of etching silicon oxide from a narrow trench and a wide trench (or open area) is described which allows the etch in the wide trench to progress further than the etch in the narrow trench. The method includes two dry etch cycles. The first dry etch cycle involves a low intensity or abbreviated sublimation step which leaves solid residue in the narrow trench. The remaining solid residue inhibits etch progress in the narrow trench during the second dry etch cycle allowing the etch in the wide trench to overtake the etch in the narrow trench.
摘要:
A method of etching silicon oxide from a narrow trench and a wide trench (or open area) is described which allows the etch in the wide trench to progress further than the etch in the narrow trench. The method includes two dry etch cycles. The first dry etch cycle involves a low intensity or abbreviated sublimation step which leaves solid residue in the narrow trench. The remaining solid residue inhibits etch progress in the narrow trench during the second dry etch cycle allowing the etch in the wide trench to overtake the etch in the narrow trench.
摘要:
A method of etching a substrate comprises forming on the substrate, a plurality of double patterning features composed of silicon oxide, silicon nitride, or silicon oxynitride. The substrate having the double patterning features is provided to a process zone. An etching gas comprising nitrogen tri-fluoride, ammonia and hydrogen is energized in a remote chamber. The energized etching gas is introduced into the process zone to etch the double patterning features to form a solid residue on the substrate. The solid residue is sublimated by heating the substrate to a temperature of at least about 100° C.
摘要:
A method of etching silicon-and-carbon-containing material is described and includes a SiConi™ etch in combination with a flow of reactive oxygen. The reactive oxygen may be introduced before the SiConi™ etch reducing the carbon content in the near surface region and allowing the SiConi™ etch to proceed more rapidly. Alternatively, reactive oxygen may be introduced during the SiConi™ etch further improving the effective etch rate.