摘要:
An optical wavelength conversion element includes a cesium-lithium-borate crystal processed into a 10-mm long optical element cut in an orientation that allows a fourth harmonic of a Nd:YAG laser to be generated. A transmittance (Ta) at 3589 cm−1 in an infrared transmission spectrum of the optical element is used as an index that indicates a content of water impurities in the crystal and is independent of a polarization direction. An actual measurement of the transmittance Ta is at least 1%, without taking into account loss at an optically polished surface of the crystal. A wavelength conversion device, a ultraviolet laser irradiation apparatus, a laser processing system, and a method of manufacturing an optical wavelength conversion element are also described.
摘要:
An optical wavelength conversion element includes a cesium-lithium-borate crystal processed into a 10-mm long optical element cut in an orientation that allows a fourth harmonic of a Nd:YAG laser to be generated. A transmittance (Ta) at 3589 cm−1 in an infrared transmission spectrum of the optical element is used as an index that indicates a content of water impurities in the crystal and is independent of a polarization direction. An actual measurement of the transmittance Ta is at least 1%, without taking into account loss at an optically polished surface of the crystal. A wavelength conversion device, a ultraviolet laser irradiation apparatus, a laser processing system, and a method of manufacturing an optical wavelength conversion element are also described.
摘要:
A borate-based crystal excellent in uniformity and reliability, which is useful as an optical wavelength conversion device, etc., and can be easily produced at low cost in a short period of time, by the steps of dissolving water-soluble starting materials in water to prepare an aqueous solution, evaporating water in the aqueous solution followed by sintering or evaporating the water and not sintering, thereby forming a crystal growth material, and melting the resultant material to grow a crystal. Further, a highly reliable laser oscillation apparatus can be achieved by using this crystal as an optical wavelength conversion device.
摘要:
A borate-based crystal excellent in uniformity and reliability, which is useful as an optical wavelength conversion device, etc., and can be easily produced at low cost in a short period of time, by the steps of dissolving water-soluble starting materials in water to prepare an aqueous solution, evaporating water in the aqueous solution followed by sintering or evaporating the water and not sintering, thereby forming a crystal growth material, and melting the resultant material to grow a crystal. Further, a highly reliable laser oscillation apparatus can be achieved by using this crystal as an optical wavelength conversion device.
摘要:
In a wavelength converting method, an ambient that is in contact with a surface of a non-linear optical crystal from which wavelength-converted light is outputted is a gas that is lower in content of nitrogen than air. A wavelength converting device includes a device for controlling the ambient in contact with a surface of the non-linear optical crystal from which the wavelength-converted light is outputted so the ambient is lower in nitrogen than air. A laser machining device includes the wavelength converting device.
摘要:
In a wavelength converting method, an ambient that is in contact with a surface of a non-linear optical crystal from which wavelength-converted light is outputted is a gas that is lower in content of nitrogen than air. A wavelength converting device includes a device for controlling the ambient in contact with a surface of the non-linear optical crystal from which the wavelength-converted light is outputted so the ambient is lower in nitrogen than air. A laser machining device includes the wavelength converting device.
摘要:
A method of manufacturing group III-nitride semiconductor crystal includes the steps of accommodating an alloy containing at least a group III-metal element and an alkali metal element in a reactor, introducing a nitrogen-containing substance in the reactor, dissolving the nitrogen-containing substance in an alloy melt in which the alloy has been melted, and growing group III-nitride semiconductor crystal is provided. The group III-nitride semiconductor crystal attaining a small absorption coefficient and an efficient method of manufacturing the same, as well as a group III-nitride semiconductor device attaining high light emission intensity can thus be provided.
摘要:
A method of manufacturing a group III-nitride crystal substrate including the steps of introducing an alkali-metal-element-containing substance, a group III-element-containing substance and a nitrogen-element-containing substance into a reactor, forming a melt containing at least the alkali metal element, the group III-element and the nitrogen element in the reactor, and growing group III-nitride crystal from the melt, and characterized by handling the alkali-metal-element-containing substance in a drying container in which moisture concentration is controlled to at most 1.0 ppm at least in the step of introducing the alkali-metal-element-containing substance into the reactor is provided. A group III-nitride crystal substrate attaining a small absorption coefficient and the method of manufacturing the same, as well as a group III-nitride semiconductor device can thus be provided.
摘要:
The present invention relates to a process for producing high-quality crystals of protein or organic substances easily and efficiently. A solution of protein or an organic substance is prepared and then is cooled slowly to be supersaturated to a low degree. This supersaturated solution is irradiated with a femtosecond laser 10. A local explosion phenomenon occurs at the focal point of the laser and thereby a crystalline nucleus is generated. A high-quality crystal is obtained when a crystal is grown on the crystalline nucleus over a long period of time. The femtosecond laser to be used herein can be a titanium:sapphire laser having a wavelength of 800 nm, a duration of 120 fs, a frequency of 1 kHz, and an output of 400 mW.
摘要:
There is provided a nonlinear optical crystal which is presented by the formula: K2Al2B2O7. This nonlinear optical crystal is a vacuum ultraviolet light generating nonlinear optical crystal which is easy to grow and of high practical use. There are also provided a wavelength conversion method using this crystal, and an element and a wavelength conversion apparatus for use in the method.
摘要翻译:提供了一种非线性光学晶体,其由下列公式表示:K 2 2 Al 2 B 2 N 2 O 7 。 这种非线性光学晶体是一种容易生长和高实用性的真空紫外线发生非线性光学晶体。 还提供了使用该晶体的波长转换方法以及用于该方法的元件和波长转换装置。