摘要:
The present invention relates to a process for producing high-quality crystals of protein or organic substances easily and efficiently. A solution of protein or an organic substance is prepared and then is cooled slowly to be supersaturated to a low degree. This supersaturated solution is irradiated with a femtosecond laser 10. A local explosion phenomenon occurs at the focal point of the laser and thereby a crystalline nucleus is generated. A high-quality crystal is obtained when a crystal is grown on the crystalline nucleus over a long period of time. The femtosecond laser to be used herein can be a titanium:sapphire laser having a wavelength of 800 nm, a duration of 120 fs, a frequency of 1 kHz, and an output of 400 mW.
摘要:
The present invention relates to a process for producing high-quality crystals of protein or organic substances easily and efficiently. A solution of protein or an organic substance is prepared and then is cooled slowly to be supersaturated to a low degree. This supersaturated solution is irradiated with a femtosecond laser 10. A local explosion phenomenon occurs at the focal point of the laser and thereby a crystalline nucleus is generated. A high-quality crystal is obtained when a crystal is grown on the crystalline nucleus over a long period of time. The femtosecond laser to be used herein can be a titanium:sapphire laser having a wavelength of 800 nm, a duration of 120 fs, a frequency of 1 kHz, and an output of 400 mW.
摘要:
A method of manufacturing group III-nitride semiconductor crystal includes the steps of accommodating an alloy containing at least a group III-metal element and an alkali metal element in a reactor, introducing a nitrogen-containing substance in the reactor, dissolving the nitrogen-containing substance in an alloy melt in which the alloy has been melted, and growing group III-nitride semiconductor crystal is provided. The group III-nitride semiconductor crystal attaining a small absorption coefficient and an efficient method of manufacturing the same, as well as a group III-nitride semiconductor device attaining high light emission intensity can thus be provided.
摘要:
A method of manufacturing a group III-nitride crystal substrate including the steps of introducing an alkali-metal-element-containing substance, a group III-element-containing substance and a nitrogen-element-containing substance into a reactor, forming a melt containing at least the alkali metal element, the group III-element and the nitrogen element in the reactor, and growing group III-nitride crystal from the melt, and characterized by handling the alkali-metal-element-containing substance in a drying container in which moisture concentration is controlled to at most 1.0 ppm at least in the step of introducing the alkali-metal-element-containing substance into the reactor is provided. A group III-nitride crystal substrate attaining a small absorption coefficient and the method of manufacturing the same, as well as a group III-nitride semiconductor device can thus be provided.
摘要:
There is provided a nonlinear optical crystal which is presented by the formula: K2Al2B2O7. This nonlinear optical crystal is a vacuum ultraviolet light generating nonlinear optical crystal which is easy to grow and of high practical use. There are also provided a wavelength conversion method using this crystal, and an element and a wavelength conversion apparatus for use in the method.
摘要翻译:提供了一种非线性光学晶体,其由下列公式表示:K 2 2 Al 2 B 2 N 2 O 7 。 这种非线性光学晶体是一种容易生长和高实用性的真空紫外线发生非线性光学晶体。 还提供了使用该晶体的波长转换方法以及用于该方法的元件和波长转换装置。
摘要:
In a method for growing a single crystal by bringing a seed crystal (4) into contact with a melt (2) of raw materials melted under heating in a crucible (1) a blade member (5) or a baffle member in disposed in the raw material melt (2) in the crucible (1) and a single crystal is grown by pulling up it with rotating the crucible (1) to thereby grow various single crystals including CLBO from the highly viscous raw material melt (2) as high quality and high performance crystals.
摘要:
There is provided a method of manufacturing a group-III nitride crystal in which a nitrogen plasma is brought into contact with a melt containing a group-III element and an alkali metal to grow the group-III nitride crystal. Furthermore, there is also provided a method of manufacturing a group-III nitride crystal in which the group-III nitride crystal is grown on a substrate placed in a melt containing a group-III element and an alkali metal, with a minimal distance between a surface of the melt and a surface of the substrate set to be at most 50 mm.
摘要:
An optical wavelength conversion element includes a cesium-lithium-borate crystal processed into a 10-mm long optical element cut in an orientation that allows a fourth harmonic of a Nd:YAG laser to be generated. A transmittance (Ta) at 3589 cm−1 in an infrared transmission spectrum of the optical element is used as an index that indicates a content of water impurities in the crystal and is independent of a polarization direction. An actual measurement of the transmittance Ta is at least 1%, without taking into account loss at an optically polished surface of the crystal. A wavelength conversion device, a ultraviolet laser irradiation apparatus, a laser processing system, and a method of manufacturing an optical wavelength conversion element are also described.
摘要:
A borate-based crystal excellent in uniformity and reliability, which is useful as an optical wavelength conversion device, etc., and can be easily produced at low cost in a short period of time, by the steps of dissolving water-soluble starting materials in water to prepare an aqueous solution, evaporating water in the aqueous solution followed by sintering or evaporating the water and not sintering, thereby forming a crystal growth material, and melting the resultant material to grow a crystal. Further, a highly reliable laser oscillation apparatus can be achieved by using this crystal as an optical wavelength conversion device.
摘要:
A method for producing a GaN crystal capable of achieving at least one of the prevention of nucleation and the growth of a high-quality non-polar surface is provided. The production method of the present invention is a method for producing a GaN crystal in a melt containing at least an alkali metal and gallium, including an adjustment step of adjusting the carbon content of the melt, and a reaction step of causing the gallium and nitrogen to react with each other. According to the production method of the present invention, nucleation can be prevented, and as shown in FIG. 4, a non-polar surface can be grown.