Molded Oxide Product and Process for Producing Same
    2.
    发明申请
    Molded Oxide Product and Process for Producing Same 审中-公开
    模制氧化物产品及其生产方法

    公开(公告)号:US20130011664A1

    公开(公告)日:2013-01-10

    申请号:US13503786

    申请日:2011-03-25

    摘要: A molded oxide product of the present invention contains an oxide region and an organic cross-linked region and has at least a surface layer formed of an inorganic glassy material. The molded oxide product can combine both organic and inorganic advantages such as good workability of organic materials and high weather resistance, heat resistance and hardness of inorganic materials. The molded oxide product can be produced through the following steps: step A for preparing a precursor R2-M-O-M′ having a polymerizable functional group-containing organic group R2 and a M-O-M′ bond; step B for applying an application liquid containing the precursor; step C for hardening the application liquid by photocuring and/or thermosetting; and step D for performing oxidation treatment on at least a surface layer of the hardened product in such a manner as to convert at least the surface layer of the hardened product to be of inorganic glassy material.

    摘要翻译: 本发明的模塑氧化物产品含有氧化物区域和有机交联区域,并且至少具有由无机玻璃状材料形成的表面层。 成型的氧化物产品可以结合有机和无机的优点,如有机材料的良好的加工性和高耐候性,耐热性和无机材料的硬度。 可以通过以下步骤制备模制的氧化物产物:用于制备具有可聚合官能团的有机基团R 2和M-O-M'键的前体R 2 -M-O-M'的步骤A; 步骤B,用于施加含有前体的涂布液; 步骤C,用于通过光固化和/或热固化使涂布液硬化; 以及步骤D,用于至少将硬化产物的表层转化为无机玻璃状材料的至少在硬化产品的表面层上进行氧化处理。

    Wiper blade and method for producing the same
    4.
    发明授权
    Wiper blade and method for producing the same 有权
    雨刮片及其制造方法

    公开(公告)号:US07776400B2

    公开(公告)日:2010-08-17

    申请号:US11905921

    申请日:2007-10-05

    IPC分类号: B05D3/02

    摘要: A wiper blade (1) comprising a base portion (3) to be attached to a wiper arm, a lip portion (4) to sweep away a water droplet or dust etc. adhered to a glass window, a thin neck portion (2) for connecting the lip portion (4) and the base portion (3), and a sweeping surface layer portion formed on a side surface of a cross section of the lip portion (4), the sweeping surface layer (7) comprising a scale-like powder (9) having good sliding property and a binder (10) comprising a water-repellency silicone-base rubber composition for binding the scale-like powder (9) to the lip portion (4). The scale-like powder (9) is laminated in a thickness direction of the lip portion (4) and the laminated scale-like powder is bound to each other with the binder (10).

    摘要翻译: 一种刮水片(1),其包括要附接到刮水器臂的基部(3),用于扫除粘附到玻璃窗的水滴或灰尘等的唇部(4),薄的颈部(2) 用于连接唇部(4)和基部(3),以及形成在唇部(4)的横截面的侧表面上的扫掠表面层部分,扫掠表面层(7) 具有良好滑动性的粉末(9)和粘合剂(10),其包含用于将鳞片状粉末(9)与唇部(4)结合的拒水性硅酮基橡胶组合物。 鳞片状粉末(9)在唇部(4)的厚度方向上层叠,层叠的鳞片状粉末用粘合剂(10)彼此结合。

    Honeycomb carrier for exhaust gas clarification catalyst and method for production thereof
    5.
    发明申请
    Honeycomb carrier for exhaust gas clarification catalyst and method for production thereof 有权
    废气净化催化剂用蜂窝载体及其制备方法

    公开(公告)号:US20060239880A1

    公开(公告)日:2006-10-26

    申请号:US10566270

    申请日:2004-07-29

    IPC分类号: B01J23/02

    摘要: To provide a honeycomb carrier to support a catalyst to clean e.g. an exhaust gas of an automobile particularly containing NOx, which is excellent in heat resistance, thermal shock resistance, mechanical strength and thermal decomposition resistance and has a great corrosion resistance to a catalyst, and is thus capable of being used with stability for a long period of time, and a process for its production. The material for the honeycomb carrier is an aluminum magnesium titanate sintered product obtained by firing at from 1,000 to 1,700° C. a molded product formed from a raw material mixture comprising 100 parts by mass, as calculated as oxides, of a mixture comprising a Mg— containing compound, an Al-containing compound and a Ti— containing compound in the same metal component ratio as the metal component ratio of Mg, Al and Ti in an aluminum magnesium titanate represented by the empirical formula MgxAl2(1+x)Ti(1+x)O5 (wherein 0

    摘要翻译: 提供蜂窝载体以支持催化剂清洁例如 特别是含有NOx的汽车的废气,其耐热性,耐热冲击性,机械强度和耐热分解性优异,对催化剂具有很大的耐腐蚀性,因此能够长期稳定地使用 的时间,以及其生产过程。 蜂窝载体的材料是通过在1000〜1700℃下烧成而得到的铝镁钛酸盐烧结体,由原料混合物形成的成型体,该原料混合物含有以氧化物计算的100质量份的由Mg 含铝化合物,含Al化合物和含钛化合物,其以与经验式Mg x S表示的铝镁钛酸盐中的Mg,Al和Ti的金属组分比相同的金属组分比 2(1 + x)Ti(1 + x)O 5(其中0

    Method for producing aluminum titanate sintered compact
    7.
    再颁专利
    Method for producing aluminum titanate sintered compact 有权
    钛酸铝烧结体的制造方法

    公开(公告)号:USRE42646E1

    公开(公告)日:2011-08-23

    申请号:US12285247

    申请日:2003-04-16

    IPC分类号: C04B35/478

    摘要: The present invention provides a raw material composition for preparing a sintered body of aluminum titanate, the composition comprising (i) 100 parts by weight of a mixture comprising 40 to 50 mol % of TiO2 and 60 to 50 mol % of Al2O3, (ii) 1 to 10 parts by weight of an alkali feldspar represented by the formula: (NxK1-x)AlSi3O8 (0≦x≦1), and (iii) 1 to 10 parts by weight of at least one Mg-containing component selected from the group consisting of a Mg-containing oxide with spinel structure, MgCO3 and MgO, and a process for preparing a sintered body of aluminum titanate comprising sintering a formed product prepared from the raw material composition at 1300 to 1700° C. According to the present invention, a sintered body of aluminum titanate having high mechanical strength and ability to be stably used at high temperatures, as well as its inherent properties of low coefficient of thermal expansion and high corrosion resistance, can be obtained.

    摘要翻译: 本发明提供了一种制备钛酸铝烧结体的原料组合物,该组合物包括(i)100重量份的包含40-50mol%TiO 2和60-50mol%Al 2 O 3的混合物,(ii) 1〜10重量份由式(NxK1-x)AlSi3O8(0≦̸ x< 1E; 1)表示的碱长石,和(iii)1〜10重量份的至少一种含Mg成分, 由具有尖晶石结构的含镁氧化物,MgCO 3和MgO组成的组,以及制备钛酸铝烧结体的方法,包括将由原料组合物制备的成形产品烧结在1300至1700℃。根据本发明 可以获得具有高机械强度和在高温下稳定使用的能力的钛酸铝烧结体,以及其低热膨胀系数和高耐腐蚀性的固有性质。