Polyphenylene ether resin composition having narrow molecular weight distribution
    4.
    发明授权
    Polyphenylene ether resin composition having narrow molecular weight distribution 有权
    具有窄分子量分布的聚苯醚树脂组合物

    公开(公告)号:US08445573B2

    公开(公告)日:2013-05-21

    申请号:US12990811

    申请日:2009-05-08

    IPC分类号: C08K5/17 B60C3/00

    摘要: A polyphenylene ether resin composition obtainable by melt-mixing a polyphenylene ether (A) comprising a structural unit (a) represented by formula (1): (wherein R1 and R2 each independently represent a hydrogen atom, a halogen atom, an optionally substituted alkyl group, and the like), and/or a structural unit (b) represented by formula (2): (wherein R3 and R4 each independently represent a hydrogen atom, a halogen atom, an optionally substituted alkyl group, and the like), with a nitrogen compound (B) comprising at least one group selected from the group consisting of primary amino groups, secondary amino groups and tertiary amino groups in a single molecule thereof, wherein the polyphenylene ether (A) comprises 0.1% by mass or more and 1.5% by mass or less of at least one type of aromatic hydrocarbon (C) containing 7 or 8 carbon atoms.

    摘要翻译: 通过将包含由式(1)表示的结构单元(a)的聚苯醚(A)熔融混合而获得的聚苯醚树脂组合物:其中R 1和R 2各自独立地表示氢原子,卤素原子,任选取代的烷基 基团等)和/或由式(2)表示的结构单元(b):(其中R 3和R 4各自独立地表示氢原子,卤素原子,任选取代的烷基等), 与在单分子中含有选自伯氨基,仲氨基和叔氨基中的至少一个基团的氮化合物(B),其中聚苯醚(A)的含量为0.1质量%以上, 至少一种含有7或8个碳原子的芳族烃(C)的1.5质量%以下。

    POLYAMIDE AND POLYAMIDE COMPOSITION
    5.
    发明申请
    POLYAMIDE AND POLYAMIDE COMPOSITION 有权
    聚酰胺和聚酰胺组合物

    公开(公告)号:US20120165466A1

    公开(公告)日:2012-06-28

    申请号:US13393604

    申请日:2010-09-07

    IPC分类号: C08L77/06 C08G69/26

    摘要: [Problem to be Solved]To provide a polyamide having a high melting point, which has excellent strength, toughness, and stability under heating.[Solution]This polyamide is obtained by polymerizing an (a) dicarboxylic acid comprising at least 50 mol % of an alicyclic dicarboxylic acid and a (b) diamine comprising at least 50 mol % of a diamine having a pentamethylenediamine skeleton, wherein the polyamide has a cyclic amino end amount of 30 to 60μ equivalents/g.

    摘要翻译: [待解决的问题]提供具有优异的强度,韧性和加热下的稳定性的具有高熔点的聚酰胺。 [溶液]该聚酰胺通过使包含至少50摩尔%的脂环族二羧酸的(a)二羧酸和包含至少50摩尔%的具有五亚甲基二胺骨架的二胺的(b)二胺聚合而获得,其中聚酰胺具有 环氨基末端量为30〜60μ当量/ g。

    POLYPHENYLENE ETHER RESIN COMPOSITION HAVING NARROW MOLECULAR WEIGHT DISTRIBUTION
    6.
    发明申请
    POLYPHENYLENE ETHER RESIN COMPOSITION HAVING NARROW MOLECULAR WEIGHT DISTRIBUTION 有权
    具有窄分子量分布的聚苯乙烯醚树脂组合物

    公开(公告)号:US20110166269A1

    公开(公告)日:2011-07-07

    申请号:US12990811

    申请日:2009-05-08

    IPC分类号: C08L71/12 C08K5/17

    摘要: A polyphenylene ether resin composition obtainable by melt-mixing a polyphenylene ether (A) comprising a structural unit (a) represented by the following formula (1): (wherein R1 and R2 each independently represent a hydrogen atom, a halogen atom, an optionally substituted alkyl group, and the like), and/or a structural unit (b) represented by the following formula (2): (wherein R3 and R4 each independently represent a hydrogen atom, a halogen atom, an optionally substituted alkyl group, and the like), with a nitrogen compound (B) comprising at least one group selected from the group consisting of primary amino groups, secondary amino groups and tertiary amino groups in a single molecule thereof, wherein the polyphenylene ether (A) comprises 0.1% by mass or more and 1.5% by mass or less of at least one type of aromatic hydrocarbon (C) containing 7 or 8 carbon atoms.

    摘要翻译: 通过熔融混合由下述式(1)表示的结构单元(a)的聚苯醚(A)可以得到的聚苯醚树脂组合物:(其中,R 1和R 2各自独立地表示氢原子,卤素原子, 取代烷基等)和/或由下式(2)表示的结构单元(b):(其中R 3和R 4各自独立地表示氢原子,卤素原子,任选取代的烷基和 (B)包含在单分子中含有伯氨基,仲氨基和叔氨基中的至少一个基团的氮化合物(B),其中聚苯醚(A)含有0.1% 质量以上且1.5质量%以下的至少一种含有7或8个碳原子的芳香族烃(C)。

    Copolymer polyamide
    7.
    发明授权

    公开(公告)号:US09611356B2

    公开(公告)日:2017-04-04

    申请号:US13990937

    申请日:2012-01-06

    摘要: An object of the present invention is to provide a copolymer polyamide which has excellent strength, high-temperature strength, low water absorbance, low blocking properties, releasability and plasticizing time stability, and a copolymer polyamide composition which has excellent vibration fatigue characteristics, surface appearance and continuous productivity. A copolymer polyamide of the present invention is obtained by polymerizing (a) at least one alicyclic dicarboxylic acid, (b) one diamine having 8 or more carbon atoms, and (c) at least one copolymer component selected from the group consisting of the following (c-1) to (c-3): a (c-1) dicarboxylic acid other than the alicyclic dicarboxylic acid; a (c-2) diamine having fewer carbon atoms than the (b) diamine; and a (c-3) lactam and/or aminocarboxylic acid, and the copolymer polyamide satisfies specific conditions.

    Masterbatch pellet, production method therefor and polyamide resin composition containing masterbatch pellet
    10.
    发明授权
    Masterbatch pellet, production method therefor and polyamide resin composition containing masterbatch pellet 有权
    母粒颗粒,其制备方法和含有母料颗粒的聚酰胺树脂组合物

    公开(公告)号:US08765861B2

    公开(公告)日:2014-07-01

    申请号:US13697194

    申请日:2011-05-20

    申请人: Kazunori Terada

    发明人: Kazunori Terada

    IPC分类号: C08J3/22 C08K3/22 B29B9/00

    摘要: A masterbatch pellet is provided for obtaining a polyamide resin composition excellent in mechanical strength and heat aging resistance. The masterbatch pellet is obtained by melt-kneading a raw material component containing a thermoplastic resin (A) and a metal oxide (B), wherein a content of the metal oxide (B) is 0.5% by mass or more and a fraction of the metal oxide (B) after the melt kneading is present as an aggregated particle of 5 μm or more in a major axis length. A proportion of the aggregated particle of 5 μm or more in a major axis length in a whole metal oxide after the melt kneading is preferably 30% by mass or less.

    摘要翻译: 提供母粒颗粒以获得机械强度和耐热老化性优异的聚酰胺树脂组合物。 通过熔融捏合含有热塑性树脂(A)和金属氧化物(B)的原料成分,得到母料颗粒,其中金属氧化物(B)的含量为0.5质量%以上, 熔融捏合后的金属氧化物(B)作为长轴长度为5μm以上的凝集粒子存在。 熔融混炼后的整个金属氧化物的长轴长度为5μm以上的凝集粒子的比例优选为30质量%以下。