摘要:
The present invention provides a method for manufacturing a shaped product constituted by a fiber-reinforced composite material including reinforcing fibers and a thermoplastic resin. The shaped product maintains isotropy of the fibers to the end thereof even if press-molded under conditions in which charge ratio of a prepreg to a die is low. Specifically, the method includes using a specific prepreg obtained by impregnating the reinforcing fibers with thermoplastic resin, and molding-processing the prepreg under specific conditions.
摘要:
This method for manufacturing a shaped product is characterized in preparing a specific random mat including a thermoplastic resin and carbon fiber bundles having an average fiber length of 5-100 mm, impregnating a thermoplastic resin into the random mat, pressing the random mat in a metal mold in a range of 0.1-20 MPa, and then taking out the random mat from the metal mold.
摘要:
There is provided a shaped product made of a fiber-reinforced composite material including reinforcing fibers having an average fiber length of 5 to 100 mm and a thermoplastic resin. In the shaped product, a volume fraction of reinforcing fibers is 5 to 80%, a reference plane (S) and a standing plane (B) inclined at an angle of 45 to 90 degrees with respect to the reference plane are included, a ratio of an area of the standing plane (B) to an area of the reference plane (S) is 0.5 to 100, and in the fiber-reinforced composite material constituting the shaped product, a ratio of a reinforcing fiber bundle (A) including the reinforcing fibers of a critical number of single fiber or more to the total amount of the reinforcing fibers is 20 Vol % or more and 99 Vol % or less.
摘要:
A molded product, including a fiber-reinforced composite material containing reinforcing fibers having an average fiber length of 5 mm to 100 mm and a thermoplastic resin, wherein the molded product has thickness gradient, an amount of the thermoplastic resin is 10 to 1,000 parts by weight per 100 parts by weight of thee reinforcing fibers, and the reinforcing fibers have a fiber areal weight of from 25 g/m2 to 3,000 g/m2 and are substantially two-dimensionally randomly oriented.
摘要翻译:一种模制品,其包含纤维增强复合材料,其含有平均纤维长度为5mm至100mm的增强纤维和热塑性树脂,其中所述模塑产品具有厚度梯度,所述热塑性树脂的量为10至1,000份 每100重量份的增强纤维的重量,并且增强纤维的纤维面积重量为25g / m 3至3,000g / m 2,并且基本上二维随机取向。
摘要:
This production method for a composite shaped product having an undercut portion is able to readily manufacture a composite shaped product having a complicated shape having an undercut portion, by including: a step (i) of forming an impregnated precursor by heating and pressurizing a non-impregnated precursor including carbon fibers with an average fiber length of 1 to 100 mm and a thermoplastic resin; a step (ii) of heating the impregnated precursor at the melting point of the thermoplastic resin or more; a step (iii) of arranging the heated impregnated precursor into a mold having an undercut structure; a step (iv) of clamping the undercut structure after or simultaneously being operated and pressurizing the impregnated precursor; and a step (v) of unclamped the mold, re-operating the undercut structure and taking out the composite shaped material from the unclamped mold.
摘要:
The present invention provides a method for manufacturing a shaped product constituted by a fiber-reinforced composite material including reinforcing fibers and a thermoplastic resin. The shaped product maintains isotropy of the fibers to the end thereof even if press-molded under conditions in which charge ratio of a prepreg to a die is low. Specifically, the method includes using a specific prepreg obtained by impregnating the reinforcing fibers with thermoplastic resin, and molding-processing the prepreg under specific conditions.
摘要:
There is provided a shaped product made of a fiber-reinforced composite material including reinforcing fibers having an average length of 5 mm or more and 100 mm or less and a thermoplastic resin, in which a volume fraction of reinforcing fibers (Vf=100×volume of reinforcing fibers/(volume of reinforcing fibers+volume of thermoplastic resin)) is 5 to 80%, grains are formed on a surface of the shaped product, and a ratio of a reinforcing fiber bundle (A) including the reinforcing fibers of a critical number of single fiber or more, the critical number defined by Formula (1), to the total amount of the reinforcing fibers is 20 Vol % or more and 99 Vol % or less: Critical number of single fiber=600/D (1) (wherein D is an average fiber diameter (μm) of single reinforcing fiber).
摘要:
There is provided a shaped product made of a fiber-reinforced composite material including reinforcing fibers having an average length of 5 mm or more and 100 mm or less and a thermoplastic resin, in which a volume fraction of reinforcing fibers (Vf=100×volume of reinforcing fibers/(volume of reinforcing fibers+volume of thermoplastic resin)) is 5 to 80%, grains are formed on a surface of the shaped product, and a ratio of a reinforcing fiber bundle (A) including the reinforcing fibers of a critical number of single fiber or more, the critical number defined by Formula (1), to the total amount of the reinforcing fibers is 20 Vol % or more and 99 Vol % or less: Critical number of single fiber=600/D (1) (wherein D is an average fiber diameter (μm) of single reinforcing fiber).
摘要:
This method for manufacturing a shaped product is characterized in preparing a specific random mat including a thermoplastic resin and carbon fiber bundles having an average fiber length of 5-100 mm, impregnating a thermoplastic resin into the random mat, pressing the random mat in a metal mold in a range of 0.1-20 MPa, and then taking out the random mat from the metal mold.
摘要:
A method for manufacturing a shaped product includes 1) heating at least three prepregs having a thickness of 0.3 mm to 5.0 mm each including reinforcing fibers having an average fiber length of 3 to 100 mm and a thermoplastic resin, 2) arranging those prepregs so as to constitute at least two layers including P layer and Q layer which are in contact with each other, and 3) then pressing those layers to manufacture one shaped product. A prepreg (p1) in the P layer and a prepreg (q1) in the Q layer are arranged such that at least a part thereof overlaps with each other, and two or more prepregs in the same layer are arranged so as not to be in contact with each other.